In this work, ultrafast differential scanning calorimetry (UFDSC) is used to study the dynamics of phase separation. Taking poly(vinyl methyl ether)/polystyrene (PVME/PS) blend as the example, we firstly obtained the phase diagram that has lower critical solution temperature (LCST), together with the glass transition temperature (Tg) of the homogeneous blend with different composition. Then, the dynamics of the phase separation of the PVME/PS blend with a mass ratio of 7:3 was studied in the time range from milliseconds to hours, by the virtue of small time and spatial resolution that UFDSC offers. The time dependence of the glass transition temperature (Tg) of PVME‐rich phase, shows a distinct change when the annealing temperature (Ta) changes from below to above 385 K. This corresponds to the transition from the nucleation and growth (NG) mechanism to the spinodal decomposition (SD) mechanism, as was verified by morphological and rheometric investigations. For the SD mechanism, the temperature‐dependent composition evolution in PVME‐rich domain was found to follow the Williams–Landel–Ferry (WLF) laws. © 2017 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2017 , 55, 1357–1364  相似文献   

2.
The influence of nanosilica on the concentration fluctuation of polystyrene/poly (vinyl methyl ether) (PS/PVME) mixtures was investigated during phase separation. The amplitude of concentration fluctuation was quantified by dielectric spectrums based on the idea of Lodge–Mcleish model and the linearized Cahn–Hilliard theory could describe the amplitude evolution of concentration fluctuation at the early stage of phase separation. Hydrophilic nanosilica A200 dispersed in PVME‐rich phase behaved an obvious inhibition effect on the concentration fluctuation of blend matrix, while hydrophobic nanosilica R974 dispersed in PS‐rich phase had little effect on the concentration fluctuation. The kinetics and amplitude evolution of concentration fluctuation during phase separation for PS/PVME/A200 nanocomposites were remarkably restrained due to the surface adsorption of PVME on A200. As the segmental dynamics of PVME and PS in homogeneous matrix was hardly influenced by A200 and R974, the enhanced miscibility and the significantly constrained flow relaxation of PVME chains might contribute to the retarded concentration fluctuation of PS/PVME/A200 nanocomposites. While the weak interaction between R974 and components of blend matrix and little effect of R974 on the molecular dynamics of PS chains may result in the weak retardation of concentration fluctuation for blend matrix. © 2017 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2017 , 55, 1337–1349  相似文献   

3.
The effect of phase‐separated morphology on the rheological properties of polystyrene/poly(vinyl methyl ether) (PS/PVME) blend was investigated by optical microscopy (OM), light scattering (LS) method, and rheology. The blend had a lower critical solution temperature (LCST) of 112°C obtained by turbidity experiment using LS at a heating rate of 1°C/h. Three different blend compositions (critical 30/70 PS/PVME by weight) and two off‐critical (50/50 and 10/90)) were prepared. The rheological properties of each composition were monitored with phase‐separation time after a temperature jump from a homogeneous state to the preset phase‐separation temperature. For the 30/70 and 50/50 blends, it was found that with phase‐separation time, the storage and loss moduli (G′ and G″) increased at shorter times due to the formation of co‐continuous structures resulting from spinodal decomposition. Under small oscillatory shearing, shear moduli gradually decreased with time at longer phase‐separation times due to the alignment of co‐continuous structures toward the flow direction, as verified by scanning electron microscopy. However, for the 10/90 PS/PVME blend, the rheological properties did not change with phase‐separation times. © 1999 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 37: 889–906, 1999  相似文献   

4.
The segmental dynamics of backbone‐deuterated polystyrenes (d3PS) with varying molecular weights (1.7–67 kg/mol) have been measured in blends with poly(vinyl methyl ether) (PVME). 2H NMR T1 values at 15 and 77 MHz are reported for the pure d3PS and for the dilute d3PS component in PVME matrices. The temperature shift that is needed to superpose the NMR T1 data for the pure d3PS and the d3PS as a dilute component in the blend ranges from 45 to 70 K. In the framework of Lodge/McLeish model, the self‐concentration value for d3PS in these dilute blends with PVME is found to be independent of molecular weight. We thus establish for this system that the substantial influence of molecular weight on the blend segmental dynamics can be explained by homopolymer Tg differences. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 2252–2262, 2007  相似文献   

