Effects of oxidation pretreatment temperature on Kovar used as CO_2 reforming catalyst
Authors:Sharon Rose de la Rama  Hiroshi Yamada  Tomohiko Tagawa
Affiliation:Department of Chemical Engineering, Nagoya University Chikusa, Nagoya 464-8603, Japan
Abstract:
The effect of oxidation pretreatment temperature (500~1 000 ℃) on the catalytic activity of Kovar applied on hydrocarbon CO2 reforming was examined. Catalytic performance evaluation using tetradecane at 800 ℃ with 70 μmol/s CO2 revealed 700 and 1 000 ℃ as the best pre-oxidation temperature in producing CO and H2, respectively. XRD and SEM-EDX analyses showed that a separate metal oxide layer composed of iron oxide (Fe2O3 and F3O4), nickel, cobalt, and possibly their respective oxides started to form when oxidation was conducted at 700 ℃ or higher.The presence of iron enhanced the stability of nickel in the structure while the compact structure of Fe3O4 resulted into the formation of a thick and rigid metal oxide layer on the surface of the Kovar tube. The strong physical bond between the metal oxide layer and Kovar tube provided the catalyst good mechanical strength and consequently good catalytic activity.
Keywords:CO reforming catalyst  Kovar  oxidation pretreatment
本文献已被 CNKI 等数据库收录!
点击此处可从《燃料化学学报》浏览原始摘要信息
点击此处可从《燃料化学学报》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号