相似文献
 共查询到20条相似文献,搜索用时 343 毫秒
1.
The magnetic and magnetodielectric properties of Ho0.5Nd0.5Fe3(BO3)4 ferroborate with the competing Ho–Fe and Nd–Fe exchange couplings have been experimentally and theoretically investigated. Step anomalies in the magnetization curves at the spin-reorientation transition induced by the magnetic field Bc have been found. The spontaneous spin-reorientation transition temperature TSR ≈ 8 K has been refined. The measured magnetic properties and observed features are interpreted using a single theoretical approach based on the molecular field approximation and calculations within the crystal field model of the rare-earth ion. Interpretation of the experimental data includes determination of the crystal field parameters for Ho3+ and Nd3+ ions in Ho0.5Nd0.5Fe3(BO3)4 and parameters of the Ho–Fe and Nd–Fe exchange couplings.  相似文献   

2.
The thermally stimulated recombination processes and luminescence in crystals of the lithium borate family Li6(Y,Gd,Eu)(BO3)3 have been investigated. The steady-state luminescence spectra under X-ray excitation (X-ray luminescence spectra), the temperature dependences of the X-ray luminescence intensity, and the glow curves for the Li6Gd(BO3)3, Li6Eu(BO3)3, Li6Y0.5Gd0.5(BO3)3: Eu, and Li6Gd(BO3)3: Eu compounds have been measured in the temperature range 90–500 K. In the X-ray luminescence spectra, the band at 312 nm corresponding to the 6 P J 8 S 7/2 transitions in the Gd3+ ion and the group of lines at 580–700 nm due to the 5 D 07 F J transitions (J = 0–4) in the Eu3+ ion are dominant. For undoped crystals, the X-ray luminescence intensity of these bands increases by a factor of 15 with a change in the temperature from 100 to 400 K. The possible mechanisms providing the observed temperature dependence of the intensity and their relation to the specific features of energy transfer of electronic excitations in these crystals have been discussed. It has been revealed that the glow curves for all the crystals under investigation exhibit the main complex peak with the maximum at a temperature of 110–160 K and a number of weaker peaks with the composition and structure dependent on the crystal type. The nature of shallow trapping centers responsible for the thermally stimulated luminescence in the range below room temperature and their relation to defects in the lithium cation sublattice have been analyzed.  相似文献   

3.
The luminescence and thermally stimulated recombination processes in lithium borate crystals Li6Gd(BO3)3 and Li6Gd(BO3)3:Ce have been studied. The steady-state luminescence spectra under X-ray excitation (X-ray luminescence), temperature dependences of the intensity of steady-state X-ray luminescence (XL), and thermally stimulated luminescence (TSL) spectra of these compounds have been investigated in the temperature range of 90–500 K. The intrinsic-luminescence 312-nm band, which is due to the 6 P J 8 S 7/2 transitions in Gd3+ matrix ions, dominates in the X-ray luminescence spectra of these crystals; in addition, there is a wide complex band at 400–420 nm, which is due to the d → f transitions in Ce3+ impurity ions. It is found that the steady-state XL intensity in these bands increases several times upon heating from 100 to 400 K. The possible mechanisms of the observed temperature dependence of the steady-state XL intensity and their correlation with the features of electronic-excitation energy transfer in these crystals are discussed. The main complex TSL peak at 110–160 K and a number of minor peaks, whose composition and structure depend on the crystal type, have been found in all crystals studied. The nature of the shallow traps that are responsible for TSL at temperatures below room temperature and their relation with defects in the lithium cation sublattice are discussed.  相似文献   

4.
This paper reports on a study of the luminescence emitted by Li6Gd(BO3)3: Ce3+ crystals under selective photoexcitation to lower excited states of the host ion Gd3+ and impurity ion Ce3+ within the 100–500-K temperature interval, where the mechanisms of migration and relaxation of electronic excitation energy have been shown to undergo noticeable changes. The monotonic 10–15-fold increase in intensity of the luminescence band at 3.97 eV has been explained within a model describing two competing processes, namely, migration of electronic excitation energy over chains of Gd3+ ions and vibrational energy relaxation between the 6 I j and 6 P j levels. It has been shown that radiative transitions in Ce3+ ions from the lower excited state 5d 1 to 2 F 5/2 and 2 F 7/2 levels of the ground state produce two photoluminescence bands, at 2.08 and 2.38 eV (Ce1 center) and 2.88 and 3.13 eV (Ce2 center). Possible models of the Ce1 and Ce2 luminescence centers have been discussed.  相似文献   