5.
The effect of simple shear flow on the phase behavior and morphology was investigated for both polystyrene/poly(vinyl methyl ether) (PS/PVME) and poly(methyl methacrylate)/poly(styrene‐co‐acrylonitrile) (PMMA /SAN‐29.5) blends, which have LCST (lower critical solution temperature)‐type phase diagram. The measurements were carried out using a special shear apparatus of two parallel glass plates type. The PS/PVME blends showed shear‐induced demixing and shear‐induced mixing at low and high shear rate values, respectively. In addition, the rotation speed and the sample thickness were found to have a pronounced effect on the phase behavior under shear flow. On the‐other hand, PMMA/SAN blend showed only shear‐induced mixing and the magnitudes of the elevation of the cloud points were found to be composition and molecular weight dependent. The morphology of the PMMA/SAN=75/25 blend indicated that shear‐induced mixing occurred at a critical shear rate value, below which the two phases were highly oriented and elongated in the flow direction.  相似文献   

6.
The liquid–liquid phase‐separation (LLPS) behavior of poly(n‐methyl methacrylimide)/poly(vinylidene fluoride) (PMMI/PVDF) blend was studied by using small‐angle laser light scattering (SALLS) and phase contrast microscopy (PCM). The cloud point (Tc) of PMMI/PVDF blend was obtained using SALLS at the heating rate of 1 °C min?1 and it was found that PMMI/PVDF exhibited a low critical solution temperature (LCST) behavior similar to that of PMMA/PVDF. Moreover, Tc of PMMI/PVDF is higher than its melting temperature (Tm) and a large temperature gap between Tc and Tm exists. At the early phase‐separation stage, the apparent diffusion coefficient (Dapp) and the product (2Mk) of the molecules mobility coefficient (M) and the energy gradient coefficient (k) arising from contributions of composition gradient to the energy for PMMI/PVDF (50/50 wt) blend were calculated on the basis of linearized Cahn‐Hilliard‐Cook theory. The kinetic results showed that LLPS of PMMI/PVDF blends followed the spinodal decomposition (SD) mechanism. © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 1923–1931, 2008  相似文献   

7.
We have investigated the fluorescence emission spectra of pyrene and anthracene dyes covalently bonded to polystyrene (PS) upon phase separation from poly(vinyl methyl ether) (PVME). The specific chemical structure of the fluorescent labels is found to affect the measured phase separation temperature TS, with fluorophores covalently attached in closer proximity to the PS backbone identifying phase separation a few degrees earlier. The sharp increase in fluorescence intensity upon phase separation that occurs for all fluorophores with little change in spectral shape is consistent with a mechanism of static fluorescence quenching resulting from the specific interaction with a nearby quenching molecular unit. Based on recent work that has identified a weak hydrogen bond occurring between the aromatic hydrogens of PS and the ether oxygen of PVME, we believe a similar weak hydrogen bond is likely occurring between the PVME oxygen and the aromatic dyes providing a local (few nanometer) sensitivity to phase separation. © 2011 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys, 2011  相似文献   

8.
The phase behavior of statistical copolymers composed of (4‐tert‐butylstyrene) (B) and (4‐tert‐butoxystyrene) (O), abbreviated as s‐BO, with polyisoprene (I) was investigated by optical microscopic (OM) observation and small‐angle neutron scattering (SANS) measurements. It has been known that B/I blend shows lower critical solution temperature (LCST) type phase diagram, while O/I blend has upper critical solution temperature (UCST) type one. Several blends of s‐BOs having mol fraction of B, mB, comparable to 0.50, with I showed both UCST and LCST type phase diagram. Furthermore, UCST type phase behavior was observed for blends having small mB, while LCST type one was for that of large mB at all used temperatures. Hence, the phase behavior of s‐BO/I blend can be understood as a result of the competition of two interactions having opposite temperature dependence. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47: 2272–2280, 2009  相似文献   

