Abstract: | Polystyrene-block-polybutadiene-block-poly(ϵ-caprolactone) SBC triblock copolymers with a PCL matrix exhibit microphase separation into three different phases within the spherulitic superstructures. Mixing of the PS-block can occur upon melting of the PCL-block if the molecular weight is low enough. Even though the crystallization takes place well below the PS-glass transition, a deformation of the amorphous microphases into ellipsoidal core-shell cylindrical microdomains is observed by TEM. These copolymers have mechanical properties which are dominated by the PCL (poly(ϵ-caprolactone)) matrix with an influence of the amorphous blocks. |