共查询到20条相似文献,搜索用时 15 毫秒
1.
This work presents the annealing temperature effect on the properties of mercury (Hg)-doped titanium dioxide (TiO2). Thin films and polycrystalline powders have been prepared by sol-gel process. The structure, surface morphology and optical properties, as a function of the annealing temperature, have been studied by atomic force microscopy (AFM), Raman, reflectance and ellipsometric spectroscopies. In order to determine the transformation points, we have analyzed the xerogel-obtained powder by differential scanning calorimetry (DSC). Raman spectroscopy shows the crystalline anatase and rutile phases for the films annealed at 400 °C and 1000 °C respectively. The AFM surface morphology results indicate that the particle size increases from 14 to 57 nm by increasing the annealing temperature. The complex index and the optical band gap (Eg) of the films were determined by the spectroscopic ellipsometry analysis. We have found that the optical band gap decreases by increasing the annealing temperature. 相似文献
2.
Titanium dioxide (TiO2) thin films doping of various iron ion (Fe3+) concentrations were deposited on silicon (Si) (100) and quartz substrates by sol-gel Spin Coating technique followed by a thermal treatment at 600 °C. The structure, surface morphology and optical properties, as a function of the doping, have been studied by X-ray diffractometer (XRD), Raman, ultraviolet-visible (UV-vis) and Spectroscopic Ellipsometry (SE). XRD and Raman analyzes of our thin films show that the crystalline phase of TiO2 thin films comprised only the anatase TiO2, but the crystallinity decreased when the Fe3+ content increased from 0% to 20%. During the Fe3+ addition to 20%, the phase of TiO2 thin film still maintained the amorphous state. The grain size calculated from XRD patterns varies from 29.3 to 22.6 nm. The complex index and the optical band gap (Eg) of the films were determined by the spectroscopic ellipsometry analysis. We have found that the optical band gap decreased with an increasing Fe3+ content. 相似文献
3.
Titanium dioxide thin films have been deposited by reactive magnetron sputtering on glass substrate and subsequently irradiated by UV radiation using a KrF excimer laser. In this work, we have study the influence of the laser fluence (F) ranging between 0.05 and 0.40 mJ/cm2 on the constitution and microstructure of the deposited films. Irradiated thin films are characterized by profilometry, scanning electron microscopy and X-ray diffraction. As deposited films are amorphous, while irradiated films present an anatase structure. The crystallinity of the films strongly varies as a function of F with maximum for F = 0.125 J/cm2. In addition to the modification of their constitution, the irradiated areas present a strongly modified microstructure with appearance of nanoscale features. The physico-chemical mechanisms of these structural modifications are discussed based on the theory of nucleation. 相似文献
4.
Jinming LiuXiaoru Zhao Libing DuanMengmeng Cao Huinan SunJifeng Shao Shuai ChenHaiyan Xie Xiao ChangChangle Chen 《Applied Surface Science》2011,257(23):10156-10160
Nb-doped TiO2 (TNO) thin films were prepared by sol-gel dip-coating method with Nb content in a wide range of 0-20 at.%. The prepared films were preheated at 400 °C and then undertaken by two different post-annealing processes: (a) three times vacuum annealing and (b) multi-round annealing. The designed multi-round annealing was shown to be an effective way to improve the conductive properties of the films, compared to the traditional vacuum annealing process. The minimum resistivity reached approximately 0.5 Ω cm with Nb doping concentration around 12 at.%, and the carrier density increased with Nb-doping concentration until the critical point of 12 at.%, which might be the optimal doping content for our TNO films prepared by sol-gel method. 相似文献
5.
C. Sudakar P. Kharel R. Suryanarayanan J.S. Thakur V.M. Naik R. Naik G. Lawes 《Journal of magnetism and magnetic materials》2008
Thin films of pure TiO2 have been prepared using both spin-coating and sputter-deposition techniques on sapphire and quartz substrates. The structural characteristics of the films have been investigated in detail using Raman spectroscopy and high-resolution transmission electron microscopy (HRTEM). When annealed in vacuum, all films demonstrate room temperature ferromagnetism, while the air-annealed samples show much smaller, often negligible, magnetic moments. The magnetization of the vacuum-annealed sputtered samples depends on film thickness, with the volume magnetization decreasing monotonically with increasing thickness. Furthermore, the magnetization per unit area also decreases slightly with increasing film thickness. These results suggest that ferromagnetism in the vacuum-annealed TiO2 films is mediated by surface defects or interfacial effects, but does not arise from stoichiometric crystalline TiO2. 相似文献
6.
