A series of novel soluble poly(aryl ether ketone)s (PAEKs) based on 5,10‐bis(4‐hydroxyphenyl)?15,20‐diphenylporphyrin (cis‐DHTPP), 4,4′‐(hexafluoroisopropylidene) diphenol (6FBPA) and 4,4′‐difluorobenzophenone (DFB) were synthesized and characterized by FT‐IR, 1H‐NMR, UV–vis and fluorescence spectroscopies. The intrinsic photophysical properties of porphyrins were preserved because of the absence of photoinduced electron transfer in the polymer chains. Investigation of the copolymers thermal properties indicated that these polymers had high glass transition temperatures and excellent thermal stabilities. The results of Z‐scan and optical limiting measurements manifested that incorporation of the porphyrin chromophore into the main chain engendered the novel PAEKs with superior nonlinear optical properties and optical limiting function, which could be effectively tuned by varying the molar ratio of porphyrin monomers. © 2014 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2014 , 52, 1282–1290  相似文献   

2.
A novel triphenylamine (TPA)‐containing bis(ether anhydride) monomer, namely 4,4′‐bis(3,4‐dicarboxyphenoxy)triphenylamine dianhydride, was synthesized and reacted with various aromatic diamines leading to a series of new poly(ether‐imide)s (PEI). Most of these PEIs were soluble in organic solvents and could be easily solution cast into flexible and strong films. The polymer films exhibited good thermal stability with glass‐transition temperatures in the range 211–299 °C. The polymer films exhibited reversible electrochemical processes and stable color changes (from transparent to navy blue) with high coloration efficiency and contrast ratio upon electro‐oxidation. During the electrochemical oxidation process, a crosslinked polymer structure was developed due to the coupling reaction between the TPA radical cation moieties in the polymer chains. These polymers can be used to fabricate electrochromic devices with high coloration efficiency, high redox stability, and fast response time. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2014 , 52, 825–838  相似文献   

3.
The thermal alignment of the liquid crystalline fluorene‐thiophene copolymer (F8T2) on rubbed polyimide surfaces is investigated by ex‐situ and in‐situ X‐ray scattering experiments. The ex‐situ characterization allows an assignment of the observed diffraction peaks to distances between polymer backbones (1.6 nm), distances between the flexible side groups of the polymer chains (0.43 nm), and intramolecular distances of adjacent ring units (0.5 nm). The in‐situ characterization allows a temperature dependent observation of the polymer chain alignment. A gradual alignment process of the polymer backbones is observed for temperatures up to 563 K. Decreasing temperature after the polymer chain alignment is accompanied by a glass transition of the side chains at 380 K. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47:1599–1604, 2009  相似文献   

4.
The dynamic heat capacity and glass‐transition temperature of polystyrene (PS)/poly(vinyl acetate‐co‐butyl acrylate) (VAc–BA) (50:50 w/w) structured latex films as a function of annealing time at 70, 77, and 85 °C were examined with modulated‐temperature differential scanning calorimetry. The PS and poly(vinyl acetate‐con‐butyl acrylate) components were considered to be the cores and shells, respectively, in the structured latex. The dynamic heat capacity decreased with time. The glass‐transition temperatures of the PS and VAc–BA phases shifted to higher values after annealing. The results of thermogravimetry showed that there existed about 1.8% residual water in the films. The mean free volume and relative concentration of holes at room temperature (before and after annealing) and 85 °C, as a function of time, were obtained with positron annihilation lifetime spectroscopy (PALS). The PALS results indicated no significant change in free volume during annealing. It is believed that the loss, by diffusion, of residual water mainly caused a decrease in heat capacity and an increase in the glass‐transition temperatures. As little as 1.8% residual water in the structured latex films had a significant influence on the thermal properties. © 2001 John Wiley & Sons, Inc. J Polym Sci Part B: Polym Phys 39: 1659–1664, 2001  相似文献   

