共查询到20条相似文献,搜索用时 109 毫秒
1.
乙酰丙酮金属络合物对酸酐固化环氧树脂体系潜伏性促进作用的研究 总被引:4,自引:0,他引:4
A transition metal acetylacetone was studied as latent accelerator in the curing of anhydride cured epoxy resin by DSC, TEA, and rotation viscometer technique. The results reveal that the metal acetylacetone serves as an latent accelerator for anhydride curable epoxy resin system, and the rate of curing is found to increase with enhanced concentrations of the metal chelate. The system provides very fast gel time at 160-180℃ and combined with very good storage stability (> two months). Curing kinetic studies reveal that the overall suring process follows first order kinetics. The electrical,mechanical and thermal properties of cured com-pound of epoxy resin system catalyzed by the MT(acac)n and BDMA accelerator and cured by anhydride was also studied and compared in this paper. 相似文献
2.
偶联剂对玻璃纤维/环氧树脂基复合材料介电性能的影响 总被引:2,自引:0,他引:2
偶联剂对玻璃纤维/环氧树脂基复合材料介电性能的影响陈平刘胜平张明艳(哈尔滨理工大学电工材料系哈尔滨150040)关键词环氧树脂基复合材料,介电性能,偶联剂,浸润性玻璃纤维/环氧树脂基复合材料(GFRP)具有优异的电气和力学性能.然而孔隙的存在强烈地... 相似文献
3.
咪唑固化不同类型环氧树脂的固化特征、固化动力学及其反应活性 总被引:2,自引:0,他引:2
以咪唑为固化剂,对缩水甘油醚型、缩水甘油酯型环氧树脂(简称链型环氧树脂)及脂环环氧树脂的固化特征、固化动力学及反应活性进行了研究.DSC实验结果表明,固化过程均分两阶段进行,链型环氧树脂固化反应表观活化能低于脂环环氧树脂.各树脂第一阶段的表观反应活化能均低于第二阶段活化能.当脂环环氧树脂中混入不同比例的链型环氧树脂后,固化反应速率均较脂环环氧树脂单独固化时快,当链型环氧树脂量大于50%时,更为明显. 相似文献
4.
2-乙基-4-甲基咪唑固化环氧树脂的固化反应机理、动力学及其反应活性 总被引:1,自引:0,他引:1
本文应用DSC和FTIR对2-乙基-4-甲基咪唑固化双酚A二缩水甘油醚型环氧树脂体系的固化反应机理和2-乙基-4-甲基咪唑固化双酚A二缩水甘油醚型、缩水甘油酯与脂环型环氧树脂体系的固化反应特征、动力学及其反应活性进行了研究.结果表明,双酚A二缩水甘油醚型环氧树脂/咪唑体系的固化反应是分两步独立进行的,第一步是加成反应,第二步是催化聚合反应.缩水甘油酯与脂环型环氧树脂(TDE-85)/咪唑体系的固化反应过程也分两步进行,第一阶段反应主要是缩水甘油酯型环氧基进行的加成反应和催化聚合反应,第二阶段主要是脂环型环氧基进行的加成反应.各体系第一阶段的表现反应活化能均低于第二阶段活化能.当TDE-85型环氧树脂中引入缩水甘油醚型环氧树脂后,固化反应速率均较TDE-85环氧树脂单独固化时快. 相似文献
5.
聚苯乙烯—钛酸钡复合材料介电性能的研究 总被引:4,自引:0,他引:4
以聚苯乙烯与化学沉淀法钛酸钡陶瓷为基本组成,采用溶液共混,溶液聚合,表面处理后溶液聚合三种方法进行复合,发现后两种复合的钛酸钡颗粒表面发生界面变化,形成活性界面,使得溶液聚合法和表面处理后溶液聚合所得到的材料具有较低的介电损耗,在高频下能保持较高的介电系数。 相似文献
6.
7.
8.
采用熔融共混及模压的方法制备了碳纳米管(CNT)-高密度聚乙烯(HDPE)复合材料,并用介电谱仪研究了逾渗值附近的导电填料对复合材料体系在不同温度、频率条件下的介电常数、介电损耗、交流电阻率的变化规律。结果表明:复合材料的介电常数、介电损耗均随CNT质量分数增加而逐渐增大;在频率为103~106 Hz,温度为40~130℃时,HDPE基体的介电常数随频率和温度的变化较小,而添加CNT填料的复合材料的介电常数随频率和温度的增加而略微降低。当w(CNT)0.5%时,复合材料的交流电阻率表现出对频率的强烈依赖性;而当w(CNT)0.5%时,在低频处表现出直流特性,在高频处显示出交流电阻率的降低。 相似文献
9.
10.
Avrami法研究环氧树脂/蒙脱土/咪唑纳米复合材料的固化动力学 总被引:6,自引:1,他引:6
运用Flory凝胶化理论和Avrami法研究环氧树脂/有机蒙脱土/咪唑插层型纳米复合体系在不同温度及不同有机蒙脱土用量时的固化动力学。实验表明,随固化温度的提高,Avrami速率常数k值增大,凝胶化时间tg缩短,凝胶点后的t1/2降低,固化速率加快,当固化温度低于90℃时,Avrami指数n值为3左右,而固化温度高于90℃时,n值为2左右。有机蒙脱土的加入,使固化速率加快,但并不改变固化反应的机理,Avrami方程可以很好地描述凝胶点后的固化动力学。 相似文献
11.