Previous studies suggest that granular interfaces induce a natural and persistent super-hydrophilicity in TiO2-SiO2 composite thin films deposited by sol-gel route. This effect enables to consider self-cleaning applications that do not require a permanent UV exposure, whereas such a permanent exposure is necessary for pure TiO2 films. In this study, TiO2-SiO2 composite thin films have been deposited from a TiO2 anatase crystalline suspension and different SiO2 polymeric sols. Wettability studies show that a suitable control of the TiO2-SiO2 mixed sol formulations noticeably enhances persistence of the natural super-hydrophilicity in composite films. It is shown that, beside granular interface effects, modifications in the composite film morphologies can noticeably influence wettability properties. 相似文献
7.
Porous TiO2 films were deposited on SiO2 pre-coated glass-slides by sol-gel method using octadecylamine (ODA) as template. The amount of ODA in the sol played an important role on the physicochemical properties and photocatalytic performance of the TiO2 films. The films prepared at different conditions were all composed of anatase titanium dioxide crystals, and TiO2 crystalline size got larger with increasing ODA amount. The maximum specific surface area of 41.5 m2/g was obtained for TiO2 powders prepared from titanium sol containing 2.0 g ODA. Methyl orange degradation rate was enhanced along with increasing ODA amount and reached the maximal value at 2.0 g addition of ODA. After 40 min of UV-light irradiation, methyl orange degradation rate reached 30.5% on the porous film, which was about 10% higher than that on the smooth film. Porous TiO2 film showed almost constant activity with slight decrease from 30.5% to 28.5% after 4 times of recycles. 相似文献
8.
Nickel-doped anatase TiO2 nanoparticles have been prepared by sol-gel method. The X-ray powder diffraction study reveals that all the prepared samples have pure anatase phase tetragonal system. The average crystallite size of the prepared sample is 14 nm, when found through transmission electron microscope. A strong frequency dependence of both dielectric constant (?′) and dielectric loss (tan δ) were observed for various dopant levels at room temperature in the frequency range of 42 Hz to 5 MHz. At low frequency, the piling up of mobile charge carriers at the grain boundary produces interfacial polarization giving rise to high dielectric constant. The asymmetric shape of frequency dependence of the dielectric loss for the primary relaxation process is observed for each concentration. From the ac conductivity studies, the reduction in conductivity may arise due to the decreasing particle with the increase in Ni-dopant level. 相似文献
9.
Indium tin oxide (ITO) and titanium dioxide (TiO2) single layer and double layer ITO/TiO2 films were prepared using reactive pulsed laser ablation deposition (RPLAD) with an ArF excimer laser for applications in dye-sensitized solar cells (DSSCs). The films were deposited on SiO2 substrates either at room temperatures (RT) or heated to 200-400 °C. Under optimized conditions, transmission of ITO films in the visible (vis) range was above 89% for films produced at RT and 93% for the ones deposited at higher temperatures. Increasing the substrate temperature from RT to 400 °C enhances the transmission of TiO2 films in the vis-NIR from about 70% to 92%. High transmission (≈90%) was observed for the double layer ITO/TiO2 with a transmission cut-off above 900 nm. From the transmission data, the energies gaps (Eg), as well as the refractive indexes (n) for the films were estimated. n ≈ 2.03 and 2.04, respectively for ITO films and TiO2 film deposited at 400 °C in the visible region. Post-annealing of the TiO2 films for 3 h at 300 and 500 °C was performed to enhance n. The refractive index of the TiO2 films increases with the post-annealing temperature. The direct band gap is 3.6, 3.74 and 3.82 eV for ITO films deposited at RT, 200, and 400 °C, respectively. The TiO2 films present a direct band gap of 3.51 and 3.37 eV for as deposited TiO2 films and when annealed at 400 °C, respectively. There is a shift of about 0.1 eV between ITO and ITO/TiO2 films deposited at 200 °C. The shift decreases by half when the TiO2 film was deposited at 400 °C. Post-annealing was also performed on double layer ITO/TiO2. 相似文献
10.