5.
Neutron spin‐echo spectroscopy has been used to measure the time‐scale of fluctuations associated with the inter‐chain correlation peak observed in the diffraction pattern of the perfluorosulfonate ionomer, Nafion®. We have successfully measured the chain dynamics as a function of water content and temperature and have demonstrated that the chain dynamics become faster with increasing temperature. The addition of water also results in shorter relaxation times due to a plasticization of the chain motions. At water contents above a λ ≈ 6, the chain dynamics seem to approach a plateau and the relaxation times of the chains are no longer being plasticized by the presence of additional water molecules. The increased mobility in molecular relaxations induced by the presence of water points to the molecular origins of the temperature‐ and humidity‐dependent softening mechanisms in Nafion and other perfluorinated sulfonic acid membrane materials. Moreover, these results show that there is a strong inter‐dependence of the dynamics of water and the polymer chains in Nafion membranes. © 2014 Wiley Periodicals, Inc. J. Polym. Sci. Part B: Polym. 2014 , 52, 624–632  相似文献   

6.
Poly(phenylenevinylene‐alt‐fluorenevinylene) ( PF ) or poly(fluorenevinylene) ( F ) derivatives that carried alkyl chains with terminal tertiary amino groups were successfully synthesized via Heck coupling. They were postquaternized by reacting with bromoethane to the corresponding cationic polyelectrolytes PFQ and FQ . The neutral polymers PF and F as well as the quaternized polymer FQ were soluble in common organic solvents such as THF, chloroform, dichloromethane, and toluene. In contrast, the quaternized polymer PFQ did not dissolve in these solvents but was soluble in environmentally friendlier solvents like water and alcohols. The neutral precursors exhibited higher thermal stability and glass‐transition temperatures than the corresponding quaternized counterparts. All polymers emitted intense blue‐greenish light in solution (462–489 nm) with relatively high photoluminescence (PL) quantum yields 0.32–0.57, and as thin films (475–557 nm) with optical band gaps of 2.48–2.57 eV. The water soluble PFQ could find potential applications as chemo or biosensor. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 1481–1491, 2007  相似文献   

7.
The phase behavior of poly(N‐tertbutylacrylamide‐co‐acrylamide) (PNTBAM) in pure water and mixture of water–methanol is studied at different temperatures. The different compositions of PNTBAM are prepared by free‐radical polymerization technique and their phase behavior is studied by turbidimetry. The effects of copolymer and solvent composition on the phase behavior of the copolymers are discussed. It has been suggested that the inhomogenities in polymer chains are responsible for lowering the rate of phase transition by increasing the N‐tertbutylacrylamide (NTBAM) and methanol contents in copolymer and mixture, respectively. For the first time we have revealed that there are second‐order binary interactions in the water–methanol which are dominant in the special range of copolymer composition. © 2009 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 47: 455–462, 2009  相似文献   

8.
Polylactide (PLA)‐grafted dextran was synthesized with a trimethylsilyl protection method to produce novel biodegradable, biomedical materials. PLA‐grafted dextrans with various lengths and numbers of graft chains were synthesized. The properties of solution‐cast films prepared from PLA‐grafted dextrans were investigated with thermal and dynamic mechanical analyses. The graft‐copolymer films exhibited lower glass‐transition temperatures, melting temperatures (Tm's), and crystallinities as well as higher viscosity properties as compared with poly‐L ‐lactide film. The Tm and crystallinity and mechanical properties at 37 °C could be adjusted by controlling the molecular structure such as the lengths and numbers of graft chains. Furthermore, the biodegradability of PLA‐grafted dextran films was investigated through the weight change of film and the molecular weight change of polymer during the in vitro degradation test. PLA‐grafted dextrans exhibited different degradation behavior from poly‐L ‐lactide with the introduction of a polysaccharide segment and branched structure as well as the change of end‐functional group. The degradation rate of PLA‐grafted dextran and the cast film prepared from PLA‐grafted dextran could be adjusted by controlling the sugar content or the length of graft chains. © 2003 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 41: 2462–2468, 2003  相似文献   

