1.
The infrared (IR) chemiluminescence spectra of CO2 were measured during the steady-state CO + O2 reaction over Pt(110) and Pt(111) surfaces. Analysis of the IR emission spectra indicates that the bending vibrational temperature (TVB), as well as the antisymmetric vibrational temperature (TVAS), was higher on Pt(110) than on Pt(111). On the Pt(110) surface, the highly excited bending vibrational mode compared to the antisymmetric vibrational mode was observed under reaction conditions at low CO coverage (theta(CO) < 0.2) or at high surface temperatures (TS > or = 700 K). This can be related to the activated complex of CO2 formation in a more bent form on the inclined (111) terraces of the Pt(110)(1 x 2) structure. On the other hand, at high CO coverage (theta(CO) > 0.2) or at low surface temperatures (TS < 650 K), TVAS was higher than TVB, which can be caused by the reconstruction of the Pt(110)(1 x 2) surface to the (1 x 1) form with high CO coverage.  相似文献   

2.
Examinations of CO2 formed during steady-state CO oxidation reactions were performed using infrared (IR) chemiluminescence. The CO2 was formed using a molecular-beam method over Pd(110) and Pd(111). The CO2 formation rate is temperature dependent under various partial pressure conditions. The temperature of the maximum formation rate is denoted as TSmax. Analyses of IR emission spectra at surface temperatures higher than TSmax showed that the average vibrational temperature (TVAV) is higher for Pd(111) than for Pd(110). The antisymmetric vibrational temperature (TVAS) is almost equal on both surfaces. These results suggest that the activated CO2 complex is more bent on Pd(111) and straighter on Pd(110). Furthermore, the difference in the TVAV value was small for surface temperatures less than TSmax. The TVAS value was much higher than TVAV on both surfaces. These phenomena were observed only when the surface temperature was lower than TSmax: they became more pronounced at lower temperatures, suggesting that the activated complex of CO2 formation is much straighter on both Pd surfaces than that observed at higher surface temperatures. Combined with kinetic results, the higher CO coverage at the lower surface temperatures is inferred to be related to the linear activated complex of CO2 formation.  相似文献   

3.
The rotational and vibrational energies of product CO(2) in the CO oxidation on Pd(110) surfaces were measured as functions of desorption angles. The antisymmetric vibrational temperature (T(a)) was separately determined from the other vibrational modes from the normalized chemiluminescence intensity. The rotational temperature (T(rot)) and vibrational temperature averaged over the symmetric and bending modes (T(sb)) were then determined by the position and width of spectra by comparison with simulated spectra. On Pd(110)-(1x1), with increases in the desorption angle, T(a), T(sb) and T(rot) decreased in the [001] direction but remained constant in [11[combining macron]0]. However, such anisotropy disappeared when the ratio of exposure of O(2) to that of CO decreased, resulting in a gradual decrease of the three temperatures with increases in the desorption angle. On Pd(110) with missing rows, the three temperatures increased in [001] but decreased in [11[combining macron]0], indicating that the transition state changes with the geometry of the substrate. On Pd(110) with missing rows, T(a) was significantly lower than T(sb), although T(a) was close to or higher than T(sb) on Pd(110)-(1x1). However, there was no significant difference in the angular dependence between T(a), T(sb) and T(rot).  相似文献   

4.
The catalytic CO + NO reaction to form CO2, N2, and N2O has been studied on a Pd(111) surface at pressures up to 240 mbar using in situ polarization modulation infrared reflection absorption spectroscopy (PM-IRAS). At 240 mbar, for a pressure ratio of PCO:PNO = 3:2 and under reaction conditions, besides adsorbed CO, the formation of isocyanate (-NCO) was observed. Once produced at 500-625 K, the isocyanate species was stable within the entire temperature range studied (300-625 K). On the other hand, its formation required a total CO + NO pressure of at least 0.6 mbar, illustrating the importance of in situ infrared experiments under high-pressure conditions. The significance of the isocyanate formation for the CO + NO reaction on Pd(111) is discussed.  相似文献   