K. Karthik S. Kesava Pandian K. Suresh Kumar N. Victor Jaya 《Applied Surface Science》2010,256(14):4757-10561
Cobalt-doped TiO2 nanoparticles were synthesized by sol-gel method. The associated structural, optical, compositional and magnetic properties of the nanoparticles as a function of cobalt concentration have been systematically studied. The X-ray powder diffraction reveals that all samples have pure anatase phase tetragonal system and the lattice parameter analysis indicated that Co ions may substitute into the lattice of TiO2. The average particle size is 15 nm, when found through transmission electron microscope. Optical spectroscopy measurement showed that the bandgap value decreases upon increasing Co concentration. The magnetic measurements revealed that the enhanced room temperature ferromagnetism (RTFM) strongly depends on the doping content. 相似文献
11.
Chemical vapor deposition (CVD) method was used in titania surface modification. Titania layers were obtained in sol-gel process and prepared as thin films on silicon wafers in dip-coating method. In order to define the influence of modification on titania surface properties (e.g., friction), various types of fluoroalkylsilanes were used. The effectiveness of the modification was monitored by FT-IR spectroscopy. The topography and frictional measurements were investigated with the use of atomic force microscopy (AFM). 相似文献
12.
Cr doped TiO2-SiO2 nanostructure thin film on glass substrates was prepared by a sol-gel dip coating process. X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS) were used to characterize the structural and chemical properties of the films. A UV-vis spectrophotometer was used to measure the transmittance spectra of the thin film. The hydrophilicity of the thin film during irradiation and storage in a dark place was measured by a contact angle analyzer. The results indicated that Cr doping has a significant effect on the transmittance and super-hydrophilicity of TiO2-SiO2 thin film. 相似文献
13.
We investigate an environmentally friendly aqueous solution system for rutile TiO2 violet color nanocrystalline thin films growth on ITO substrate at room temperature. Film shows considerable absorption in visible region with excitonic maxima at 434 nm. X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), selected area electron diffraction (SAED), UV-vis, water surface contact angle and energy dispersive X-ray analysis (EDX) techniques in addition to actual photo-image that shows purely rutile phase of TiO2 with violet color, super-hydrophilic and densely packed nanometer-sized spherical grains of approximate diameter 3.15 ± 0.4 nm, characterize the films. Band gap energy of 4.61 eV for direct transition was obtained for the rutile TiO2 films. Film surface shows super-hydrophilic behavior, as exhibited water contact angle was 7°. Strong visible absorption (not due to chlorine) leaves future challenge to use these films in extremely thin absorber (ETA) solar cells. 相似文献
14.
ZnGa2O4:Cr3+ thin films with bright red emission were synthesized using a sol-gel process, characterized by scanning electron microscopy (SEM), X-ray diffraction (XRD), Auger electron spectroscopy (AES) and UV-vis and fluorescence spectrophotometry measurements. Effects of calcining temperature, film thickness, calcining duration and substrates on the crystal structure and photoluminescent property have been investigated. It is found that the crystallinity, Ga/Zn ratio and band gap energy (Eg) are significant factors influencing optical characteristics, while the nature of substrates affect the surface morphologies of ZnGa2O4:Cr3+ thin films. 相似文献
15.
CdS doped TiO2 thin films (with CdS content=0, 3, 6, 9 and 12 at%) were grown on glass substrates. The X-ray diffraction analysis revealed that the films are polycrystalline of monoclinic TiO2 structure. The microstructure parameters of the films such as crystallite size (Dν) and microstrain (e) are calculated. Both the crystallites size and the microstrain are decreased with increasing CdS content. The optical constants have been determined in terms of Murmann's exact equations. The refractive index and extinction coefficient are increased with increasing CdS content. The optical band gap is calculated in the strong absorption region. The possible optical transition in these films is found to be an allowed direct transition. The values of Egopt are found to decrease as the CdS content increased. The films with 3 at% CdS content have better decomposition efficiency than undoped TiO2. The films with 6 at% and 9 at% CdS content have decomposition efficiency comparable to that of undoped TiO2, although they have lower band gap. The CdS doped TiO2 could have a better impact on the decomposing of organic wastes. 相似文献
16.
