首页 | 本学科首页   官方微博 | 高级检索  
相似文献
 共查询到20条相似文献,搜索用时 31 毫秒
1.
微流控芯片技术因具有微量、快速、高效和高通量等特点,已成为分析化学领域中的研究热点之一.在微流控芯片中,最常见的可用作芯片的材料为玻璃、石英和各种塑料.玻璃和石英有很好的电渗性和光学性质,可采用标准的刻蚀工艺加工和用化学方法进行表面改性,但加工成本较高,封接难度较大.  相似文献   

2.
Liu J  Wang J  Chen Z  Yu Y  Yang X  Zhang X  Xu Z  Liu C 《Lab on a chip》2011,11(5):969-973
A three-layer poly (methyl methacrylate) (PMMA) electrophoresis microchip integrated with Pt microelectrodes for contactless conductivity detection is presented. A 50 μm-thick PMMA film is used as the insulating layer and placed between the channel plate (containing the microchannel) and the electrode plate (containing the microelectrode). The three-layer structure facilitates the achievement of a thin insulating layer, obviates the difficulty of integrating microelectrodes on a thin film, and does not compromise the integration of microchips. To overcome the thermal and chemical incompatibilities of polymers and photolithographic techniques, a modified lift-off process was developed to integrate Pt microelectrodes onto the PMMA substrate. A novel two-step bonding method was created to assemble the complete PMMA microchip. A low limit of detection of 1.25 μg ml(-1) for Na(+) and high separation efficiency of 77,000 and 48,000 plates/m for Na(+) and K(+) were obtained when operating the detector at a low excitation frequency of 60 kHz.  相似文献   

3.
A sol-gel method was employed to fabricate a poly(methyl methacrylate) (PMMA) electrophoresis microchip that contains a hydrophilic channel wall. To fabricate such a device, tetraethoxysilane (TEOS) was injected into the PMMA channel and was allowed to diffuse into the surface layer for 24 h. After removing the excess TEOS, the channel was filled with an acidic solution for 3 h. Subsequently, the channel was flushed with water and was pretreated in an oven to obtain a sol-gel-modified PMMA microchip. The water contact angle for the sol-gel-modified PMMA was approximately 27.4 degrees compared with approximately 66.3 degrees for the pure PMMA. In addition, the electro-osmotic flow increased from 2.13x10(-4) cm2 V(-1) s(-1) for the native-PMMA channel to 4.86x10(-4) cm2 V(-1) s(-1) for the modified one. The analytical performance of the sol-gel-modified PMMA microchip was demonstrated for the electrophoretic separation of several purines, coupled with amperometric detection. The separation efficiency of uric acid increased to 74,882.3 m(-1) compared with 14,730.5 m(-1) for native-PMMA microchips. The result of this simple modification is a significant improvement in the performance of PMMA for microchip electrophoresis and microfluidic applications.  相似文献   

4.
A simple method based on electric heating wires has been developed for the rapid fabrication of poly(methyl methacrylate) (PMMA) electrophoresis microchips in ordinary laboratories without the need for microfabrication facilities. A piece of stretched electric heating wire placed across the length of a PMMA plate along its midline was sandwiched between two microscope slides under pressure. Subsequently, alternating current was allowed to pass through the wire to generate heat to emboss a separation microchannel on the PMMA separation channel plate at room temperature. The injection channel was fabricated using the same procedure on a PMMA sheet that was perpendicular to the separation channel. The complete microchip was obtained by bonding the separation channel plate to the injection channel sheet, sealing the channels inside. The electric heating wires used in this work not only generated heat; they also served as templates for embossing the microchannels. The prepared microfluidic microchips have been successfully employed in the electrophoresis separation and detection of ions in connection with contactless conductivity detection.  相似文献   

