Studying the process of ionization of hydrogen in conditions of its forced delivery to a porous nickel oxide electrode
Authors:A V Semykin  I A Kazarinov  E A Khomskaya
Institution:(1) Saratov State University, ul. Astrakhanskaya 83, Saratov, 410012, Russia
Abstract:The hydrogen ionization process is studied experimentally on an industrial sintered nickel oxide electrode in models of sealed nickel-metal hydride batteries. It is shown that the hydrogen ionization rates that are reached during overcharge by high current densities in conditions of forced gas delivery into the electrode pores (up to 40 mA cm?2) exceed the self-discharge rate of a nickel-hydrogen battery by two orders of magnitude. Up to 70% of hydrogen delivered into the compact assembly block undergoes ionization during forced charge of models of sealed nickel-metal hydride batteries with a closed hydrogen cycle. Two independent methods (potentiostatic and manometric) are used to determine the relationship between rates of hydrogen ionization with the degree of the electrode filling with gas and perform estimation of the process intensity at a unit reaction surface. It is established that, in conditions of forced gas delivery, practically all the hydrogen oxidation current is generated at the surface of the nickel oxide electrode beneath thin films of an electrolyte solution at the rate of 4–5 mA cm?2. It is shown that the hydrogen oxidation rate on a nickel oxide electrode filled in part by gas is independent of the electrode potential, probably because of a tangible contribution made by diffusion limitations to the overall hampering of the process.
Keywords:porous nickel oxide electrode  ionization  hydrogen cycle  sealed battery  interelectrode gap
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号