5.
Magnetic and electron paramagnetic resonance (EPR) properties of EuFe3(BO3)4 single crystals have been studied over the temperature range of 300–4.2 K and in a magnetic field up to 5 T. The temperature, field and orientation dependences of susceptibility, magnetization and EPR spectra are presented. An antiferromagnetic ordering of the Fe subsystem occurs at about 37 K. The easy direction of magnetization perpendicular to the c axis is determined by magnetic measurements. Below 10 K, we observe an increase of susceptibility connected with the polarization of the Eu sublattice by an effective exchange field of the ordered Fe magnetic subsystem. In a magnetic field perpendicular to the c axis, we have observed an increase of magnetization at T < 10 K in the applied magnetic field, which can be attributed to the appearance of the magnetic moment induced by the magnetic field applied in the basal plane. According to EPR measurements, the distance between the maximum and minimum of derivative of absorption line of the Lorentz type is equal to 319 Gs. The anisotropy of g-factor and linewidth is due to the influence of crystalline field of trigonal symmetry. The peculiarities of temperature dependence of both intensity and linewidth are caused by the influence of excited states of europium ion (Eu3+). It is supposed that the difference between the g-factors from EPR and the magnetic measurements is caused by exchange interaction between rare earth and Fe subsystems via anomalous Zeeman effect.  相似文献   

6.
The neodymium ferroborate NdFe3(BO3)4 undergoes an antiferromagnetic transition at T N = 30 K, which manifests itself as a λ-type anomaly in the temperature dependence of the specific heat C and as inflection points in the temperature dependences of the magnetic susceptibility χ measured at various directions of an applied magnetic field with respect to the crystallographic axes of the sample. Magnetic ordering occurs only in the subsystem of Fe3+ ions, whereas the subsystem of Nd3+ ions remains polarized by the magnetic field of the iron subsystem. A change in the population of the levels of the ground Kramers doublet of neodymium ions manifests itself as Schottky-type anomalies in the C(T) and χ(T) dependences at low temperatures. At low temperatures, the magnetic properties of single-crystal NdFe3(BO3)4 are substantially anisotropic, which is determined by the anisotropic contribution of the rare-earth subsystem to the magnetization. The experimental data obtained are used to propose a model for the magnetic structure of NdFe3(BO3)4.  相似文献   

7.
The magnetic properties of the Nd0.5Gd0.5Fe3(BO3)4 single crystal have been studied in principal crystallographic directions in magnetic fields to 90 kG in the temperature range 2–300 K; in addition, the heat capacity has been measured in the range 2–300 K. It has been found that, below the Néel temperature T N = 32 K down to 2 K, the single crystal exhibits an easy-plane antiferromagnetic structure. A hysteresis has been detected during magnetization of the crystal in the easy plane in fields of 1.0–3.5 kG, and a singularity has been found in the temperature dependence of the magnetic susceptibility in the easy plane at a temperature of 11 K in fields B < 1 kG. It has been shown that the singularity is due to appearance of the hysteresis. The origin of the magnetic properties of the crystal near the hysteresis has been discussed.  相似文献   

8.
Optical absorption spectra of trigonal crystal TbFe3(BO3)4 have been studied in the region of 7F65D4 transition in Tb3+ ion depending on temperature (2–220 K) and on magnetic field (0–60 kOe). Splitting of the Tb3+ excited states, both under the influence of the external magnetic field and effective exchange field of the Fe-sublattice, have been determined. Landé factors of the excited states have been found. Stepwise splitting of one of the absorption lines has been discovered in the region of the Fe-sublattice magnetic ordering temperature. This is shown to be due to the abrupt change of equilibrium geometry of the local Tb3+ ion environment only in the excited state of the Tb3+ ion. In general, the magnetic ordering is accompanied by temperature variations of the Tb3+ local environment in the excited states. The crystal field splitting components have been identified. In particular, it has been shown that the ground state (in D 3 symmetry approximation) consists of two close singlet states of A 1 and A 2 type, which are split and magnetized by effective exchange field of the Fe-sublattice. Orientations of magnetic moments of the excited electronic states relative to that of the ground state have been experimentally determined in the magnetically ordered state of the crystal. A pronounced shift of one of absorption lines has been observed in the vicinity of the TbFe3(BO3)4 structural phase transition. The temperature interval of coexistence of the phases is about 3 K.  相似文献   

9.
The HS → LS spin crossover effect (high-spin → low-spin transition) induced by high pressure in the range 45–53 GPa is observed in trivalent Fe3+ ions in the paramagnetic phase of a Gd57Fe3(BO3)4 gadolinium iron borate crystal. This effect is studied in high-pressure diamond-anvil cells by two experimental methods using synchrotron radiation: nuclear resonant forward scattering (NFS) and Fe K β high-resolution x-ray emission spectroscopy (XES). The manifestation of the crossover in the paramagnetic phase, which has no order parameter to distinguish between the HS and LS states, correlates with the optical-gap jump and with the insulator-semiconductor transition in the crystal. Based on a theoretical many-electron model, an explanation of this effect at high pressures is proposed.  相似文献   