5.
Nitric oxide (NO) reduction with carbon monoxide (CO) on the Pd(111) surface was studied under isothermal conditions by molecular beam techniques as a function of temperature, NO:CO beam composition, and beam flux. Systematic experiments were performed under transient and steady state conditions. Displacement of adsorbed CO by NO in the transient state of the reaction was observed at temperatures between 375 and 475 K for all the NO:CO compositions studied. NO accumulation occurs on Pd(111) surface under steady state conditions, below 475 K, due to stronger chemisorption of NO. The steady state reaction rates attain a maximum at about 475 K, nearly independent of beam composition. N2 was found to be the major product of the reduction, along with a minor production of N2O. The production of N2 and N2O indicates molecular and dissociative adsorption of NO on Pd(111) at temperatures up to 525 K. Postreaction TPD measurements were performed in order to determine the nitrogen coverage under steady-state conditions. Finally, the results are discussed with respect to the rate-controlling character of the different elementary steps of the reaction system.  相似文献   

6.
Employing the first-principles pseudopotential plane-wave methods and nudged-elastic-band simulations, we studied the reaction of CO oxidation on Pd-decorated Au(111) surface. We found that the contiguous Pd ensembles are required for the CO + O(2) reaction. Interestingly, Pd dimer is an active site for the two-step reaction of CO+O(2)→OOCO→CO(2)+O, and a low energy barrier (0.29 eV) is found for the formation of the intermediate metastable state (OOCO) compared to the barrier of 0.69 eV on Pd trimer. Furthermore, the residual atomic O in the CO + O(2) reaction can be removed by another CO on Pd dimer with the barrier of 0.56 eV close to the value of 0.52 eV on Pd monomer via Langmuir-Hinshelwood mechanism. The higher energy barriers (0.96 and 0.64 eV) are also found for the CO + O reaction on Pd trimers. The calculated results indicate Pd dimer is highly reactive for CO oxidation by O(2) via association mechanism on Pd-decorated Au(111) surface.  相似文献   

7.
The angular and velocity distributions of desorbing products were analyzed in the course of a catalyzed N2O + CO reaction on Pd(110). The reaction proceeded steadily above 450 K, and the N2 desorption merely collimated sharply along 45 degrees off the surface normal toward the [001] direction. It is proposed that this peculiar N2 desorption is induced by the decomposition of adsorbed N2O oriented along the [001] direction. On the basis of the observation of similar inclined N2 desorption in both NO + CO and N2O + CO reactions, the N2 formation via the intermediate N2Oa dissociation was confirmed in catalytic NO reduction.  相似文献   

8.
The vibrational temperatures of product CO(2) were measured in CO oxidation on Pd(111) as a function of the desorption angle by means of infrared chemiluminescence. The antisymmetric vibration temperature was separately determined from the other vibrational modes from the normalized chemiluminescence intensity. The product CO(2) desorption is sharply collimated along the surface normal. The antisymmetric vibrational temperature increased from 1300 to 1600 K as the desorption angle increased from 0 degrees to 30 degrees , whereas the averaged vibrational temperature over bending and symmetric modes decreased from 2450 to 1530 K. From these angle dependences, an energy partitioning model in repulsive desorption is proposed.  相似文献   

9.
A combination of time-resolved X-ray absorption spectroscopy (XAS), hard X-ray diffraction (HXRD), diffuse reflectance infrared spectroscopy (DRIFTS), and mass spectrometry (MS) reveals a series of size-dependent phenomena at Pd nanoparticles upon CO/(NO+O(2)) cycling conditions. The multitechnique approach and analysis show that such size-dependent phenomena are critical for understanding Pd CO elimination behavior and, particularly, that different Pd(I) and Pd(0) centers act as active species for a size estimated by XAS to be, respectively, below and above ca. 3 nm. The relative catalytic performance of these two noble metal species indicates the intrinsic higher activity of the Pd(I) species.  相似文献   