5.
Chen Z  Zhang L  Chen G 《Electrophoresis》2007,28(14):2466-2473
A method based on the in situ polymerization of methyl methacrylate (MMA) has been developed for the rapid fabrication of a novel separation platform, fiber electrophoresis microchip. To demonstrate the concept, prepolymerized MMA molding solution containing a UV initiator was sandwiched between a poly(methyl methacrylate) (PMMA) cover plate and a PMMA base plate bearing glycerol-permeated fiberglass bundles and was exposed to UV light. During the UV-initiated polymerization, the fiberglass bundles were embedded in the PMMA substrate to form fiberglass-packed microchannels. When the glycerol in the fiberglass bundles was flushed away with water, the obtained porous fiberglass-packed channels could be employed to perform electrophoresis separation. Scanning electron micrographs (SEMs) and microscopic images offered insights into the fiber electrophoresis microchip. The analytical performance of the novel microchip has been demonstrated by separating and detecting dopamine and catechol in connection with end-column amperometric detection. The fiber-based microchips can be fabricated by the new approach without the need for complicated and expensive lithography-based microfabrication techniques, indicating great promise for the low-cost production of microchips, and should find a wide range of applications.  相似文献   

6.
We have developed a new method for the high-speed separation and high-sensitivity detection of complex oligosaccharides based on microchip electrophoresis (nu-CE) with light-emitting diode (LED) confocal fluorescence detection. Oligosaccharides labeled with 8-aminopyrene-1,3,6-trisulfonate (APTS) were found to strongly adsorb to the surface of polymethylmethacrylate (PMMA) microchips. Accordingly, three classes of major dynamic coating additives were systematically investigated, and cellulose derivatives were found to specifically suppress such adsorption and allow high-performance separation on PMMA chips. Additive concentration, buffer pH and applied field strength were found to be key factors in the high-performance separation& of APTS-labeled oligosaccharides on PMMA chips. Under optimal conditions, 15 oligosaccharides in dextrin hydrolysate can be separated within 45 s with an electrophoretic separation efficiency of over 400 000 theoretical plates per meter. The relative standard deviation (RSD) values of migration times of fourteen oligosaccharides were less than 0.50% between six different channels, and the detection limit for APTS-labeled glucose was about 1.98 x 10(-8) mol/L or 8.61 amol with a signal-to-noise ratio (S/N) of 3. The high speed, high efficiency and high sensitivity of this micro-CE-based method indicate that it can be widely applied to analysis of complex oligosaccharides.  相似文献   

7.
Yan Xiao 《Talanta》2007,72(4):1316-1321
The separation of three kinds of aminophenol isomers were achieved within 1 min in polyelectrolytes multilayers modified PDMS microchips by layer-by-layer assembly with electrochemical detection (EC). Two polyelectrolytes, poly(dially dimethyl ammonium chloride) (PDDA) and poly(sodium-4-styrene-sulfonate) (PSS) were used to form polyelectrolyte multilayers (PEMs). The surface characteristic of the modified microchip was studied by XPS. The electroosmotic flow (EOF) on PEMs modified PDMS microchips was more stable than that of the native PDMS microchips and the adsorption of samples was greatly reduced on PEMs modified PDMS microchips during the electrophoretic process. The column efficiencies on PEMs modified microchip were increased by 100 times and the signals enhanced by 2 times compared with those of native microchips. The separation conditions such as running buffer pH, running buffer concentration and separation voltage were also optimized.  相似文献   

8.
A novel covalent strategy was developed to modify the poly(dimethylsiloxane) (PDMS) surface. Briefly, dextran was selectively oxidized to aldehyde groups with sodium periodate and subsequently grafted onto amine-functionalized PDMS surface via Schiff base reaction. As expected, the coated PDMS surface efficiently prevented the biomolecules from adsorption. Electro-osmotic flow (EOF) was successfully suppressed compared with that on the native PDMS microchip. Moreover, the stability of EOF was greatly enhanced and the hydrophilicity of PDMS surface was also improved. To apply thus-coated microchip, the separation of peptides, protein and neurotransmitters was investigated in detail. For comparison, these analytes were also measured on the native PDMS microchips. The results demonstrated that these analytes were efficiently separated and detected on the coated PDMS microchips. Furthermore, the relative standard deviations of their migration times for run-to-run, day-to-day, and chip-to-chip reproducibilities were in the range of 0.6-2.7%. In addition, the coated PDMS microchips showed good stability within 1 month.  相似文献   

