Multiblock copolymers of poly(2,5‐benzophenone) and disulfonated poly(arylene ether sulfone) for proton‐exchange membranes. I. Synthesis and characterization |
| |
Authors: | Hang Wang Anand S. Badami Abhishek Roy James E. McGrath |
| |
Affiliation: | 1. Macromolecules and Interfaces Institute, Virginia Polytechnic Institute and State University, Blacksburg, Virginia 24061;2. Macromolecules and Interfaces Institute, Virginia Polytechnic Institute and State University, Blacksburg, Virginia 24061Macromolecules and Interfaces Institute, Virginia Polytechnic Institute and State University, Blacksburg, Virginia 24061 |
| |
Abstract: | ![]() Nanophase‐separated, hydrophilic–hydrophobic multiblock copolymers are promising proton‐exchange‐membrane materials because of their ability to form various morphological structures that enhance transport. A series of poly(2,5‐benzophenone)‐activated, telechelic aryl fluoride oligomers with different block molecular weights were successfully synthesized by the Ni(0)‐catalyzed coupling of 2,5‐dichlorobenzophenone and the end‐capping agent 4‐chloro‐4′‐fluorobenzophenone. These telechelic oligomers (hydrophobic) were then copolymerized with phenoxide‐terminated, disulfonated poly(arylene ether sulfone)s (hydrophilic) by nucleophilic, aromatic substitution to form hydrophilic–hydrophobic multiblock copolymers. High‐molecular‐weight multiblock copolymers with number‐average block lengths ranging from 3000 to 10,000 g/mol were successfully synthesized. Two separate glass‐transition temperatures were observed via differential scanning calorimetry in the transparent multiblock copolymer films when each block length was longer than 6000 g/mol. Tapping‐mode atomic force microscopy also showed clear nanophase separation between the hydrophilic and hydrophobic domains and the influence of the block length as it increased from 6000 to 10,000 g/mol. Transparent and creasable films were solvent‐cast and exhibited moderate proton conductivity and low water uptake. These copolymers are promising candidates for high‐temperature proton‐exchange membranes in fuel cells, which will be reported separately in part II of this series. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 284–294, 2007 |
| |
Keywords: | atomic force microscopy (AFM) block copolymers fuel cells morphology multiblock copolymers phase separation poly(arylene ether sulfone) poly(p‐phenylene)exchange membranes synthesis |
|
|