Crystalline titanium dichloride—an active catalyst in ethylene polymerization. II. Polymer structure,polymerization variables,and scope |
| |
Authors: | C. J. Benning W. R. Wszolek F. X. Werber |
| |
Abstract: | Polymerization of ethylene with ball-milled titanium dichloride leads to a completely linear polymer with terminal unsaturation corresponding to approximately one carbon–carbon double bond per molecule. Polymerization rate is first-order in both monomer and catalyst concentration at 140°C. Due to a thermal deactivation of the catalyst, the polymerization rate falls sharply with temperature above 180°C. Propylene and butene-1 will copolymerization with ethylene in this system, propylene more efficiently than butene-1. Evidence for copolymerization of trans-2-butene, but not of the cis-isomer or of isobutene, in trace concentrations is presented. Propylene is homopolymerized to a product low in isotactic content. The significance of the structural and (limited) kinetic data in terms of the mechanism of polymerization are discussed. |
| |