共查询到20条相似文献,搜索用时 15 毫秒
1.
V. K. Agarwal V. P. Arora Abhai Mansingh 《Molecular Crystals and Liquid Crystals》2013,570(1-2):117-125
Dielectric measurements have been made in the stable and metastable solid phases of EBBA in the frequency range 0.1 KHz to 100 KHz and in the temperature range - 170 to - 10°C. The dielectric dispersion was absent in the stable phase while in the metastable phase, obtained by rapid cooling, a clear dielectric dispersion was seen. In addition to the primary dispersion extending above about - 125°C there also appears a clear secondary dispersion region below - 125°C. The strength of the second dispersion is lower by one order of magnitude than the primary dispersion. The primary dispersion is of the Debye type with a symmetric distribution of relaxation times. The Cole-Cole distribution parameter varies with temperature and shows a maximum at about -64°C. The results in the primary dispersion region can be qualitatively explained by assuming the free rotation of dipoles above -64°C and a restricted rotation of dipoles at low temperatures. 相似文献
2.
3.
一维光子晶体结构参数的随机扰动对其光学特性的影响 总被引:6,自引:3,他引:3
用特征矩阵法研究结构参数存在随机扰动的情况下一维光子晶体的光学特性, 无论是加工过程中介质层几何厚度的误差, 还是介质层折射率的随机波动都会影响一维光子晶体的光学特性.随机扰动对一维光子晶体带结构高频部分影响较大, 造成带结构消失, 甚至全部变成禁带; 随机扰动对光子晶体缺陷模式的影响是使缺陷模的位置发生随机平移, 平移的程度与随机度有关, 介质层折射率的随机变化要比介质层厚度的随机变化对缺陷模位置的影响要大; 周期数目的增加可以部分地减小缺陷模的平移, 但同时会使缺陷模透射率减小,增加缺陷层厚度可以有效降低随机扰动对光子晶体缺陷模式的影响. 本文的研究将对一维光子晶体的设计工作提供有价值的参考. 相似文献
4.
Bridgman法生长的大尺寸钨酸铅晶体的光学和闪烁性能 总被引:2,自引:0,他引:2
本文报道了我们采用改进的Bridgman法为欧洲核子研究中心(CERN)大型强子对撞机(LHC)上的紧凑型μ子螺线管(CMS)实验生长的大尺寸掺Y3+钨酸铅闪烁晶体,给出了晶体的光学和闪烁性能,如光致发光谱、X射线致发光光谱、纵/横向的透射光谱、光产额以及辐照硬度.测试结果表明,掺Y2O3的钨酸铅晶体光产额很高(>13pe/MeV),且全为100ns以内的快发光,其辐照硬度已接近CMS电磁量能器(ECAL)端帽晶体的要求,同一批晶体彼此间的性能一致性好. 相似文献
5.
6.
7.
8.
9.
10.
From a combined study of the electrical properties between room temperature and 77 K and optical absorption at 300 K of bulk CuInSe2 samples doped with different oxygen concentrations, two shallow acceptor levels are found. The activation energy EA1 and EA2 of these levels in the dilute limit tends to be around 30 and 36 meV, respectively. The increase of EA1 and decrease of EA2 with the increase of oxygen content can be explained consistently on the basis that the ratio of Cu to In atoms increases with the increase of oxygen incorporated into CuInSe2 lattice. 相似文献
11.
本文采用顶部籽晶高温溶液法,以Li4P2O7为助熔剂,生长了大尺寸BaBPO5单晶.进行了BaBPO5晶体的结构测定,结果表明该晶体属三方晶系,空间群:P3221,晶胞参数为a=b=0.71329(10)nm,c=0.70368(14)nm,α=β=90°,γ=120°, Z=3.该晶体结构中沿[001]方向存在BO4四面体链,每一个硼氧四面体用它的两个顶点分别与两个PO4四面体相连组成螺旋状的链.硼氧四面体、磷氧四面体和钡氧多面体结合在一起形成一个三维网络结构.同时,对BaBPO5的粉末倍频效应进行了研究. 相似文献
12.
13.
14.
