Thermal properties of pitch-polymer compositions and derived activated carbons |
| |
Authors: | Grzegorz Makomaski Wies?awa Ciesińska Janusz Zieliński |
| |
Affiliation: | 1. Institute of Chemistry in Plock, Warsaw University of Technology, Lukasiewicza 17, 09-400, Plock, Poland
|
| |
Abstract: | The evaluation of the possibilities to use coal-tar pitch modified with waste poly(ethylene terephthalate) or phenol?Cformaldehyde resin for the preparation of activated carbons was carried out. The measurement of thermal analysis (DSC), softening point, coking value, content of components insoluble in toluene and quinoline of pitch-polymer compositions were carried out. Coal-tar pitch and pitch-polymer compositions were carbonized and activated with steam at 800?°C to 50?% burn-off. For the obtained activated carbons the determination of thermal analysis (DSC), BET surface area on the basis of volumetric low-temperature adsorption of nitrogen, mesopore, and micropore volume from benzene adsorption/desorption isotherms (gravimetric McBain-Bakr method) were carried out. |
| |
Keywords: | |
本文献已被 SpringerLink 等数据库收录! |
|