M. Jawaid Othman Y. Alothman M. T. Paridah H. P. S Abdul Khalil 《International Journal of Polymer Analysis and Characterization》2014,19(1):62-69
In this work, oil palm empty fruit bunch (EFB) and jute fibers were treated with 2-hydroxy ethyl acrylate (2-HEA) to improve interfacial bonding of oil palm EFB and jute fibers with epoxy matrix. Hybrid composites were fabricated by incorporation of modified oil palm EFB and jute fibers into an epoxy matrix by the hand lay-up technique. Mechanical (flexural and impact) and morphological properties of modified hybrid composites were measured. Results indicated that flexural and impact properties of modified fiber–reinforced hybrid composites improved as compared to untreated hybrid composites due to better fiber/matrix interfacial bonding, which was confirmed by scanning electron microscopy. We confirmed that treated oil palm/jute hybrid composite may be fabricated by advanced techniques such as resin transfer molding, extrusion, and injection molding for industrial applications in the automotive sector. 相似文献
12.
用IR、DSC等分析方法研究了端2-噁唑啉聚环氧丙烷(活性聚醚)与环氧树脂的固化反应,对固化机理作了讨论。并考察了不同分子量活性聚醚对环氧树脂的增韧作用。结果表明,此活性聚醚对环氧树脂增韧效果明显,固化树脂综合性能较好。 相似文献
13.
采用交叉反应研究在促进剂2-甲基咪唑存在下活性酯固化邻甲酚环氧树脂的反 应机理,用傅立叶转换红外(FTIR)原位测量技术,NMR,气-质联用(GC-MS)等 手段研究了模型化合物的反应动力学,并提出了其反应机理。结果表明,在促进剂 2-甲基咪唑存在下活性酯固化邻甲酚环氧树脂的反应是通过分子内机理进行的。 相似文献
14.
15.
To prepare a high-performance epoxy resin with excellent thermal, chemical and corrosion stability, diaminoxanthone(DAX) was used to cure diglycidylether of bisphenol-A(DGEBA)-based epoxy resin and blend of DGEBA with functionalized Fe3O4 nanoparticles. Kinetic parameters of curing and thermal degradation of epoxy resin systems were estimated by differential scanning calorimetry(DSC) and thermogravimetric analysis(TGA), respectively. The 10% weight loss temperature has been increased from 340 °C to 366 °C and there was an increase in the char yield from 32.6% to 45.3% for the above systems. The corrosion performance of epoxy coated carbon steel was examined by potentiodynamic polarization, along with immersion test in 1.0 mol/L HCl solution. The results showed that epoxy resins cured with DAX had low tendency to corrosion. In addition, the cured epoxy resin containing 10% Fe3O4 had higher anticorrosion activity than bare DGEBA system. The results showed that functionalized Fe3O4 nanoparticles enhanced char formation and improved the thermal stability as well as anticorrosion activity of the resin. 相似文献
16.
CuCrO2—CuCr2O4两相共生体系的合成及其对CO—NO反应催化性能的研究 总被引:3,自引:1,他引:2
以柠檬酸络合法制备了CuCrO2-CuCr2O4两相共生体系,并对它的催化性能和TPR行为作了考察,结果表明,两相共生对样品的催化性能及TPR行为有显著的影响,两相共生的样品,在Cu/Cr摩尔比为0.7时,具有较高的催化活性,在TPR过程中,具有尖晶石结构的CuCr2O4首先被原成CuCrO2结构,在更高的温度下后者被还原。 相似文献
17.
18.
19.
Ru/TPPTS催化的水/有机两相对氯硝基苯CO还原为对氯苯胺的研究 总被引:2,自引:0,他引:2
将水溶性膦/钌配合物用于以CO为还原剂的水/有机相对氯硝基苯选择还原为对氯苯胺的反应。考察了CTAB、反应温度和压力等反应转化率和选择性的影响。当130C、4MPa、3mol/NaOH反应条件下反应10h后,对氯硝基苯的转化率可达95%,产物对氯苯胺的选择性达到99%以上。 相似文献
20.
FOX-7的合成和反应机理研究 总被引:11,自引:0,他引:11
以2-甲基咪唑为原料合成出1,1-二氨基-2,2-二硝基乙烯(FOX-7)并进行了结构表征,从中间体过滤母液中分离出副产物2-甲基-4(5)-硝基咪唑和仲班酸.直接合成的2-甲基-4(5)-硝基咪唑和仲班酸,最佳收率分别为67.3%和63.3%.首次提出了一个较为完整而详细的合成FOX-7的反应机理,硝基重排成亚硝酸酯是反应的关键步骤.FOX-7主要是通过2-甲基咪唑→2-甲基-4(5)-二氢-5-咪唑啉酮→2-(二硝基亚甲基)-5,5-二硝基-4-咪唑烷二酮→2-(二硝基亚甲基)-4,5-咪唑烷二酮→FOX-7步骤形成.论述了各中间体形成的详细过程并进行了证明,应用该机理解释了硝化过程中主产物和副产物的变化规律. 相似文献