《Applied Surface Science》2011,257(9):4227-4231
TiO2 represents one of the most important sol-gel materials, due to its photocatalytic properties, in the case of both powders and coatings. Nanostructured titania has been reported to be used in many applications in different fields ranging from optics to gas sensor via solar energy. Recent researches point out the existence of new procedures used in order to enhance the efficiency of the photocatalytic process. The metal ion doping is such an example. Two types of 2 wt.% Au containing TiO2 powders have been embedded in sol-gel vitreous TiO2 matrices. Au-doped TiO2 films have been prepared from these sols, by dipping procedure using quartz microscopic slides, as substrates. The relationship between the synthesis conditions and the properties of titania nanosized materials, such as thermal stability, phase composition, crystallinity, and the influence of dopant was investigated. The hydrophilic properties of the films were correlated with their structure, composition and surface morphology. 相似文献
17.
Yumin Liu Aili Wang Min Ren Hui Feng Jun Chen Tingshun Jiang Longbao Yu 《Applied Surface Science》2009,255(16):7427-7433
The evolution of alumina coating layers on rutile TiO2 particle surfaces was investigated starting from aluminum sulfate by a chemical liquid deposition method. The morphology of the alumina coating layers was determined by transmission electron microscopy. The chemical structure and the evolution mechanism of the alumina coating layers on TiO2 surfaces were investigated by Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy, and powder X-ray diffraction techniques. The dispersibility of the alumina-coated TiO2 powders was determined by dynamic laser scattering (DLS) mode. The alumina coating layers existed in boehmite phase, AlOOH, and anchored at the surfaces of TiO2 via Ti-O-Al bond. The formation of alumina coating layers on TiO2 surfaces depended on the pH value of the deposition solution and the alumina loading. After coated by alumina layer, the dispersibility, whiteness, brightness, and light scattering index of the resultant samples were promoted. 相似文献
18.
In this work, TiO2-SiO2-In2O3 composite thin films on glass substrates were prepared by the sol-gel dip coating process. X-ray diffraction (XRD), X-ray fluorescence spectroscopy (XRF) and X-ray photoelectron spectroscopy (XPS) were used to evaluate the structural and chemical properties of the films. UV-vis spectrophotometer was used to measure the transmittance spectra of thin films. The water contact angle (WCA) of thin films during UV/vis irradiation and storage in a dark place was measured by a contact angle analyzer. The results indicated that fabrication of composite film has a significant effect on transmittance and superhydrophilicity of TiO2 films. 相似文献
19.
Yumin Liu Aili Wang Dongzhi Zhang Chunyan Liu Jun Chen Hui Feng Hengping Yao Tingshun Jiang 《Applied Surface Science》2008,254(9):2809-2819
SiO2-coated TiO2 powders were prepared by the chemical deposition method starting from rutile TiO2 and Na2SiO3. The SiO2-coated TiO2 powders were characterized by X-ray photoelectron spectroscopy, Zeta-potential analysis, Fourier transform infrared spectroscopy, and transmission electron microscopy. The evolution of island-like and uniform coating layers was found to depend upon the ratio of Na2SiO3 to TiO2, reaction temperature, and pH. The whiteness and brightness of the SiO2-coated TiO2 powders increased in response to an increase in the SiO2 loading, but there was a maximum value among the light scattering indexes. The SiO2-coated TiO2 powders possessed more negative Zeta potentials than the naked TiO2. The dispersibility of the SiO2-coated TiO2 powders with the continuous and uniform SiO2 coating layers was higher than that of the naked TiO2 and the SiO2-coated TiO2 powders with the island-like SiO2 coating layers. 相似文献
20.
CoPt-TiO2 nanocomposite films were synthesized by rapid thermal annealing of CoPt/TiO2 multilayers. The effects of annealing temperature, annealing time, Ag addition and TiO2 volume fraction on the microstructures and magnetic properties of the CoPt-TiO2 nanocomposite films were studied. Results showed that the ordering degree of CoPt and coercivity of CoPt-TiO2 nanocomposites increased with annealing temperature. Increasing annealing time and Ag addition were able to increase the ordering degree and coercivity of CoPt. However, complete L10-ordering of CoPt at 550 °C annealing was not realized by increasing annealing time up to 30 min and Ag addition up to 30 vol.%. Increasing TiO2 volume fraction at 700 °C annealing did not lead to the change of ordering of CoPt. However, the grain structure of the films changed slightly when TiO2 volume fraction was larger than 56%. The coercivity of the film decreased slightly with the addition of TiO2. 相似文献