9.
A new class of thermosetting poly(2,6‐dimethyl‐1,4‐phenylene oxide)s containing pendant epoxide groups were synthesized and characterized. These new epoxy polymers were prepared through the bromination of poly(2,6‐dimethyl‐1,4‐phenylene oxide) in halogenated aromatic hydrocarbons followed by a Wittig reaction to yield vinyl‐substituted polymer derivatives. The treatment of the vinyl‐substituted polymers with m‐chloroperbenzoic acid led to the formation of epoxidized poly(2,6‐dimethyl‐1,4‐phenylene oxide) with variable pendant ratios, and the structures and properties were studied with nuclear magnetic resonance spectroscopy, Fourier transform infrared spectroscopy, differential scanning calorimetry, thermogravimetric analysis, and gel permeation chromatography. The ratios of pendant functional groups were tailored for the polymer properties, and the results showed that the glass‐transition temperatures increased as the benzylic protons were replaced by bromo‐, vinyl‐, or epoxide‐functional groups, whereas the thermal stability decreased in comparison with the original polymer. Within a molar fraction of 20–50%, the degree of functionalization had little effect on the glass‐transition temperature; however, it correlated inversely with the thermal stability of each functionalized polymer. The thermal curing behavior of the epoxide‐functionalized polymer was enhanced by the increment of the pendant functionality, which resulted in a significant increase in the glass‐transition temperature as well as the thermal stability after the curing reaction. © 2006 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 44: 5875–5886, 2006  相似文献   

10.
Novel X‐type polyurethane 4 containing 4‐(4‐nitrophenylazo)‐6‐nitroresorcinoxy groups as nonlinear optical (NLO) chromophores, which are parts of the polymer main chains, was prepared and characterized. Polyurethane 4 is soluble in common organic solvents such as acetone and N,N‐dimethylformamide. It shows thermal stabilities up to 270 °C from thermogravimetric analysis with glass transition temperature obtained from differential scanning calorimetry of about 134 °C. The second harmonic generation (SHG) coefficient (d33) of poled polymer film at 1064 nm fundamental wavelength is 5.37 × 10?9 esu. Polymer 4 exhibits a thermal stability up to Tg, and no significant SHG decay is observed below 135 °C, which is acceptable for NLO device applications. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2014 , 52, 760–766  相似文献   

11.
Linear and crosslinked polymers based on N‐isopropylacrylamide (NIPAAm) exhibit unusual thermal properties. Aqueous solutions of poly(N‐isopropylacrylamide) (PNIPAAm) phase‐separate upon heating above a lower critical solution temperature (LCST), whereas related hydrogels undergo a swelling–shrinking transition at an LCST. A linear copolymer made of NIPAAm/acryloxysuccinimide (98/2 mol/mol) and two hydrogels with different hydrophilicities were prepared. Fourier transform infrared (FTIR) spectroscopy was employed to determine the transition temperature and provide insights into the molecular details of the transition via probing of characteristic bands as a function of temperature. The FTIR spectroscopy method described here allowed the determination of the transition temperature for both the linear and crosslinked polymers. The transition temperatures for PNIPAAm and the gel resulting from the crosslinking with polylysine or N,N′‐methylenebisacrylamide (MBA) were in the same range, 30–35 °C. For the gels, the transition temperature increased with the hydrophilicity of the polymer matrix. The spectral changes observed at the LCST were similar for the free chains and the hydrogels, implying a similar molecular reorganization during the transition. The C H stretching region suggests that the N‐isopropyl groups and the backbone both underwent conformational changes and became more ordered upon heating above the LCST. An analysis of the amide I band suggests that the amide groups of the linear polymer were mainly involved in hydrogen bonding with water molecules below the LCST, the chain being flexible and disordered in a water solution. During the transition, around 20% of these intermolecular hydrogen bonds between the polymer and water were broken and replaced by intramolecular hydrogen bonds. Similar changes were also observed at the LCST of a gel crosslinked with MBA. © 2000 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 38: 907–915, 2000  相似文献   

12.
Poly(N,N‐diethylacrylamide) (PDEA) possesses a lower critical solution temperature (LCST) in aqueous media. The solution properties of PDEA at various temperatures have been characterized with techniques such as rheology and dynamic light scattering. There is a decrease in the coil size before the phase transition due to a coil‐to‐globule transition. At the LCST, rheological and dynamic light scattering studies have also confirmed an aggregation phenomenon. This aggregation modifies the rheological properties of the polymer solutions. High frequencies hinder the phase‐transition process and reduce the LCST of the polymers. © 2003 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 41: 1627–1637, 2003  相似文献   

