摘    要:报道了一种稳定的白色有机薄膜电致发光器件.电流效率6cd/A,在电流密度20mA/cm2驱动下,亮度为1026cd/m2;最高亮度21200cd/m2,色度(x=0.32,y=0.40).该器件具有较平稳的效率电流关系,即具有弱的电流荧光猝灭.初始亮度100cd/m2下,半亮度寿命达22245h.

关 键 词:有机电致发光器件  白光器件  稳定性
文章编号:1000-7032(2005)02-0149-04
收稿时间:2004-08-25
修稿时间:2004年8月25日

White Organic Light Emitting Diode and Its Stability
ZHANG Zhi-lin,JIANG Xue-Yin,ZHU Wen-qing,XU Shao-hong.White Organic Light Emitting Diode and Its Stability[J].Chinese Journal of Luminescence,2005,26(2):149-152.
Authors:ZHANG Zhi-lin  JIANG Xue-Yin  ZHU Wen-qing  XU Shao-hong
Institution:School of Materials Science & Engineering, Shanghai University, Shanghai 201800, China
Abstract:Three kinds of white organic light emitting devices (WOLED) were constructed:Cell-S, with a single-doped red dye in the light emitting layer(EML); Cell-D, with both red and blue dyes doped in a single EML(double-doped); Cell-T, with red and blue dyes doped in one EML and a green dye in another layer(triple-doped).The structure of these devices are as follows:Cell-S:CuPc(12nm)/NPB(40nm)/ADN:DCJTB(50nm)/Alq3(12nm)/LiF(4nm)/Al; Cell-D:CuPc(12nm)/NPB(40nm)/ADN:DCJTB:TBPe(50nm)/Alq3(12nm)/LiF(4nm)/Al; Cell-T:CuPc(12nm)/NPB(40nm)/ADN:DCJTB:TBPe(50nm)/Alq3:C545(12nm)/LiF(4nm)/Al. Experimentals indicate that the Cell-T and Cell-D show much higher luminance and efficiency than that of Cell-S.The Cell-T achieves a current efficiency of 6cd/A and a power efficiency 3.11 lm/W, which is twice that of Cell-S, 1026cd/m2 at driving current 20mA/cm2 and maximum luminance 21200cd/m2, In addition, it exhibits a flatcd/Avs. current density response, indicating a weak current induced fluorescence quenching. At the driving current 12mA/cm2, at the initial luminance of 575cd/m2, the half life is over 3862h for Cell-T, for an initial luminance of 100cd/m2, the half life (t/2) is projected to be 22245h with a little change of EL spectrum before and after aging.