Abstract: | Aromatic polyamides (aramids) having pendant t-butyl group were synthesized by the direct polycondensation of 5-t-butylisophthalic acid with various aromatic diamines in N-methyl-2-pyrrolidone (NMP) using triphenyl phosphite and pyridine as condensing agents. The aramids having inherent viscosities of 0.6–2.4 dL/g were obtained in quantitative yields. These polymers were readily soluble in various solvents such as NMP,N,N-dimethylacetamide, dimethyl sulfoxide, and pyridine, and gave transparent, tough and flexible films by casting from the NMP solutions. The aramids had glass transition temperatures between 250 and 330°C, and started to lose weight around 350°C, with 10% weight loss being recorded at about 450°C in air. |