Abstract: | Electron-microscopic texture and physical properties of a styrene–butadiene–styrene (SBS) block copolymer obtained by casting from toluene, carbon tetrachloride, ethyl acetate, and methyl ethyl ketone are discussed. Two peaks are observed in the mechanical loss (tan delta;) curve at ?70 and 100°C which are attributed to segmental motion of polybutadiene and polystyrene, respectively. The polybutadiene peak heights are in the order of solubility in the solvent used; the polystyrene peak heights are in converse order. In addition to these peaks, a third peak is observed at 10°C for specimens cast from ethyl acetate or methyl ethyl ketone. A transition corresponding to this peak is also noticed in thermal analysis. It is proposed that aggregation of styrene blocks is relatively incomplete in specimens cast from solution in poor solvents. |