13.
The free volume and related mobility properties of substituted poly(p-phenylene) polymers are examined. The techniques used range from positron annihilation, dielectric relaxation, and dynamic mechanical spectroscopy to thermally stimulated currents. Fractional free volume is determined for the samples with different substituted side groups and related to the glass transition temperature. Bulkier groups lead to a greater fractional free volume and lower glass transition temperatures. Comparison of molecular relaxation times using the different characterization techniques demonstrates that there is strong coupling between motion of the main chain and the side groups, on which the dipoles reside. Intermolecular coupling between the main chains at the primary relaxation is shown in this work to be related to the nature of the side chains and resultant free volume, as are the temperature locations of local, secondary relaxations. A qualitative model describing the effect of regiochemistry on the motions and packing of these materials is also proposed. © 1998 John Wiley & Sons, Inc. J Polym Sci B: Polym Phys 36: 1465–1481, 1998  相似文献   

14.
The high selectivity of solid‐state crosslinked poly(vinyl alcohol) (CPVA) membranes containing silver hexafluoroantimonate (AgSbF6), with respect to olefin/paraffin mixtures, was previously reported. The structure and coordination properties of CPVA/AgSbF6 complexes were investigated in this study with wide‐angle X‐ray scattering (WAXS), differential scanning calorimetry (DSC), X‐ray photoelectron spectroscopy (XPS), and theoretical ab initio calculations, and they were compared with those of poly(vinyl alcohol) (PVA)/AgSbF6 complexes. Contrary to expectations, the measurements of the intersegmental d‐spacings and glass‐transition temperatures indicated that the chain mobility in the PVA/AgSbF6 membranes was lower than that in the CPVA/AgSbF6 membranes. The different extents of transient crosslinking in the two systems were attributed mostly to their different coordination structures; silver ions in PVA/AgSbF6 were coordinated with hydroxyl oxygens located near the polymer main chains, whereas those in CPVA/AgSbF6 were coordinated with aldehyde oxygens located far from the main chains. According to WAXS spectra, AgSbF6 was completely dissolved in both PVA and CPVA, and this disrupted the crystallinity of the polymers. However, our DSC study showed that the silver ions dissolved in both polymer matrices recrystallized into silver oxide at elevated temperatures. The binding energy of Ag3d5/2, as determined from XPS spectra, shifted to lower values with the addition of increasing amounts of the polymer matrix, indicating the increasing coordination of silver ions with polymer chains. The presence of various oxygen species with and without coordination to silver ions was confirmed from O1s XPS spectra of CPVA membranes containing silver ions. © 2004 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 42: 621–628, 2004  相似文献   

15.
A series of poly(arylene ether ether nitrile)s with different chain lengths of the alkylsulfonates (SPAEEN‐x: x refers number of the methylene units) are successfully synthesized for fuel cell applications. The polymers produced flexible and transparent membranes by solvent casting. The resulting membranes display a high thermal stability, oxidative stability, and higher proton conductivity than that of Nafion 117 at 80 °C and 95% relative humidity (RH). Furthermore, the SPAEEN‐12 with the longest alkylsulfonated side chain exhibits a higher proton conductivity at 30% RH than that of SPAEEN‐6 despite the lower IEC value, which indicates that the introduction of longer alkylsufonated side chains to the polymer main chain induces an efficient proton conduction by the formation of a well‐developed phase‐separated morphology. © 2013 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2014 , 52, 21–29  相似文献   

16.
We have discovered that pentamethylcyclopentasiloxane (D5H) can be readily polymerized into poly(pentmethylcyclopentasiloxane) (PD5) with a Pt (Karstedt) catalyst in the presence of water in bulk or in solution at 100 °C and that the product is a solid with extraordinary properties. The polymerization starts with the oxidation of the SiH groups by water into an intermediate containing SiOH groups (SiH + H2O → SiOH + H2), which is followed immediately by the condensation (2SiO → Si? O? Si) of D5H rings into complex aggregates of cyclosiloxane moieties. According to Raman spectroscopy, an average of three of the five SiH functionalities are converted, and the final product contains only a negligible number of SiOH groups. The melting and glass‐transition temperatures of the monomer are exceptionally low: Tm,D5H = ?137.6 ± 1 and Tg,D5H = ?152 ± 2 °C. The polymer exhibits an unprecedented combination of properties: it is a stiff and brittle solid, is insoluble in common solvents, does not exhibit a melting endotherm but has an extremely low glass transition (Tg,PD5 = ?151 ± 0.5 °C), and is thermally stable up to at least 700 °C. Brillouin scattering indicates very slow variation of the relaxation time with temperature, a property characteristic of strong glass‐forming systems such as silica glass. This characteristic may account for the unique combination of properties of the new polymer: an extremely low glass‐transition temperature combined with solidlike properties even at ambient temperature (more than twice its glass‐transition temperature). © 2002 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 40: 1285–1292, 2002  相似文献   

