首页 | 本学科首页   官方微博 | 高级检索  
     检索      

原位固相接枝改性碳酸钙/聚丙烯复合材料的制备
引用本文:朱德钦,生瑜,邹寅将,方镇,苏晓芬.原位固相接枝改性碳酸钙/聚丙烯复合材料的制备[J].应用化学,2013,30(12):1411-1416.
作者姓名:朱德钦  生瑜  邹寅将  方镇  苏晓芬
作者单位:(福建省高分子材料重点实验室,福建师范大学材料科学与工程学院 福州 350007)
基金项目:福建省科技厅重大资助项目(2012Y4002);福建省科技厅重点资助项目(2008Y0036);福建省自然科学基金资助(2010J01276)
摘    要:用马来酸酐(MAH)在碳酸钙(CaCO3)表面引入双键,通过原位固相接枝法将聚丙烯蜡(PPW)化学键合在CaCO3表面,制得3种接枝率的CaCO3-MAH-PPW。 将这3种改性CaCO3填充聚丙烯(PP)制备复合材料,研究了PP/CaCO3界面作用对复合材料强度的影响。 结果表明,CaCO3表面经PPW接枝改性后在PP中的分散性提高,与PP相容性变好;随着改性CaCO3表面PPW接枝率的提高,CaCO3与PP之间界面作用逐渐增强。 当PPW接枝率为4.48 mg PPW/g CaCO3时,CaCO3与PP之间的界面作用最强,复合材料拉伸强度下降最小,杨氏模量提升最大,当m(PP)∶m(CaCO3)=100∶50时,杨氏模量达0.86 GPa,是纯PP的1.63倍;而PPW化学接枝率为2.49 mg PPW/g CaCO3时,CaCO3与PP之间的界面作用适中,复合材料缺口冲击强度提升最大,且当m(PP)∶m(CaCO3)=100∶10时,缺口冲击强度达3.91 kJ/m2,是纯PP的1.35倍。

关 键 词:聚丙烯  碳酸钙  原位固相接枝改性  界面作用  材料强度  
收稿时间:2013-03-18
修稿时间:2013-05-17

Preparation of Polypropylene Composites Filled with Surface-modified Calcium Carbonate by in-situ Solid Phase Grafting
ZHU Deqin,SHENG Yu,ZOU Yinjiang,FANG Zhen,SU Xiaofen.Preparation of Polypropylene Composites Filled with Surface-modified Calcium Carbonate by in-situ Solid Phase Grafting[J].Chinese Journal of Applied Chemistry,2013,30(12):1411-1416.
Authors:ZHU Deqin  SHENG Yu  ZOU Yinjiang  FANG Zhen  SU Xiaofen
Institution:(Fujian Key Laboratory of Polymer Materials,College of Materials Science and ; Engineering of Fujian Normal University,Fuzhou 350007,China)
Abstract:The surface of calcium carbonate(CaCO3) was firstly pretreated with maleic anhydride(MAH) to introduce active double bond groups, then grafted chemically by polypropylene wax(PPW) via in-situ solid phase grafting to increase its compatibility with polypropylene. Three kinds of modified CaCO3 with different chemical grafting ratio of PPW were prepared by changing experimental conditions, and their PP-based composites were produced. The effects of interfacial interaction between CaCO3-MAH-PPW and PP matrix on the strength of PP-based composite filled with modified CaCO3 were studied. The results show that the dispersibility of CaCO3-MAH-PPW in PP is improved, suggesting an improved compatibility between them. With the improvement of grafting ratio of PPW on the surface of CaCO3, the interfacial interaction between CaCO3 and PP increases gradually. When the grafting ratio of PPW is 4.48 mg PPW/g CaCO3, the interfacial interaction between CaCO3 and PP is strongest and the decrease of tensile strength of composites is the least, the young′s modulus increases most at the same time. When m(PP)∶m(CaCO3)=100∶50, the young′s modulus reaches 0.86 GPa, which is the 1.63 times of PP′s. When the grafting ratio of PPW is 2.49 mg PPW/g CaCO3, the interfacial interaction between CaCO3 and PP is suitable and the notch impact strength of composites improves the most. And when m(PP)∶m(CaCO3)=100∶10, its notch impact strength is 3.91 kJ/m2, which is the 1.35 times of PP′s.
Keywords:polypropylene  calcium carbonate  solid phase grafting in-situ  interfacial interaction  material strength
点击此处可从《应用化学》浏览原始摘要信息
点击此处可从《应用化学》下载免费的PDF全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号