Preparation and electrorheological properties of triethanolamine-modified TiO2
Authors:J.G. Cao
Affiliation:The State Key Laboratory of Applied Surface Physics, Department of Physics, Fudan University, Shanghai 200433, China
Abstract:
The high molecular dielectric dipole moment of doping material is promising to improve the electrorholegical (ER) effect. It is found that triethanolamine (the molecular dipole moment of triethanolamine is 3.48)-modified TiO2 has good ER properties. Under 5 kV/mm external electric field, the yield stress is 32.6 kPa, which is about 50 times higher than that of pure TiO2 and the leaking electric current density is lower than 16 μA/cm2. The sedimentation rate is about 98% in 20 days.
Keywords:Electrorheological fluids   Molecular dipole moment