Abstract: | Investigation on the Formation of Double-ring Silicate Ions in Trimethyl-(2-hydroxyethyl) Ammoniumsilicate Solutions The formation of double-four ring silicate ions have been investigated after the mixing of Tetramethoxysilan with Trimethyl-(2-hydroxyethyl)ammoniumhydroxide in the molar ratio 1:1 (cSiO2 = 1.53 mol · kg?1) in dependence of the time. About 20–30% of the rapid hydrolysing esters has reacted to double-three- and double-four ring ions after a short time, whereas 70–80% first condense to oligomers and polymers. In the further course of reaction also the oligomers, the polymers and the intermediate formed double-three-ring species changes to double-four-ring ions. After three hours about 90% of the silicon dioxide is in the double-four-ring constitution. |