Changes in the mechanical properties of compression moulded samples of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) degraded by Streptomyces omiyaensis SSM 5670
Authors:Élida B Hermida  O Yashchuk  SS Miyazaki
Institution:a CONICET, Av.Rivadavia 1917, 1033 Buenos Aires, Argentina
b Institute of Technology “Prof. Jorge A. Sabato”, UNSAM-CNEA, Av.Gral Paz 1499, B1650KNA San Martin, Argentina
c Department of Materials (CNEA), Av.Gral Paz 1499, B1650KNA San Martin, Argentina
d Department of Applied Biology and Foods, Faculty of Agronomy, University of Buenos Aires, Av. San Martín 4453, 1417 Buenos Aires, Argentina
Abstract:Streptomyces omiyaensis SSM 5670 was characterized by its ability to use compression moulded samples of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) as its sole carbon source. Biodegradation of PHBV in liquid mineral salts medium was investigated using scanning electron microscopy, gravimetric measurements, capillary viscometry, tensile testing and wide angle X-ray spectroscopy. The biodegradation of PHBV proceeds via surface erosion mechanism, resulting in the formation of pits by microbial attack. PHBV specimens lost about 45% of their original weight after 45 days of exposure. During the degradation process the elastic modulus reduces less than 10%. The formation of pores and microcracks initiated at the degraded pits determines the reduction of the elongation and stress at break. However, the true stress at break is practically independent of the degradation time. No significant changes of PHBV molecular weight or crystallinity were observed during biodegradation. The polymer chain cleavage occurred only at the specimen surface and does not discriminate between crystalline and amorphous states.
Keywords:Biodegradation  Tensile testing  Surface erosion  Poly(3-hydroxybutyrate)  Poly(3-hydroxybutyrate-co-3-hydroxyvalerate)  Streptomyces sp