10.
A Cu(111) surface displays a low activity for the oxidation of carbon monoxide (2CO + O(2) → 2CO(2)). Depending on the temperature, background pressure of O(2), and the exposure time, one can get chemisorbed O on Cu(111) or a layer of Cu(2)O that may be deficient in oxygen. The addition of ceria nanoparticles (NPs) to Cu(111) substantially enhances interactions with the O(2) molecule and facilitates the oxidation of the copper substrate. In images of scanning tunneling microscopy, ceria NPs exhibit two overlapping honeycomb-type moire? structures, with the larger ones (H(1)) having a periodicity of 4.2 nm and the smaller ones (H(2)) having a periodicity of 1.20 nm. After annealing CeO(2)/Cu(111) in O(2) at elevated temperatures (600-700 K), a new phase of a Cu(2)O(1+x) surface oxide appears and propagates from the ceria NPs. The ceria is not only active for O(2) dissociation, but provides a much faster channel for oxidation than the step edges of Cu(111). Exposure to CO at 550-750 K led to a partial reduction of the ceria NPs and the removal of the copper oxide layer. The CeO(x)/Cu(111) systems have activities for the 2CO + O(2) → 2CO(2) reaction that are comparable or larger than those reported for surfaces of expensive noble metals such as Rh(111), Pd(110), and Pt(100). Density-functional calculations show that the supported ceria NPs are able to catalyze the oxidation of CO due to their special electronic and chemical properties. The configuration of the inverse oxide/metal catalyst opens new interesting routes for applications in catalysis.  相似文献   

11.
Surface-nitrogen removal steps were analyzed in the course of a catalyzed NO + H(2) reaction on Pd(110) by angle-resolved mass spectroscopy combined with cross-correlation time-of-flight techniques. Four removal steps, i.e., (i) the associative process of nitrogen atoms, 2N(a) --> N(2)(g), (ii) the decomposition of the intermediate, NO(a) + N(a) --> N(2)O(a) --> N(2)(g) + O(a), (iii) its desorption, N(2)O(a) --> N(2)O(g), and (iv) the desorption as ammonia, N(a) + 3H(a) --> NH(3)(g), are operative in a comparable order. Above 600 K, process (i) is predominant, whereas the others largely contribute below 600 K. Process (iv) becomes significant at H(2) pressures above a critical value, about half the NO pressure. Hydrogen was a stronger reagent than CO toward NO reduction and relatively enhanced the N(a) associative process.  相似文献   

12.
The N(2)O decomposition kinetics and the product (N(2) and CO(2)) desorption dynamics were studied in the course of a catalyzed N(2)O+CO reaction on Pd(110) by angle-resolved mass spectroscopy combined with cross-correlation time-of-flight techniques. The reaction proceeded steadily above 400 K, and the kinetics was switched at a critical CO/N(2)O pressure ratio. The ratio was about 0.03 at 450 K and reached approximately 0.08 at higher temperatures. Below it, the reaction was first order in CO, and negative orders above it. Throughout the surveyed conditions, the N(2) desorption sharply collimated along about 45 degrees off the normal toward the [001] direction. Desorbing N(2) showed translational temperatures in the range of 2000-5000 K. It is proposed that the decomposition proceeds in N(2)O(a) oriented along the [001] direction. On the other hand, the CO(2) desorption sharply collimated along the surface normal, showing a translational temperature of about 1600 K.  相似文献   

13.
Inclined N2 desorption was examined in the course of a catalyzed N2O + D2 (or CO) reaction on Pd(110) by angle-resolved mass spectroscopy combined with cross-correlation time-of-flight techniques. N2 desorption collimated at around 45 degrees off the normal toward the [001] direction in the temperature range of 400-800 K. Its collimation angle and kinetic energy were insensitive to both the surface temperature and surface conditions throughout the kinetic transition. It is proposed that this peculiar N2 desorption is induced by the decomposition of N2O oriented along the [001] direction.  相似文献   