9.
Nagata H  Tabuchi M  Hirano K  Baba Y 《Electrophoresis》2005,26(14):2687-2691
In this paper, we describe a method for size-based electrophoretic separation of sodium dodecyl sulfate (SDS)-protein complexes on a polymethyl methacrylate (PMMA) microchip, using a separation buffer solution containing SDS and linear polyacrylamide as a sieving matrix. We developed optimum conditions under which protein separations can be performed, using polyethylene glycol (PEG)-coated polymer microchips and electrokinetic sample injection. We studied the performance of protein separations on the PEG-coated PMMA microchip. The electrophoretic separation of proteins (21.5-116.0 kDa) was completed with separation lengths of 3 mm, achieved within 8 s on the PEG-coated microchip. This high-speed method may be applied to protein separations over a large range of molecular weight, making the PEG-coated microchip approach applicable to high-speed proteome analysis systems.  相似文献   

10.
The surface properties of microfluidic devices play an important role in their flow behavior. We report here on an effective control of the surface chemistry and performance of polymeric microchips through a bulk modification route during the fabrication process. The new protocol is based on modification of the bulk microchip material by tailored copolymerization of monomers during atmospheric-pressure molding. A judicious addition of a modifier to the primary monomer solution thus imparts attractive properties to the plastic microchip substrate, including significant enhancement and/or modulation of the EOF (with flow velocities comparable to those of glass), a strong pH sensitivity and high stability. Carboxy, sulfo, and amino moieties have thus been introduced (through the incorporation of methylacrylic acid, 2-sulfoethyl-methacrylate and 2-aminoethyl-methacrylate monomers, respectively). A strong increase in the electroosmotic pumping compared to the native poly(methylmethacrylate)(PMMA) microchip (ca. electroosmotic mobility increases from 2.12 to 4.30 x 10(-4) cm(2) V(-1) s(-1)) is observed using a 6% methylacrylate (MAA) modified PMMA microchip. A 3% aminoethyl modified PMMA microchip exhibits a reversal of the electroosmotic mobility (for example, -5.6 x 10(-4) cm(2) V(-1) s(-1) at pH 3.0). The effects of the modifier loading and the pH on the EOF have been investigated for the MAA-modified PMMA chips. The bulk-modified devices exhibit reproducible and stable EOF behavior. The one step fabrication/modification protocol should further facilitate the widespread production of high-performance plastic microchip devices.  相似文献   

11.
A capillary electrophoresis (CE) microchip made of a new and promising polymeric material: Topas (thermoplastic olefin polymer of amorphous structure), a cyclic olefin copolymer with high chemical resistance, has been tested for the first time with analytical purposes, employing an electrochemical detection. A simple end-channel platinum amperometric detector has been designed, checked, and optimized in a poly-(methylmethacrylate) (PMMA) CE microchip. The end-channel design is based on a platinum wire manually aligned at the exit of the separation channel. This is a simple and durable detection in which the working electrode is not pretreated. H(2)O(2) was employed as model analyte to study the performance of the PMMA microchip and the detector. Factors influencing migration and detection processes were examined and optimized. Separation of H(2)O(2) and L-ascorbic acid (AsA) was developed in order to evaluate the efficiency of microchips using different buffer systems. This detection has been checked for the first time with a microchip made of Topas, obtaining a good linear relationship for mixtures of H(2)O(2) and AsA in different buffers.  相似文献   

12.
Poly(methylmethacrylate) (PMMA) microchip electrophoresis of sodium dodecyl sulfate-protein complexes (SDS-PC) using linear-poly(acrylamide) (L-PA) as a separation matrix was investigated. Prior to electrophoresis, channel walls of PMMA were modified with methylcellulose (MC) to prevent adsorption between channel walls and SDS-PC. Size-based protein separation (SBPS) was successfully performed using the MC-coated microchips with Ferguson plot-fittings. The entangled L-PA solution provided high resolution of peaks of SDS-PC when the concentration of L-PA was increased. Some investigations into the separation mechanism, such as the plot of the logarithm of mobility of each SDS-PC versus the logarithm of the molecular weight of the complex exhibiting linear behavior, indicated that the separation mechanism was dependent on mass discrimination, in accordance with Ogston model.  相似文献   

