(1) Institute of Technical Physics, Czechosl. Acad. Sci., Prague
Abstract:
On the basis of the correlation of diffraction data (intensity and width) of a precipitate with the intensity of reflection of a matrix solid solution it is shown that the change in primary extinction during the decomposition of a solid solution of Agin Alis caused by the precipitation of the phase Ag2Aland not by the production of lattice defects (zones, stacking faults).
I. Al-Ag
( ) , Ag Al Ag2Al, ( , ).
Reported in part at the VIth Scientific Technical Conference on the Application of X-rays held in Leningrad in 1958.The author thanks M. Mikovský for preparing the single crystals of the alloy Al-Ag having a high primary extinction and J. Laek and Prof. J. Bedná for carefully checking their homogeneity and chemical composition.