外加铁矿石对哈密低阶煤热解特性影响
引用本文:外加铁矿石对哈密低阶煤热解特性影响.外加铁矿石对哈密低阶煤热解特性影响[J].燃料化学学报,2016,44(2):154-161.
作者姓名:外加铁矿石对哈密低阶煤热解特性影响
作者单位:1. School of Chemical and Environmental Engineering, China University of Mining & Technology(Beijing), Beijing 100083, China; 2. College of Energy and Power Engineering, Inner Mongolia University of Technology, Hohhot 010000, China; 3. School of Civil Engineering, Hebei Institute of Architecture and Civil Engineering, Zhangjiakou 075000, China
基金项目:国家自然科学基金(51074170),新疆维吾尔族自治区科技攻关计划(201532108)和国土资源部煤炭资源勘查与综合利用重点实验室开放研究课题(KF2015-3)项目资助.
摘    要:为探讨铁矿石对哈密低阶煤热解特性影响,采用热重分析仪(thermal gravity analysis/differential thermal gravity,TG/DTG)和实验室固定床反应器(fixed bed)对哈密低阶煤进行热解实验,研究了两种铁矿石对哈密煤热解反应性、热解气和焦油分布规律的影响。利用傅里叶红外光谱(FT-IR)和色谱-质谱分析仪(GC-MS)对焦油中官能团的变化以及焦油中物质组成进行了分析对比。结果表明,当热解温度从室温升高至150℃时,原煤中添加铁矿石的煤样失重速率峰逐渐向高温阶段推移;当热解温度高于450℃时,不同铁矿石对原煤热解的催化作用差异更加明显,且镜铁矿原生矿物质赤铁矿;当两种铁矿石添加量分别为20%时,热解焦油和热解气都能得到较高的收率;对于煤样HM-JT来说,此时焦油产率为7.88%,热解气相产物H_2、CO_2、CH_4、CO产率与未添加镜铁矿的原煤煤样相比分别提高了4.27%、3.76%、4.39%、3.61%。对于煤样HM-CT来说,焦油催化裂解效果一直受到铁矿石添加量的影响。在镜铁矿和赤铁矿添加量分别增加到20%的过程中,煤样热解生成焦油的产率逐渐下降,而轻质焦油产率和轻质焦油分数逐渐增大到6.37%、58.48%、5.34%、56.22%,焦油中氧脱除率分别达到43.16%、36.89%。随着铁矿石的加入,焦油中二甲苯相对含量由4.32%分别降低至3.78%、3.93%,而甲苯相对含量由1.11%升高至1.32%、1.45%;焦油中邻甲酚和二甲酚中分子中的甲基取代基被脱除生成苯酚或甲酚,且镜铁矿对焦油中苯系物和酚类化合物的脱甲基作用强于赤铁矿。

关 键 词:铁矿石  低阶煤  热解  焦油  氧脱除  
收稿时间:2015-09-18

Effect of additive iron ore on pyrolysis characteristics of a low rank coal from Hami
ZHAO Hong-yu,LI Yu-huan,SONG Qiang,L&#,Jun-xin,SHU Yuan-feng,WANG Zi-min,YAN Jie,ZENG Ming,SHU Xin-qian.Effect of additive iron ore on pyrolysis characteristics of a low rank coal from Hami[J].Journal of Fuel Chemistry and Technology,2016,44(2):154-161.
Authors:ZHAO Hong-yu  LI Yu-huan  SONG Qiang  L&#  Jun-xin  SHU Yuan-feng  WANG Zi-min  YAN Jie  ZENG Ming  SHU Xin-qian
Abstract:The effect of iron ore on pyrolysis characteristics of a low rank coal from Hami was explored.By means of thermogravimetric analyzer(TGA),fixed bed reactor,fourier transform infrared spectroscopy(FT-IR),gas chromatograph(GC) and gas chromatography-mass spectrometer(GC-MS),the changes of pyrolysis reactivity,products distribution,the functional groups in the tar and the composition of tar of three coal samples were investigated and analyzed.The results show that when the pyrolysis temperature increases from room temperature to 150℃,the peak of weight loss rate of HM-CT and HM-JT gradually moves to high temperature.When the pyrolysis temperature is more than 450℃,the catalytic effect of different iron ores on coal pyrolysis is more obvious and in the order of specularite> the inherent minerals in HM> hematite.When the two kinds of iron ores added are up to 20%,there is a higher pyrolysis tar and gas yield.The tar yield is 7.88% for HM-JT coal sample and the yield of H2,CH4,CO2 and CO increases by 4.27%,3.76%,4.39% and 3.61%,respectively,compared with HM coal.For HM-CT coal sample,the tar catalytic cracking is influenced by the additive amount of iron ore.As the additive amount of specularite and hematite is increasing to 20%,the yield of tar decreases gradually,while the light tar yield rises to 6.37% and 5.34%,respectively for two iron ores,and the light tar fraction increases to 58.48% and 56.22%,respectively.Besides,the removal of oxygen in tar reaches to 43.16% and 36.89%,respectively.With the addition of iron ore,the relative content of m/p-xylene in tar decreases from 4.32% to 3.78% and 3.93%,respectively for two iron ores,and the relative content of toluene increases from 1.11% to 1.32% and 1.45%,respectively.The methyl substituents of o-cresol and m/p-xylenol molecules in tar are removed to produce phenol or cresol,and the demethylation for benzene series and phenolic compounds in tar on the specularite is stronger than that on the hematite.
Keywords:iron ore  low rank coal  pyrolysis  tar  oxygen removal  
本文献已被 CNKI 等数据库收录!