13.
A novel method based on in-situ surface polymerization of methyl methacrylate (MMA) has been developed for rapid fabrication of poly(methyl methacrylate) (PMMA) electrophoresis microchips with sharp inlet tips. Prepolymerized MMA containing an ultraviolet (UV) initiator was directly sandwiched between a nickel template and a PMMA plate. The image of the relief on the nickel template was precisely replicated in the synthesized PMMA layer on the surface of the commercially available PMMA plate during UV-initiated polymerization at room temperature. The chips were subsequently assembled by thermal bonding of channel plates and cover sheets. The sample was directly introduced into the separation channel through a sharp inlet tip, which was placed in the sample vial, without use of an injection cross. The attractive performance of the novel PMMA microchips has been demonstrated by using contactless conductivity detection for determination of several inorganic ions. Such rapid and simple sample introduction leads to highly reproducible signals with relative standard deviations of less than 5% for peak responses. These new approaches significantly simplify the process of fabricating PMMA devices and show great promise for high-speed microchip analysis.   相似文献   

14.
A novel fiberglass-packed channel in a microchip has been fabricated for flow injection analysis (FIA) based on the in situ polymerization of methyl methacrylate (MMA). MMA prepolymer molding solution containing an ultraviolet initiator was sandwiched between a poly(methyl methacrylate) (PMMA) cover plate and a PMMA base plate bearing a glycerol-permeated fiberglass bundle and exposed to UV light. During the UV-initiated polymerization, the fiberglass bundle was embedded in the PMMA substrate to form a fiberglass-packed microchannel. When the glycerol in the fiberglass bundle was flushed away with water, the obtained porous fiberglass-packed microchannel could serve as an electroosmotic pump and a FIA channel. Scanning electron micrographs offer insights into the fiber-based microchip. The analytical performance of the FIA system has been demonstrated by detecting catechol in connection with end-column amperometric detection. The fiber- based microchips can be fabricated by the new approach without the need for complicated and expensive lithography-based microfabrication techniques, indicating great promise for the low-cost production of microchips, and should find a wide range of applications.  相似文献   

15.
Sung WC  Lee GB  Tzeng CC  Chen SH 《Electrophoresis》2001,22(6):1188-1193
Clinical screening of abnormal chromosomes associated with fragile X syndrome (FXS) demands a high-throughput method including DNA sizing and detection of the amplified products. This study is to explore the use of polymer microchip electrophoresis for the analysis of polymerase chain reaction (PCR) products of fragile X (CGG)n alleles to facilitate a fast exclusion test of FXS. The sequences flanking the CGG-repeat of FMR1 gene was amplified by betaine-PCR and the amplified products were desalted and then analyzed by microchips which were fabricated on poly(methyl methacrylate) (PMMA) substrate. The PCR bands with more than six CGG-repeats in difference could be clearly distinguished in less than 3 min by microchip electrophoresis with a separation length of 6 cm. It was found that the signal was greatly enhanced with the use of both covalent (Cy5) and intercalating dye (TORRO-3), which has never been demonstrated before. We tested the method by reanalysis of twelve samples from males and six samples from females. For female samples with less than six repeat differences, Southern blotting method was performed to confirm or exclude the findings from microchips. It was found that the test results from all male and female samples show a 100% correlation between the microchip electrophoresis and the existing methods.  相似文献   

16.
A novel and simple method based on layer-by-layer (LBL) technique has been developed for the modification of the channel in PDMS electrophoresis microchip to create a hydrophilic surface with a stable EOF. The functional surface was obtained by sequentially immobilizing chitosan and deoxyribonucleic acid (DNA) onto the microfluidic channel surface using the LBL assembly technique. Compared to the native PDMS microchips, the contact angle of the chitosan-DNA modified PDMS microchips decreased and the EOF increased. Experimental conditions were optimized in detail. The chitosan-DNA modified PDMS microchips exhibited good reproducibility and long-term stability. Separation of uric acid (UA) and ascorbic acid (AA) performed on the modified PDMS microchip generated 43,450 and 46,790 N/m theoretical plates compared with 4048 and 19,847 N/m with the native PDMS microchip. In addition, this method has been successfully applied to real human urine samples, without SPE, with recoveries of 97-105% for UA and AA.  相似文献   