9.
Synthesis, characterization, and polymer solar cell and transistor application of a series of phenanthro[1,2‐b:8,7‐b′]dithiophene‐based donor–acceptor (D–A)‐type semiconducting polymers combined with a diketopyrrolopyrrole unit are reported. The present polymers showed some unique features such as strong aggregation behavior, high thermal stability, and short π–π stacking distance (3.5–3.6 Å), which are suitable for high performance organic materials. In addition, they have a significantly extended absorption up to 1000 nm with a band gap of ca. 1.2 eV. However, such strong intermolecular interaction reduced their solubility and molecular weights, which resulted in low crystalline nature and moderate field‐effect mobility of 0.01 cm2 V?1 s?1. Furthermore, such strong aggregation behavior led to the large‐scale phase separation in the blend films, which may prevent the effective photocurrent generation, limiting Jsc and power conversion efficiency of 2.0%. © 2015 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2015 , 53, 709–718  相似文献   

10.
Styrene radical polymerizations mediated by the imidazolidinone nitroxides 2,5‐bis(spirocyclohexyl)‐3‐methylimidazolidin‐4‐one‐1‐oxyl (NO88Me) and 2,5‐bis(spirocyclohexyl)‐3‐benzylimidazolidin‐4‐one‐1‐oxyl (NO88Bn) were investigated. Polymeric alkoxyamine (PS‐NO88Bn)‐initiated systems exhibited controlled/living characteristics at 100–120 °C but not at 80 °C. All systems exhibited rates of polymerization similar to those of thermal polymerization, with the exception of the PS‐NO88Bn system at 80 °C, which polymerized twice as quickly. The dissociation rate constants (kd) for the PS‐NO88Me and PS‐NO88Bn coupling products were determined by electron spin resonance at 50–100 °C. The equilibrium constants were estimated to be 9.01 × 10?11 and 6.47 × 10?11 mol L?1 at 120 °C for NO88Me and NO88Bn, respectively, resulting in the combination rate constants (kc) 2.77 × 106 (NO88Me) and 2.07 × 106 L mol?1 s?1 (NO88Bn). The similar polymerization results and kinetic parameters for NO88Me and NO88Bn indicated the absence of any 3‐N‐transannular effect by the benzyl substituent relative to the methyl substituent. The values of kd and kc were 4–8 and 25–33 times lower, respectively, than the reported values for PS‐TEMPO at 120 °C, indicating that the 2,5‐spirodicyclohexyl rings have a more profound effect on the combination reaction rather than the dissociation reaction. © 2002 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 41: 327–334, 2003  相似文献   

11.
This article presents thermal diffusivity (D) measurements by flash radiometry for the polymer blend of polystyrene (PS) and poly(vinyl methyl ether) (PVME) with lower critical solution temperature (LCST) phase diagram. Dependence of D on PS content measured at 100°C coincides a phase diagram determined by a cloud point measurement. D value for the blend decreases with increasing PS content and has minimum value at the PS content around 20 wt % from which D increases again with increasing PS content. If the concentration fluctuation between two components in the miscible states at the temperature close to LCST causes the remarkable phonon scattering, the composition dependence of D would resemble the phase diagram. D for the sample in the phase-separated state is larger than that for the miscible state. The larger D in the phase-separated sample would be due to the decrease of the total surface area microscopically contacted to the counter component in the phase-separated state. Dependence of D on temperature for the phase-separated sample is quite different from that of the miscible one. On an isothermal measurement of D for PS/PVME (10 : 90) at 110°C just below the cloud point, D started to increase at time above 100 min and leveled out above 250 min. Isothermal observation of sample film by a differential interference contrast microscopy showed the creation of some structure due to the nucleation and growth of interface at 225 min and it became obvious above 250 min. Thus, the increase in D at 110°C implies that D can sensitively reflect the change in microscopic structures which follows the nucleation and growth of interface. © 1997 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 35 : 1869–1876, 1997  相似文献   

