甲基丙烯酸全氟烷基代乙酯对天然橡胶乳液辐射改性研究
引用本文:李俊,耿洪斌,陈庆民.甲基丙烯酸全氟烷基代乙酯对天然橡胶乳液辐射改性研究[J].高分子学报,2006(6):838-840.
作者姓名:李俊  耿洪斌  陈庆民
作者单位:南京大学化学化工学院高分子科学与工程系,配位化学重点实验室,南京,210093
摘    要:天然橡胶的性能与其组成中的C C双键有密切关系,由于C C双键的存在,为天然橡胶的改性提供了便利,大多数天然橡胶的改性方法,如氯化、氢氯化、环化、环氧化、接枝共聚等皆是建立在这一思路基础上的.White等1]认为接枝天然橡胶的目的是提高天然橡胶的机械强度,赋予特殊的功能.作

关 键 词:天然橡胶乳液  甲基丙烯酸全氟烷基乙酯  辐射改性  表征  接触角
收稿时间:2006-03-20
修稿时间:2006-04-12

MODIFICATION OF NATURAL RUBBER LATEX BY RADIATION GRAFTING WITH PERFLUOROALKYLETHYL METHACRYLATE
LI Jun,GENG Hongbin,CHEN Qingmin.MODIFICATION OF NATURAL RUBBER LATEX BY RADIATION GRAFTING WITH PERFLUOROALKYLETHYL METHACRYLATE[J].Acta Polymerica Sinica,2006(6):838-840.
Authors:LI Jun  GENG Hongbin  CHEN Qingmin
Institution:Department of Polymer Science and Engineering, State Key Laboratory of Coordination Chemistry, School of Chemistry and Chemical Engineering, Nanfing University, Nanjing 210093
Abstract:A modification of natural rubber latex(NRL) grafted with perfluoroalkylethyl methacrylate(Zonyl TM) under sensitizer butyl acrylate(BA) by()~(60)Co gamma ray emulsion copolymerization was presented in this paper.The components of the NRL films were studied by Fourier-transfer infrared(FT-IR) spectrometry.The contact angle(CA) analysis showed that the NRL films exhibited a high water contact angle after modification,which changed of 81.1 degree to 110 degree.The surface analysis of X-ray photoelectron spectroscopy(XPS) revealed that the fluorinated segments were preferentially self-organized at the film-air surface.Furthermore,the effect of the Zonyl TM and BA contents on the properties of NRL films was discussed by CA in detail.It showed that the NRL films with 0.94 wt% Zonyl TM and 2.77 wt% or 4.55 wt% BA had better modification effect than the others.
Keywords:Natural rubber latex  Perfluoroalkylethyl methacrylate  Radiation grafted  Characterization  Contact angle