中温固体氧化物燃料电池阴极材料LaBiMn2O6的制备与性能研究
引用本文:肖辉,孙丽萍,赵辉,霍丽华,Jean-Marc Bassat,Aline Rougier,S&#;bastien Fourcade,Jean-Claude Grenier.中温固体氧化物燃料电池阴极材料LaBiMn2O6的制备与性能研究[J].无机化学学报,2013,29(18).
作者姓名:肖辉  孙丽萍  赵辉  霍丽华  Jean-Marc Bassat  Aline Rougier  S&#;bastien Fourcade  Jean-Claude Grenier
作者单位:黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080;黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080;黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080;黑龙江大学化学化工与材料学院, 功能无机材料化学教育部重点实验室, 哈尔滨 150080;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France
基金项目:国家自然科学基金(No.51302069,51372073)、高等学校博士学科点专项科研基金(No.20132301110002)和人事部留学人员科技活动择优资助项目.
摘    要:采用固相法合成了中温固体氧化物燃料电池(IT-SOFCs)阴极材料LaBiMn2O6,并利用X射线衍射(XRD)和电化学阻抗谱(EIS)进行表征.结果表明该材料与电解质Ce0.7Bi0.3O1.85(CBO)在1 000 ℃烧结12 h不发生反应.交流阻抗和直流极化测试结果发现,阴极极化电阻随测试温度的增加而逐渐减小,700 ℃空气中的极化电阻为0.71 Ω·cm2;氧分压测试结果显示,在600~700 ℃范围内,电极反应的速率控制步骤为电极上发生的电荷转移反应.电极过电位为85 mV时,700 ℃的阴极电流密度达到 216 mA·cm-2 ,表明LaBiMn2O6是一种潜在的中温固体氧化物燃料电池(IT-SOFCs)阴极材料.

关 键 词:中温固体氧化物燃料电池(IT-SOFCs)  阴极材料  LaBiMn2O6  电极反应

Preparation and Electrochemical Properties of LaBiMn2O6 Cathode for IT-SOFCs
XIAO Hui,SUN Li-Ping,ZHAO Hui,HUO Li-Hu,Jean-Marc Bassat,Aline Rougier,S&#;bastien Fourcade and Jean-Claude Grenier.Preparation and Electrochemical Properties of LaBiMn2O6 Cathode for IT-SOFCs[J].Chinese Journal of Inorganic Chemistry,2013,29(18).
Authors:XIAO Hui  SUN Li-Ping  ZHAO Hui  HUO Li-Hu  Jean-Marc Bassat  Aline Rougier  S&#;bastien Fourcade and Jean-Claude Grenier
Institution:Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China;Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China;Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China;Key Laboratory of Functional Inorganic Material Chemistry, Ministry of Education, School of Chemistry and Materials Science, Heilongjiang University, Harbin 150080, China;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France;CNRS, Université de Bordeaux, ICMCB, 87 avenue du Dr. A. Schweitzer, F-33608 Pessac-Cedex, France
Abstract:
Keywords:intermediate temperature solid oxide fuel cells (IT-SOFCs)  cathode material  LaBiMn2O6  electrode reaction