12.
Donor–acceptor block copolymers (BCP), incorporating poly(3‐hexylthiophene) (P3HT), and a polystyrene copolymer with pendant fullerenes (PPCBM) provide desired stable nanostructures, but mostly do not exhibit balanced charge carrier mobilities. This work presents an elegant approach to match hole and electron transport in BCP by blending with molecular PCBM without causing any macrophase separation. An insufficient electron mobility of PPCBM can be widely compensated by adding PCBM which is monitored by the space‐charge limited current method. Using X‐ray diffraction, atomic force microscopy, and differential scanning calorimetry, we verify the large miscibility of the PPCBM:PCBM blend up to 60 wt % PCBM load forming an amorphous, molecularly mixed fullerene phase without crystallization. Thus, blending BCP with PCBM substantially enhances charge transport achieving an electron mobility of μe=(3.2 ± 1.7) × 10?4 cm2V?1s?1 and hole mobility of μh=(1.8 ± 0.6) × 10?3 cm2V?1s?1 in organic field‐effect transistors (OFET). The BCP:PCBM blend provides a similarly high ambipolar charge transport compared to the established P3HT:PCBM system, but with the advantage of an exceptionally stable morphology even for prolonged thermal annealing. This work demonstrates the feasibility of high charge transport and stable morphology simultaneously in a donor–acceptor BCP by a blend approach. © 2016 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2016 , 54, 1125–1136  相似文献   

13.
The heat capacity of poly(vinyl methyl ether) (PVME) has been measured using adiabatic calorimetry and temperature‐modulated differential scanning calorimetry (TMDSC). The heat capacity of the solid and liquid states of amorphous PVME is reported from 5 to 360 K. The amorphous PVME has a glass transition at 248 K (?25 °C). Below the glass transition, the low‐temperature, experimental heat capacity of solid PVME is linked to the vibrational molecular motion. It can be approximated by a group vibration spectrum and a skeletal vibration spectrum. The skeletal vibrations were described by a general Tarasov equation with three Debye temperatures Θ1 = 647 K, Θ2 = Θ3 = 70 K, and nine skeletal modes. The calculated and experimental heat capacities agree to better than ±1.8% in the temperature range from 5 to 200 K. The experimental heat capacity of the liquid rubbery state of PVME is represented by Cp(liquid) = 72.36 + 0.136 T in J K?1 mol?1 and compared to estimated results from contributions of the same constituent groups of other polymers using the Advanced Thermal AnalysiS (ATHAS) Data Bank. The calculated solid and liquid heat capacities serve as baselines for the quantitative thermal analysis of amorphous PVME with different thermal histories. Also, knowing Cp of the solid and liquid, the integral thermodynamic functions of enthalpy, entropy, and free enthalpy of glassy and amorphous PVME are calculated with help of estimated parameters for the crystal. © 2005 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 43: 2141–2153, 2005  相似文献   

14.
The morphological development and crystallization behavior of a poly(ethylene terephthalate)/poly(hydroxyl ether of bisphenol A) (phenoxy) blend were studied with time‐resolved light scattering, optical microscopy, differential scanning calorimetry, and small‐angle X‐ray scattering (SAXS). During annealing at 280 °C, liquid–liquid phase separation via spinodal decomposition proceeded in the melt‐extruded specimen. After the formation of a domain structure, the blend slowly underwent phase homogenization by the interchange reactions between the two polymers. Specimens annealed for various times (ts) at 280 °C were subjected to a temperature drop and the effects of liquid‐phase changes on crystallization were then investigated. The shifts in the position of the cold‐crystallization peaks indicated that the crystallization rate is associated with the composition change of the separated phases as well as the change of the sequence distribution in polymer chains during annealing. The morphological parameters at the lamellar level were determined by a correlation function analysis on the SAXS data. The crystal thickness (lc) increased with ts, whereas the amorphous layer thickness (la) showed little dependence on ts. Observation of a constant la value revealed that a large number of noncrystallizable species formed by the interchange reactions between the two polymers were excluded from the lamellar stacks and resided in the interfibrillar regions, interspherulitic regions, or both. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 223–232, 2008  相似文献   

