The effect of segment length and concentration on dielectric properties of polypropyleneoxide-based polyurethanes
Authors:Z S Petrović  I Javni  Ž Jelčić
Institution:(1) Present address: Faculty of Technology, Institute for Petrochemistry, Gas, Oil and Chemical Engineering, Novi Sad, Yugoslavia;(2) Soda-So, Túzla, Yugoslavia;(3) Institute Rudjer Boscaronkovicacute, Zagreb, Yugoslavia
Abstract:Three series of segmented polyurethanes based on MDI, variable chain extender, and polypropylene oxide of MW=1000, 2000, and 3000 were synthesized and their dielectric behavior examined.Dielectric relaxations in the segmented polyurethanes were investigated between –150°C and +150°C in the 100 Hz to 10 kHz range. In general, three transitions, designated asagr, beta, and gamma were observed, and ascribed in accordance with calorimetric relaxations to glass transitions of the hard and soft segments, and Shatzki-type motions, respectively. The effect of structure variables such as soft segment size, type of chain extender (ethylene glycol, butane diol, and hexane diol) and soft segment concentration, as well as the effect of interaction of the phases on dielectric properties was discussed. It was found that a certain degree of phase mixing exists in all series, detected by the variation of theT g of the soft segment with soft segment concentration, contrary to DSC results, which was ascribed to thermal treatment prior to the dielectric measurements. It appears that interfacial polarization becomes important only above theagr transition temperature.
Keywords:Dielectricproperties  polyurethane  elastomers  phaseseparation
本文献已被 SpringerLink 等数据库收录!
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司  京ICP备09084417号