Thermal and ionic‐conductive behaviors of liquid crystalline polymers with alkali metal salt
Authors:Yosuke Akachi  Kenji Kawamura  Naoyuki Koide
Abstract:In order to investigate the relationship between ionic conductivity and liquid crystallinity, we prepared the main‐chain type polyester having 1,4‐bisstyrylbenzene units and ethyleneoxide chain in the repeating unit. The main‐chain type polyester with lithium salt at the ratio of 0.04 per polymer repeating unit exhibited a smectic phase. However, the polyester with lithium salt (0.11) showed a nematic phase. The ionic conductivity of the polyester with lithium salt increased with increasing lithium salt concentration. The trans‐type polyester exhibited a liquid crystalline phase, while the cis‐type polyester did not show any mesophase. We found that the ionic conductivity of the trans‐type polyester with lithium salt (0.11) was larger than that of the cis‐type polyester with lithium salt (0.11). However, a liquid crystalline phase was found in the side‐chain type polyether with alkoxy chain length of below 12. A smectic phase was induced for the non‐mesomorphic polyethers with lithium salt. The layer spacing of the smectic A phase for the non‐mesomorphic polyether with lithium salt decreased from 55 to 41 Å with increasing temperature. The ionic conductivity of the polyether with lithium salt increased with decreasing the layer spacing. Copyright © 2001 John Wiley & Sons, Ltd.
Keywords:ionic conductivity  liquid crystalline polymer  nematic phase  smectic phase  cis–  trans isomerization
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号