15.
Summary: The combined influence of the thermodynamical and hydrodynamic effects of shear was tentatively considered for the first time, in the modeling of the shear‐induced phase behavior of binary polymer blends in this paper. In this model, the original “two‐fluid” model proposed by Onuki 1 , 2 was modified by replacing the quiescent thermodynamical term with the one defined in the frame of extended irreversible thermodynamics (EIT). 3 - 5 The stress term of the polymer blend was determined by using the mixing rule of “Double Reptation” 6 , 7 along with the Graessley's 8 functions to make the model applicable in both linear and weak non‐linear regions. Then the apparent shift of phase boundary of a model blend system was computed by using this theory. It's found that this modified theory can predict both the “miscibility gap” and anisotropical phase separation of the polymer blend, while the two different previous theories, that is the pure thermodynamical one and hydrodynamic one, could only predict one but not both of them. For example, this modified “two‐fluid” model predicts that the miscibility gap can be observable not only in vorticity direction but also in the velocity gradient direction.

The calculated reduced stored energy Fs/RT as a function of ΦA and the temperature T (shear rate: 0.5 s−1).  相似文献   


16.
Thermally induced phase separation (TIPS) has been developed to prepare porous membranes. The porous structures are mainly dependent on diluents adopted in the TIPS process. We obtained two typical morphologies of poly(vinylidene fluoride) (PVDF) membranes using cyclohexanone (CO) and propylene carbonate (PC) as diluents, respectively. SEM observation displays that porous spherulites are formed from PVDF/CO system, whereas smooth particles result from PVDF/PC system. The TIPS processes of these two systems have been investigated in detail by optical microscope observation and temperature‐dependent FTIR combined with two‐dimensional infrared correlation analysis. Rapid crystallization of PVDF can be seen around 110 °C in the PVDF/CO system, which is consistent with the results of temperature‐dependent FTIR spectra. The spectral evolution indicates a transform of PVDF from amorphous to α‐phase after 110 °C. The νs(C?O) band at 1712 cm?1 narrows and the νs(C? F) band at 1188 cm?1 shifts to 1192 cm?1 before crystallization, which implies the destruction of interaction between PVDF and CO. In contrast, the PVDF/PC system shows slow crystallization with all‐trans conformation assigned to β‐phase and γ‐phase below 60 °C but no obvious change of polymer?diluent interaction. We propose two mechanisms for the different phase behaviors of PVDF/CO and PVDF/PC systems: a solid?liquid phase separation after destruction of polymer?diluent interaction in the former, and a liquid?liquid phase separation process coupled with rich‐phase crystallization in the later. This work may provide new insight into the relationship among morphologies, crystal forms, and phase separation processes, which will be helpful to adjust membrane structure. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part B: Polym. Phys. 2013, 51, 1438–1447  相似文献   

17.
The effects of adding A–B diblock copolymer to a polymer blend (A/B) on phase‐separation kinetics and morphology have been investigated in a fixed shallow‐quench condition (ΔT = 1.5 °C) by in situ time‐resolved light scattering and phase‐contrast optical microscopy. A shear‐quench technique was used in this study instead of a conventional temperature‐quench method. Mixtures of nearly monodisperse low relative‐molecular masses of polybutadiene (Mw = 2.8 kg/mol), polystyrene (Mw = 2.6 kg/mol), and a near‐symmetric butadiene–styrene diblock copolymer (Mw = 6.3 kg/mol) as an interfacial modifier were studied. We observed that the addition of the diblock copolymer could either retard or accelerate the phase‐separation kinetics depending on the concentration of the diblock copolymer in the homopolymer blends. In contrast to the conventional temperature quench, we observed complex phase‐separation kinetics in the intermediate and late stages of phase separation by the shear‐quench technique. © 2001 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 39: 819–830, 2001  相似文献   

