The 0.6(Bi1-xLax)FeO 3-0.4SrTiO 3(x = 0,0.1) multiferroic ceramics are prepared by a modified Pechini method to study the effect of substitution of SrTiO3 and La in BiFeO3.The X-ray diffraction patterns confirm the single phase characteristics of all the compositions each with a rhombohedral structure.The magnetic properties of the ceramics are significantly improved by a solid solution with SrTiO3 and substitution of La.The values of the dielectric constant ε r and loss tangent tan δ of all the samples decrease with increasing frequency and become constant at room temperature.The La-doped 0.6BiFeO3-0.4SrTiO3 ceramics exhibit improved dielectric and ferroelectric properties,with higher dielectric constant enhanced remnant polarization(Pr) and lower leakage current at room temperature.Compared with a anti-ferromagnetic BiFeO3 compound,the 0.6(Bi0.9La0.1)FeO3-0.4SrTiO3 sample shows the optimal ferromagnetism with remnant magnetization M r ~ 0.135 emμ/g and ferroelectricity with Pr ~ 5.94 μC/cm 2 at room temperature. 相似文献
4.
Improved multiferroic properties of La-doped 0.6BiFeO<sub>3</sub>-0.4SrTiO<sub>3</sub> solid solution ceramics 下载免费PDF全文
The 0.6(Bi1-xLax)FeO 3-0.4SrTiO 3(x = 0,0.1) multiferroic ceramics are prepared by a modified Pechini method to study the effect of substitution of SrTiO3 and La in BiFeO3.The X-ray diffraction patterns confirm the single phase characteristics of all the compositions each with a rhombohedral structure.The magnetic properties of the ceramics are significantly improved by a solid solution with SrTiO3 and substitution of La.The values of the dielectric constant ε r and loss tangent tan δ of all the samples decrease with increasing frequency and become constant at room temperature.The La-doped 0.6BiFeO3-0.4SrTiO3 ceramics exhibit improved dielectric and ferroelectric properties,with higher dielectric constant enhanced remnant polarization(Pr) and lower leakage current at room temperature.Compared with a anti-ferromagnetic BiFeO3 compound,the 0.6(Bi0.9La0.1)FeO3-0.4SrTiO3 sample shows the optimal ferromagnetism with remnant magnetization M r ~ 0.135 emμ/g and ferroelectricity with Pr ~ 5.94 μC/cm 2 at room temperature. 相似文献
5.
6.
Multiferroic properties and exchange bias(EB) in Bi1-xSrxFeO3(x = 0–0.6) ceramics synthesized by a modified Pechini method are investigated. Sr concentration dependence of structure distorting, ferroelectric properties, and dielectric properties were studied at room temperature. Appropriate Sr doping(x = 0.05–0.2) has been found to decrease the conductivity, enhance ferroelectric properties and give rise to high dielectric constant. Compared with antiferromagnetic BiFeO3 compound, BSFO-x(0 ≤ x ≤ 0.4) ceramics show weak ferromagnetism at room temperature, and their exchange bias field and vertical magnetization shift are observed and exhibit a strong dependence on the content of Sr. This observed EB effect which keeps stable in BSFO ceramics at 10 K tend to vanish at room temperature with Sr concentration over 0.4. 相似文献