14.
NO co-adsorption with X (X = Na, O, S, and Cl) on Au and Pd(111) surfaces is studied using density functional theory (DFT) calculations to get a deeper insight into the extraordinary sulfur enhanced adsorption on the Au surface. It is found that both electronegative and electropositive adatoms can enhance NO adsorption on Au(111). In Na + NO/Au(111), the strong electrostatic attraction between Na and NO dominates and stabilizes NO adsorption, though Na-induced surface negative charging weakens NO adsorption. In (O, S, Cl) + NO/Au, the electronegative atoms would induce a slight surface distortion and enhance NO adsorption accordingly. NO adsorption on Pd(111) is enhanced by Na, but weakened by electronegative species. We suggest that the unique features of noble metals, i.e., the narrow DOS at the Fermi level (E(F)) and the deep buried d-band center, should play an important role in the promotion of NO adsorption on their surface as the CO case.  相似文献   

15.
To explore the effect of surface contaminants on water chemistry at metallic surfaces, adsorption and decomposition of water monomers on clean and X/Pd(111)(X = C, N and O) surfaces are investigated based on density functional theory calculations. It is revealed that H(2)O binds to Pd(111) surface primarily through the mixing of its 1b(1) with the Pd 4d(z(2)) state. A charge accumulation between the oxygen atom of water and the bound Pd atom is calculated, which is found to be relevant to the H(2)O-Pd interaction. Water adsorption results in a reduction of surface work function and the polarization of the X 2p states. The O-H bond scission of H(2)O on the clean Pd(111) is an energy unfavorable process. In the case of X-assisted O-H bond breaking on X/Pd(111) surfaces, however, the reaction barrier tends to be lower than that on the clean surface and decreases from C/Pd(111) to O/Pd(111). In particular, water decomposition is found to become feasible on O/Pd(111), in agreement with the experimental observations. The calculated barrier is demonstrated to be correlated linearly with the density of X 2p states at the Fermi level. A thorough energy analysis demonstrates that the following geometrical and electronic factors favor the barrier reduction on X/Pd(111) with respect to water decomposition on clean Pd(111): (i) the less deformed structure of water in TS; (ii) the decreased bonding competition between the fragments OH and H. The remarkable decrease of the barrier on O/Pd(111) is revealed to be due to the largest stabilization of the split H atom and the least deformation of water in the TS.  相似文献   

16.
As catalysis research strives toward designing structurally and functionally well-defined catalytic centers containing as few active metal atoms as possible, the importance of understanding the reactivity of small metal clusters, and in particular of systematic comparisons of reaction types and cluster sizes, has grown concomitantly. Here we report density functional theory calculations (GGA-PW91) that probe the relationship between particle size, intermediate structures, and energetics of CO and NO oxidation by molecular and atomic oxygen on Pt(x) clusters (x = 1-5 and 10). The preferred structures, charge distributions, vibrational spectra, and energetics are systematically examined for oxygen (O(2), 2O, and O), CO, CO(2), NO, and NO(2), for CO/NO co-adsorbed with O(2), 2O, and O, and for CO(2)/NO(2) co-adsorbed with O. The binding energies of oxygen, CO, NO, and of the oxidation products CO(2) and NO(2) are all markedly enhanced on Pt(x) compared to Pt(111), and they trend toward the Pt(111) levels as cluster size increases. Because of the strong interaction of both the reactants and products with the Pt(x) clusters, deep energy sinks develop on the potential energy surfaces of the respective oxidation processes, indicating worse reaction energetics than on Pt(111). Thus the smallest Pt clusters are less effective for catalyzing CO and NO oxidation in their original state than bulk Pt. Our results further suggests that oxidation by molecular O(2) is thermodynamically more favourable than by atomic O on Pt(x). Conditions and applications in which the Pt(x) clusters may be effective catalysts are discussed.  相似文献   