18.
The FT–IR spectroscopic analysis and the thermal behavior of the blends of styrene-1-vinyl naphthalene copolymers [P(S-co-1VN)] and poly(vinyl methyl ether) (PVME) were investigated in this work. The copolymers containing 23, 50, and 80% by weight of styrene were synthesized by radical polymerization. The blend films of the P(S-co-1VN) and PVME were cast from the mixed solvent of benzene/trimethylbenzene [50/50 (v/v)]. It was found from the optical clarity and the glass transition temperature behavior that the blends of PVME with P(S-co-1VN) of 80 wt % styrene and 20 wt % 1-vinylnaphthalene (1VN) show miscibility below 50 wt % of the copolymer concentration and the concentration range to show miscibility becomes wider as the composition of 1VN decreases in the copolymers. From the FT–IR results, the relative peak intensity of the 1100 cm?1 region due to COCH3 bond of PVME and the peak position of 774 cm?1 region due to the naphthyl ring of 1VN were sensitive to the miscibility of the P(S-co-1VN)/PVME blends. The frequency differences of the phenyl ring and the naphthyl ring in the P(S-co-1VN) from each frequency in the P(S-co-1VN)/PVME blends increase with increasing composition of styrene in the copolymers and with increasing concentration of PVME in the blends. A threshold energy exists to induce molecular interaction between the naphthyl ring of 1VN and the COCH3 of PVME and to result in the miscible blends, regardless of the copolymer composition as well as the blend concentration. The threshold energy was estimated as about 3.689 × 10?21 cal (779 cm?1) for the P(S-co-1VN)/PVME blend system. It can be concluded that the miscibility in P(S-co-1VN)/PVME blends is largely affected by the composition of the copolymers, and the blends become more miscible as the composition of styrene in the copolymers increases.  相似文献   

19.
Linear viscoelasticity behavior is described with the sum of two terms for polystyrene solutions in tricresyl phosphate around the coil overlapping concentration (K. Osaki, T. Inoue, & T. Uematsu, J Polym Sci Part B: Polym Phys 2001, 39, 211). One is a Rouse–Zimm (RZ) term represented by the Zimm theory with arbitrarily chosen values of the hydrodynamic interaction parameter and the longest relaxation time (τRZ). The other (the L term) consists of a relaxation mode with a single relaxation time (τL > τRZ) and a high‐frequency limiting modulus proportional to the square of the concentration. In this study, we describe the viscosity (η) and first normal stress coefficient (Ψ1) in steady shear with simple formulas. The stress due to the L term is assumed to be given by a Kaye, Bernstein, Kearsley, and Zapas (K‐BKZ) equation with the damping function h(γ) = (1 + 0.2γ2)?1/2, where γ is the magnitude of shear. Contributions to η and Ψ1 from the RZ term are derived from the RZ model, in which the relaxation time in steady flow is given by τst = τ + (τRZ ? τ)/(1 + 0.35τRZ γ˙) instead of τRZ. Here, γ˙ is the rate of shear, and τ is the τRZ value at the infinite dilution limit. η and Ψ1 at various concentrations for two polystyrene samples (with molecular weights of 2890 and 8420 kg mol?1) are well described with parameters derived from dynamic viscoelasticity. © 2002 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 40: 1038–1045, 2002  相似文献   

20.
Two regiochemically defined polythiophenes containing thiazolothiazole acceptor unit were synthesized by palladium(0)‐catalyzed Stille coupling reaction. The thermal, electrochemical, optical, charge transport, and photovoltaic properties of these copolymers were examined. Compared to P1 with head‐to‐head coupling of two middle thiophenes, P2 with head‐to‐tail coupling of two middle thiophenes exhibits 40 nm red shift of absorption spectrum in film and 0.3 eV higher HOMO level. Both polymers exhibit field‐effect hole mobility as high as 0.02 cm2 V?1 s?1. Polymer solar cells (PSCs) were fabricated based on the blend of the polymers and methanofullerene[6,6]‐phenyl C71‐butyric acid methyl ester (PC71BM). The PSC based on P1 :PC71BM (1:2, w/w) exhibits a power conversion efficiency of 2.7% under AM 1.5, 100 mW cm?2, two times of that based on P2 :PC71BM. The higher efficiency is attributed to lower HOMO (?5.6 eV) and smaller phase separation scale in P1 :PC71BM blend. Tiny change in thiophene connection of P1 and P2 lead to great difference in HOMO, phase separation scale, and efficiency of their photovoltaic devices. © 2011 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2011  相似文献   