Abstract: | Star poly(methyl methacrylate)s (P*) of various arm lengths and core sizes were synthesized in high yields by the polymer linking reaction in Ru(II)‐catalyzed living radical polymerization. The yields of the star polymers were strongly dependent on the reaction conditions and increased under the following conditions: (1) at a higher overall concentration of arm chains ([P*]), (2) with a larger degree of polymerization (DP) of the arm chains (arm length), and (3) with a larger ratio (r) of linking agents to P* (core size). In particular, the yields sharply increased in a short time at a higher temperature, in a polar solution, and at a higher complex concentration after the addition of linking agents. These star polymers were then analyzed by multi‐angle laser light scattering to determine the weight‐average molecular weight (3.8 × 103 to 1.5 × 106), the number of arm chains per molecule (f = 4–63), and the radius of gyration (Rz = 2–22 nm), which also depended on the reaction conditions (e.g., f and Rz increased as [P*], DP, and r increased). Small‐angle X‐ray scattering analyses of the star polymers showed that they consisted of spheres for which the radius of the microgel core was 2.7 nm. © 2002 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 40: 2245–2255, 2002 |