Wet oxidation behaviors of Hi-Nicalon fibers
Authors:Shoujun Wu  Laifei Cheng  Litong Zhang  Yongdong Xu  Jun Zhang  Hui Mei
Institution:National Key Laboratory of Thermostructure Composite Materials, Northwestern Polytechnical University, Xi’an Shaanxi 710072, PR China
Abstract:Wet oxidation behaviors of Hi-Nicalon fibers were investigated in environment of PH2O:O2:Ar=14:8:78kPa with a slow gas flow rate of 3.5 cm s−1 above 1300 °C for 1 h. Experimental results indicated that oxidized Hi-Nicalon fibers were covered by silica. The weight gains and surface micromorphologies were strongly affected by temperature. Below 1500 °C, the surface of the oxidized fibers were rough-hewn and cracked, and there were no changes detected in fiber diameter. After oxidation at 1600 °C, the silica locally spalled and the fiber swelled in diameter. The Young-Laplace equation was applied to interpret surface micromorphologies change during wet oxidation of the specimens. The cracks in silica produced by oxidation and the microcrystal growth of the fibers at high temperature were considered for the strength degradation of the fibers.
Keywords:Hi-Nicalon fiber  Wet oxidation  Microstructure  Tensile strength
本文献已被 ScienceDirect 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号