17.
A new environmentally friendly method is developed for preventing nonspecific biomolecules from adsorption on poly(dimethylsiloxane) (PDMS) surface via in situ covalent modification. o-[(N-Succinimdyl)succiny]-o'-methyl-poly(ethylene glycol) (NSS-mPEG) was covalently grafted onto PDMS microchannel surface that was pretreated by air-plasma and silanized with 3-aminopropyl-triethoxysilanes (APTES). The modification processes were carried out in aqueous solution without any organic solvent. The mPEG side chains displayed extended structure and created a nonionic hydrophilic polymer brushes layer on PDMS surface, which can effectively prevent the adsorption of biomolecules. The developed method had improved reproducibility of separation and stability of electroosmotic flow (EOF), enhanced hydrophilicity of surface and peak resolution, and decreased adsorption of biomolecules. EOF in the modified microchannel was strongly suppressed, compared with those in the native and silanized PDMS microchips. Seven amino acids have been efficiently separated and successfully detected on the coated PDMS microchip coupled with end-channel amperometric detection. Relative standard deviations (RSDs) of their migration time for run-to-run, day-to-day and chip-to-chip, were all below 2.3%. Moreover, the covalent-modified PDMS channels displayed long-term stability for 4 weeks. This novel coating strategy showed promising application in biomolecules separation.  相似文献   

18.
Chemiluminescence detection was used in capillary electrophoresis integrated on a microchip. Quartz microchips have two main channels and four reservoirs. Dansyl-lysine and -glycine were separated and detected with bis[(2-(3,6,9-trioxadecanyloxycarbony)-4-nitrophenyl]oxalate as peroxyoxalate chemiluminescent reagent. These dansyl amino acids came into contact with the chemiluminescence reagent to produce visible light at the interface between the separation channel and chemiluminescence reagent-containing reservoir. The detection limit (S/N = 3) for dansyl-lysine was 1 x 10(-5) M, which corresponded to the very small mass detection limit of ca. 0.4 fmol. However, the concentration sensitivity in the present system was approximately two orders of magnitude lower than that in the conventional capillary electrophoresis-chemiluminescence detection system. The relative standard deviations of migration time and peak height for dansyl-lysine were 4.2 and 4.5%, respectively. A channel conditioning before every run and an appropriate control of voltages were needed for the reproducible results. The present system had advantages in rapid separation time (within 40 s), small (several 10 pI) and accurate sample injection method using a cross-shaped injector, and simplification and miniaturization of the detection device.  相似文献   

19.
We have developed an analytical method using microchip capillary electrophoresis (microchip CE) for the high-speed separation of fluorescein-labeled salivary components in response to exercise stress. Optimal separation was obtained using a borate buffer at pH 9.5 containing 10 mM beta-cyclodextrin and 1.0% (w/v) methylcellulose. To minimize individual differences in human saliva, such as viscosity, conductivity, and contaminants, the concentration of methylcellulose in the analytical conditions played a key factor. The optimized separation conditions produced identical electropherograms successfully despite of the use of different microchips made from quartz glass or poly-methylmethacrylate (PMMA). In addition, a practical application of bicycle ergometer stress was performed. Some components in human saliva showed a marked decrease after exercise stress.  相似文献   

20.
Sun Y  Kwok YC  Nguyen NT 《Electrophoresis》2007,28(24):4765-4768
Joule heating generated in CE microchips is known to affect temperature gradient, electrophoretic mobility, diffusion of analytes, and ultimately the efficiency and reproducibility of the separation. One way of reducing the effect of Joule heating is to decrease the cross-section area of microchannels. Currently, due to the limit of fabrication technique and detection apparatus, the typical dimensions of CE microchannels are in the range of 50-200 microm. In this paper, we propose a novel approach of performing microchip CE in a bundle of extremely narrow channels by using photonic crystal fiber (PCF) as separation column. The PCF was simply encapsulated in a poly(methyl methacrylate) (PMMA) microchannel right after a T-shaped injector. CE was simultaneously but independently carried out in 54 narrow capillaries, each capillary with diameter of 3.7 microm. The capillary bundle could sustain high electric field strength up to 1000 V/cm due to efficient heat dissipation, thus faster and enhanced separation was attained.  相似文献   