10.
The specific heat was measured in the range 0.4–300 K in YFe3(BO3)4, Y0.5Gd0.5Fe3(BO3)4, and GdFe3(BO3)4 single crystals. Sharp anomalies were found at temperatures of first-order structural, second-order antiferromagnetic, and first-order spin-reorientational transitions. A Néel temperature of about 37 K was found to be virtually independent of presence of rare-earth ions, indicating rather weak coupling of Gd and Fe subsystems. The contribution of the magnetic system to specific heat was separated through the scaling procedure allowing determination of the magnetic entropy of Fe and Gd subsystems. At the lowest temperatures, the specific heat in GdFe3(BO3)4 exhibits a Schottky-type anomaly, which is due to Gd3+ eightfold degenerate ground-level splitting by the internal magnetic field of the Fe subsystem of about 7 T. The text was submitted by the authors in English.  相似文献   

11.
Results of a complex investigation of the magnetic, magnetoelectric, and magnetoelastic properties of a SmFe3(BO3)4 single crystal are presented. Samarium iron borate is similar to another easy-plane iron borate, NdFe3(BO3)4, in that it possesses a large value of the magnetic-field-induced polarization (about 500 μC/m2), the sign of which changes when the field direction is changed between axes a and b of the crystal. However, the temperature dependence of the magnetic susceptibility and the field dependence of polarization and magnetostriction of the two compounds are significantly different, which is explained by the weak effect of external magnetic field on the ground-state multiplet of samarium ion, which is characterized by an extremely small value of its g-factor.  相似文献   

12.
This paper reports on the photoluminescence (PL) and time-resolved properties of Ce3+, Eu3+, and Tb3+ in novel LiSr4(BO3)3 powder phosphors. Ce3+ shows an emission band peaking at 420 nm under 350-nm UV excitation. Energy transfer from Ce3+ to Mn2+ takes place in the co-doped samples. Eu3+ shows red emission under near UV excitation. LiSr4(BO3)3:Eu3+ phosphor could be a suitable candidate for phosphor-converted solid state lighting. The luminescence lifetime is 2.13 ms for Eu3+ in LiSr4(BO3)3:0.001Eu3+. As Eu3+ concentration increasing, the decay curves deviate from exponential behavior. Tb3+ shows the strongest 5D47 F5 emission line at 540 nm. Decay curves of 5D47 F5 and 5D37 F5 emission with different Tb3+ concentrations were also measured. Cross-relaxation process is discussed based on the decay curves.  相似文献   

13.
The layered LiNi0.5Mn0.47Al0.03O2 was synthesized by wet chemical method and characterized by X-ray diffraction and analysis of magnetic measurements. The powders adopted the α-NaFeO2 structure. This substitution of Al for Mn promotes the formation of Li(Ni0.472+Ni0.033+Mn0.474+Al0.033+)O2 structures and induces an increase in the average oxidation state of Ni, thereby leading to the shrinkage of the lattice unit cell. The concentration of antisite defects in which Ni2+ occupies the (3a) Li lattice sites in the Wyckoff notation has been estimated from the ferromagnetic Ni2+(3a)–Mn4+(3b) pairing observed below 140 K. The substitution of 3% Al for Mn reduces the amount of antisite defects from 7% to 6.4–6.5%. The analysis of the magnetic properties in the paramagnetic phase in the framework of the Curie–Weiss law agrees well with the combination of Ni2+ (S = 1), Ni3+ (S = 1/2) and Mn4+ (S = 3/2) spin-only values. Delithiation has been made by the use of K2S2O8. According to this process, known to be softer than the electrochemical one, the nickel ions in the (3b) sites are converted into Ni4+ in the high spin configuration, while Ni2+(3a)–Mn4+(3b) ferromagnetic pairs remain, as the Li+(3b) ions linked to the Ni2+(3a) ions in the antisite defects are not removed. The results show that the antisite defect is surrounded by Mn4+ ions, implying the nonuniform distribution of the cations in agreement with previous NMR and neutron experiments.  相似文献   

14.
Cascade of phase transitions in GdFe3(BO3)4 at 156, 37, and 9 K has been detected by specific heat measurements and further studied by Raman scattering and Nd3+ spectroscopic probe method. A weakly first-order structural phase transition at 156 K is followed by a second-order antiferromagnetic ordering phase transition at 37 K and a first-order spin-reorientational phase transition at 9 K.  相似文献   

