Annealing behavior of gel‐spun polyethylene fibers at temperatures lower than needed for significant shrinkage
Authors:Wenbing Hu  Alexander Buzin  Jar‐Shyong Lin  Bernhard Wunderlich
Abstract:The annealing at 373 K of ultrastrong, gel‐spun polyethylene (PE) has been studied. At this temperature, the fibers show no significant shrinkage. Still, a significant decrease in the mechanical properties is observed. The fibers have been analyzed with differential scanning calorimetry (DSC), temperature‐modulated differential scanning calorimetry (TMDSC), atomic force microscopy (AFM), and small‐angle X‐ray scattering (SAXS). During the annealing, the glass transition of the intermediate phase is exceeded, as shown by DSC. When split for structure analysis by AFM, the annealed fibers undergo plastic deformation around the base fibrils instead of brittle fracture. The quasi‐isothermal TMDSC experiments are compared to the minor structural changes seen with SAXS and AFM. The loss of performance of the PE fibers at 373 K is suggested to be caused by the oriented intermediate phase, and not by major changes in the structure or morphology. The overall metastable, semicrystalline structure is shown by TMDSC to posses local regions that can melt reversibly. © 2003 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 41: 403–417, 2003
Keywords:gel‐spun polyethylene fibers  annealing  differential scanning calorimetry (DSC)  atomic force microscopy (AFM)  temperature‐modulated differential scanning calorimetry (TMDSC)  SAXS  structural changes  properties
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号