钴掺杂Sr1.5La0.5MnO4的合成及高温电化学性能研究
引用本文:范宇航,孙丽萍,霍丽华,赵辉,Jean-Marc Bassat,Aline Rougier,S&#;bastien Fourcade,Jean-Claude Grenier.钴掺杂Sr1.5La0.5MnO4的合成及高温电化学性能研究[J].无机化学学报,2013,29(18).
作者姓名:范宇航  孙丽萍  霍丽华  赵辉  Jean-Marc Bassat  Aline Rougier  S&#;bastien Fourcade  Jean-Claude Grenier
作者单位:黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080,黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080,黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080,黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080,CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France,CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France,CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France,CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France
基金项目:国家自然科学基金(No.51302069,51372073)、高等学校博士学科点专项科研基金(No.20132301110002)和人事部留学人员科技活动择优项目(No.2014-240)资助。
摘    要:采用EDTA-柠檬酸法合成了中温固体氧化物燃料电池阴极材料Sr1.5La0.5Mn1-xCoxO4(SLMCOx),并利用粉末X射线衍射(XRD)、X射线光电子能谱(XPS)以及电化学交流阻抗谱(EIS)进行表征。结果表明,该材料与Ce0.9Gd0.1O1.95(CGO)在1 200℃烧结12 h不发生化学反应。随着Co掺入量的增加,氧化物中Mn3+和Co2+含量增多,晶格氧含量降低,晶格畸变率增大。交流阻抗谱(EIS)测试结果显示,钴的掺杂明显降低电极的极化电阻,其中Sr1.5La0.5Mn0.7Co0.3O4阴极在700℃空气中的极化电阻为0.62 Ω·cm2,明显小于Sr1.5La0.5MnO4阴极在750℃的极化电阻(1.5 Ω·cm2),表明钴掺杂的Sr1.5La0.5Mn1-xCoxO4是一种潜在的IT-SOFC阴极材料。

关 键 词:中温固体氧化物  燃料电池  阴极材料

Synthesis and High Temperature Electrochemical Properties of Co-doped Sr1.5La0.5MnO4
FAN Yu-Hang,SUN Li-Ping,ZHAO Hui,HUO Li-Hu,Jean-Marc Bassat,Aline Rougier,S&#;bastien Fourcade and Jean-Claude Grenier.Synthesis and High Temperature Electrochemical Properties of Co-doped Sr1.5La0.5MnO4[J].Chinese Journal of Inorganic Chemistry,2013,29(18).
Authors:FAN Yu-Hang  SUN Li-Ping  ZHAO Hui  HUO Li-Hu  Jean-Marc Bassat  Aline Rougier  S&#;bastien Fourcade and Jean-Claude Grenier
Institution:Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China,Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China,Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China,Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China,CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France,CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France,CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France and CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France
Abstract:
Keywords:intermediate temperature solid oxide  fuel cells (IT-SOFCs)  cathode material
点击此处可从《无机化学学报》浏览原始摘要信息