Oxo-biodegradable polyolefins show continued and increased thermal oxidative degradation after exposure to light
Authors:Nils B Vogt  Emil Arne Kleppe
Institution:a Siamalgamate Co., Ltd., 66 Soi Romklao 58, Romklao Road, Klongsampravet, Lad Krabang, Bangkok 10520, Thailand
b Nor-X Industry AS, Gursken Industriområde, 6082 Gursken, Norway
Abstract:Samples of polyethylene (PE) and polypropylene (PP) with 2% Renatura™ pro-oxidant additive were subjected to varying times of weathering (UVCON; ISO 4892-3), transferred to dark thermal exposure (at 70 °C) and the subsequent degradation monitored by measuring elongation at break and tensile strength during intervals up to 45 days. The results demonstrate that the oxidative degradation, after initial light exposure, continues more rapidly in the dark thermal conditions and that increased exposure to light increases thermal oxidative degradation.
Keywords:Oxo-biodegradation  Photo-oxo-degradation  Thermal degradation  Iron-based oxo-biodegradable additive  Landfill  Composting
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号