17.
丝光沸石负载铂,钯催化剂的NO催化还原性能   总被引:2,自引:0,他引:2  
罗孟飞  朱波 《分子催化》1997,11(1):63-66
丝光沸石负载铂、钯催化剂的NO催化还原性能1)罗孟飞朱波袁贤鑫(杭州大学催化研究所杭州310028)关键词NO催化还原丝光沸石铂钯如何消除NOx对环境造成的污染是当前人们所关心的课题之一,其中催化还原是消除NOx的常用方法[1].近几年,人们对金属离...  相似文献   

18.
CO adsorption on Pd atoms deposited on MgO(100) thin films has been studied by means of thermal desorption (TDS) and Fourier transform infrared (FTIR) spectroscopies. CO desorbs from the adsorbed Pd atoms at a temperature of about 250 K, which corresponds to a binding energy, E(b), of about 0.7 +/- 0.1 eV. FTIR spectra suggest that at saturation two different sites for CO adsorption exist on a single Pd atom. The vibrational frequency of the most stable, singly adsorbed CO molecule is 2055 cm(-)(1). Density functional cluster model calculations have been used to model possible defect sites at the MgO surface where the Pd atoms are likely to be adsorbed. CO/Pd complexes located at regular or low-coordinated O anions of the surface exhibit considerably stronger binding energies, E(b) = 2-2.5 eV, and larger vibrational shifts than were observed in the experiment. CO/Pd complexes located at oxygen vacancies (F or F(+) centers) are characterized by much smaller binding energies, E(b) = 0.5 +/- 0.2 or 0.7 +/- 0.2 eV, which are in agreement with the experimental value. CO/Pd complexes located at the paramagnetic F(+) centers show vibrational frequencies in closest agreement with the experimental data. These comparisons therefore suggest that the Pd atoms are mainly adsorbed at oxygen vacancies.  相似文献   

19.
Combining temperature-programmed reaction measurements, isotopic labeling experiments, and first-principles spin density functional theory, the dependence of the reaction temperature of catalyzed carbon monoxide oxidation on the oxidation state of Pd(13) clusters deposited on MgO surfaces grown on Mo(100) is explored. It is shown that molecular oxygen dissociates easily on the supported Pd(13) cluster, leading to facile partial oxidation to form Pd(13)O(4) clusters with C(4v) symmetry. Increasing the oxidation temperature to 370 K results in nonsymmetric Pd(13)O(6) clusters. The higher symmetry, partially oxidized cluster is characterized by a relatively high activation energy for catalyzed combustion of the first CO molecule via a reaction of an adsorbed CO molecule with one of the oxygen atoms of the Pd(13)O(4) cluster. Subsequent reactions on the resulting lower-symmetry Pd(13)O(x) (x < 4) clusters entail lower activation energies. The nonsymmetric Pd(13)O(6) clusters show lower temperature-catalyzed CO combustion, already starting at cryogenic temperature.  相似文献   

20.
采用共沉淀法制备了耐高温高比表面积的La2O3-Al2O3(LA)材料和CeO2-ZrO2-Y2O3(CZY)储氧材料,并用浸渍法制备了整体式Pd/LA和Pd/CZY汽油车尾气净化三效催化剂,考察了它们的三效催化性能和空燃比性能,并单独通过水煤气变换和CO氧化反应性能的考察,探讨了两种催化剂空燃比窗口扩大的原因.结果表明,Pd/CZY催化剂三效窗口明显较宽,且催化氧化CO的性能明显更优;对于CO+NO反应,Pd/CZY催化剂的活性较高.当反应中逐步通入O2后,抑制了该反应的进行,但CO氧化的转化率升高,而NO转化率降低,直至CO+NO反应完全被抑制,表明CO氧化反应对于抑制催化剂在NO贫燃方向的窗口具有一定的作用.另外,Pd/CZY催化剂上对于水煤气变换反应性能明显优于Pd/LA催化剂,在一定温度下逐步通入O2后,不会抑制水煤气变换反应的发生;当逐步通入NO时,可以促进水煤气变换反应的进行,表明Pd/CZY催化剂在富燃时对扩展CO转化窗口的性能明显优于Pd/LA催化剂.  相似文献   