The crystal synthesis and structure of a new organic monohydrogenmophosphate (3,4‐Cl2‐CH2C6H3NH3)2HPO4·2H2O are reported. This compound crystallizes in the monoclinic P21/n with a = 9.081(7) Å, b = 6.501(5) Å, c = 35.423(12) Å, β = 91.09(5)°, V = 2090.9(2) Å3, and Z = 4. Crystal structure was solved and refined to R = 0.042, using 2543 independent reflections. It can be described by inorganic layers, including the HPO4‐ anions and the H2O molecules, parallel to (a, b) planes and situated at z = 0 and z = 1/2. The interlayer spacing is occupied by the organic molecules which perform different interactions around the 3D network cohesion. A characterization of this compound by solid‐state (13C, 31P) MAS NMR and IR spectroscopies is also reported. (© 2007 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim) 相似文献
15.
基于第一性原理密度泛函理论,计算分析了Zn1-xHfxO(x=0,0.0312,0.0417,0.0625和0.1250)体系的晶格结构、电子结构,Mulliken电荷布居和光学性质.计算结果表明,随着Hf掺杂摩尔百分比的增大,晶体体积膨胀,费米能级进入导带,其附近的导带部分主要由杂质原子Hf的5d态贡献,Hf-O离子键成分作用凸显,故Hf的掺杂引入施主能级进而形成n型ZnO材料的可能性较大.且通过比较吸收谱、反射谱和折射谱,发现适量掺入Hf原子可使ZnO体系在高能区的透过率增加,能量损失谱出现红移.这些性质均与实验中Hf掺杂有类似结果,由此可知适量掺杂Hf的ZnO体系有望在制备光电子器件等领域发挥作用. 相似文献
16.
在结构中周期性地添加谐振单元可以构造局域共振声子晶体并产生低频禁带。本文提出了一种具有谐振单元和弹性支承谐振单元的声子晶体结构,通过声子晶体理论和振动理论对该结构的禁带特性和禁带调控特性进行了计算与分析。结果表明,该结构可在0 Hz处形成禁带;禁带内对振动的衰减强度由衰减因子和有限结构周期数共同决定;结构中存在1条可调控禁带和3条不可调禁带;可调控禁带可以通过改变谐振单元和弹性支承谐振单元的结构参数加以调控;不可调禁带包括第一禁带,它们能够较为稳定地对一定频率的弹性波产生衰减作用。该结构所具有的禁带特性在管路、桥梁和汽车减振领域具有潜在应用。 相似文献
17.
采用垂直无籽晶气相法(VUVG)生长出尺寸达26 mm×45 mm的CdSe单晶体,对CdSe晶体的稳态气相生长速率进行了深入讨论.采用气相升华法提纯后的CdSe多晶原料的X射线粉末衍射谱与PDF卡片值(65-3436)吻合,生长出的单晶体{100}和(110)面XRD衍射峰尖锐,无杂峰,且{100}面出现3级衍射峰.晶锭密度为5.74 g/cm3,与理论计算值接近.退火处理后的晶片在1000~7000 cm-1 红外波段范围内透过率达到70;.采用VUVG法生长的CdSe单晶体,结晶性能好、结构致密、尺寸大和红外透过率高,可用于制备红外非线性光学器件. 相似文献
18.
在LiNbO3中掺进ZnO和Fe2O3,以Czochralski技术生长Zn(7mol;):Fe(0.03;):LiNbO3,Zn(3mol;):Fe(0.03;):LiNbO3和Fe(0.03;):LiNbO3晶体.测试晶体的吸收光谱,Zn:Fe:LiNbO3晶体的吸收边相对Fe:LiNbO3晶体发生紫移.测试晶体的红外光谱,Zn(7mol;):Fe:LiNbO3晶体OH-吸收峰移到3529cm-1.测试晶体抗光致散射能力,Zn(3mol;):Fe:LiNbO3晶体抗光致散射能力比Fe:LiNbO3晶体提高一个数量级,Zn(7mol;):Fe:LiNbO3晶体比Fe:LiNbO3晶体高二个数量级.测试晶体的衍射效率和响应时间,Zn:Fe:LiNbO3晶体响应时间缩短,衍射效率降低.对吸收边和OH-吸收峰移动的机理,以及Zn:Fe:LiNbO3晶体抗光致散射能力增强的机理进行了研究. 相似文献
19.