15.
Epitaxial films of composition (Gd,Nd)3Ga5O12 or (Gd,Y,Nd)3Ga5O12 with a neodymium content varying from 0.3 to 15 at. % are grown by liquid-phase epitaxy from a supercooled PbO-B2O3-based solution melt on Gd3Ga5O12(111) substrates. The optical absorption spectra of the epitaxial films grown are measured in the wavelength range 0.2–1.0 µm. The results of interpreting the absorption bands observed in the spectra are used to construct the energy level diagrams of Nd3+ and Gd3+ ions in the matrices of the epitaxial films.  相似文献   

16.
A high-power diode -pumped Nd3+:YAl3(BO3)4 (Nd:YAB) laser emitting at 1338 nm is described. At the incident pump power of 9.8 W, as high as 734 mW of continuous-wave (CW) output power at 1338 nm is achieved. The slope efficiency with respect to the incident pump power was 9.0%. To the best of our knowledge, this is the first demonstration of such a laser system. The output power stability over 60 min is better than 2.6%. The laser beam quality M 2 factor is 1.21.  相似文献   

17.
The non-doped and doped Nd3+ of Ca9.03Na1.08La0.62(VO4)7 crystals were grown by the Czochralski technique. The effective segregation coefficients of Na+ and Nd3+ ions in the crystal were measured to be about 0.5 and 1.1, respectively. The XPS analysis of Ca9.03Na1.08La0.62(VO4)7 crystal indicates that the vanadium in the crystal is a mixture of V4+ (1.46 at. %) and V5+ (98.54 at. %). The hardness of Nd:Ca9.03Na1.08La0.62(VO4)7 crystal is about 383.1 VDH. Nd:Ca9.03Na1.08La0.62(VO4)7 crystal exhibits similar thermal expansion coefficients along the a (11.2×10-6 K-1) and c (13.7×10-6 K-1) axes, indicating a low thermal expansion anisotropy (αca≈1.2). The qualitative frequency-doubling experiment shows that the doping of Na+ ion can help reduce the scattering of frequency-doubling light, and the intensity of SHG for Ca9.03Na1.08La0.62(VO4)7 crystal is found to be about 3.5 times as large as that of KDP. The polarized absorption and fluorescence spectra are analyzed based on Judd–Ofelt theory, which exhibits that the π-polarized absorption and stimulated emission cross sections are 6.07×10-20 cm2 with an FWHM 12.0 nm at 810 nm and 1.42×10-19 cm2 at 1069 nm, respectively. The fluorescence lifetime is 115 μs at room temperature. All the results indicate that Nd:Ca9.03Na1.08La0.62(VO4)7 crystal is a candidate of self-frequency doubling laser material. PACS 42.62.Fi; 42.70.Mp; 81.10.Fq  相似文献   

18.
Single crystals of yttrium aluminum borate YAl3(BO3)4 doped with manganese ions are studied using electron paramagnetic resonance spectroscopy. It is shown that manganese ions introduced at low concentrations into the sample predominantly occupy yttrium ion sites in the crystal structure. The shape of the electron paramagnetic resonance spectrum unambiguously indicates that the valence of manganese ions in this case is equal to 2+. The parameters of the spin Hamiltonian of Mn2+ ions in the YAl3(BO3)4 matrix are determined at room temperature. The magnitude and sign of the fine structure parameter D allow the conclusion that the YAl3(BO3)4 single crystals doped with manganese ions have a strong crystal field at the yttrium ion sites and easy-axis anisotropy.  相似文献   

19.
The spectral properties of a promising laser material, ternary molybdate Li3Ba2Gd3(MoO4)8:Nd3+, are studied (i.e., its optical absorption spectra, luminescence spectra, kinetic of luminescence decay, and temperature dependence of luminescence). Luminescence of the crystalline matrix is detected, and the temperature dependence of its intensity and reabsorption by neodymium are investigated.  相似文献   

20.
The energies of the ground 4f n levels of tri- and divalent rare-earth ions with respect to the conduction and valence bands of Gd2O2S crystal has been determined. It is shown that the Pr3+, Tb3+, and Eu3+ ions can be luminescence centers in Gd2O2S. The levels of the Nd3+, Dy3+, Er3+, Tm3+, Sm3+, and Ho3+ ions lie in the valence band; therefore, these ions cannot play the role of activators. The ground 4f level of the Ce3+ ion is near the midgap, due to which Ce3+ effectively captures holes from the valence band and electrons from the conduction band and significantly decreases the afterglow level of the Gd2O2S:Pr and Gd2O2S:Tb phosphors.  相似文献   