17.
The effect of single walled carbon nanotube (SWCNT) fillers on the low temperature thermal properties and curing behavior of SWCNT‐silicone nanocomposite are reported for the first time. The SWCNT‐silicone composites were prepared by different mixing procedures and characterized by differential scanning calorimetry (DSC). Solution mix, with the aid of sonication and soaking achieved better dispersion of SWCNTs in the silicone. The adding of SWCNTs in polymer seriously hindered the curing of silicone elastomer. The hindrance increased with increasing concentration of SWCNT and the quality of dispersion. The glass transition temperatures (Tg) of the nanocomposites were found to be independent of the SWCNT addition, although, the steps in the heat capacity (Δcp) of the glass transition were smaller with increasing SWCNTs concentration. The melt crystallization behavior was strongly dependent on the concentration and dispersion of SWCNT in the polymer. The cooling scan showed that the higher concentration and the better dispersion of SWCNTs in the silicone resulted in higher percentage of melt crystallization of this nanocomposite. The correlation of the change of thermal properties to the dispersion of CNT in polymer may be used to determine the quality of SWCNT dispersion in silicone polymer. © 2008 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 46: 1845–1852, 2008  相似文献   

18.
A series of copoly(ether ketone)s containing double bonds along the polymer chains were synthesized from the condensation polymerization of hydroquinone with 4,4′‐difluorobenzophenone and 4,5‐bis(4‐fluorobenzoyl)‐1‐methylcyclohexene in sulfolane containing anhydrous potassium carbonate. The presence of methylcyclohexene in the polymer chains resulted in an improvement in the solubility of poly(ether ketone)s in organic solvents such as chloroform, chlorobenzene, and sulfolane. As a result, the conditions for synthesizing these polymers were much milder than those for poly(ether ether ketone). The new copoly(ether ketone)s also showed good tensile properties and reasonable thermal stability. New polyethers containing pyrazine unites were obtained from the cyclization reaction of these copoly(ether ketone)s with hydrazine. The hydrazine cycloderivatives led to an increase in the glass‐transition temperatures and a decrease in solubility in organic solvents. © 2002 Government of Canada. Exclusive world‐wide publication rights in the article have been transferred to Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 40: 3449–3454, 2002  相似文献   

19.
Poly(ethylene terephthalate) (PET), poly(ethylene terephthalate‐co‐4,4′‐bibenzoate) (PETBB55), and poly(ethylene 2,6‐naphthalate) (PEN) were cold‐drawn to achieve uniform extension without crystallization or stress whitening, and oxygen transport properties were studied at temperatures from 10 to 40 °C. Correlation of oxygen solubility and polymer specific volume made it possible to consider the oriented polyester as a one‐phase densified glass. Orientation was viewed as decreasing the amount of excess‐hole free volume and bringing the nonequilibrium polymer glass closer to the equilibrium condition. Between 10 and 40 °C, the amount of excess‐hole free volume in PET decreased as the polymer approached the glass transition temperature. In contrast, temperature changes in this range had little effect on the excess‐hole free volume in PETBB55 and PEN, which were well below their glass transition temperature. Gas diffusion was viewed as discrete jumps of the oxygen molecule between holes of excess‐free volume. The jump length was extracted from the activation energy for diffusion according to a channel‐formation model. The result agreed well with the hole spacing estimated from a simple lattice model using the hole density reported in the literature. Extending the lattice model to estimate the mean excess‐free volume hole radius from the fractional free volume resulted in good correlation with the hole radius obtained from positron annihilation lifetime spectroscopy. © 2003 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 42: 493–504, 2004  相似文献   

20.
An increased focus exists on the development of materials that might serve as ligament or tendon tissue engineering scaffolds. Requirements for a suitable candidate polymer include biodegradability, biocompatibility, and elasticity. In an attempt to meet these requirements novel citronellol‐containing polyphosphazenes were synthesized, characterized, and crosslinked to generate elastomers. Citronellol was chosen as a side group due to its anti‐inflammatory properties in addition to the presence of a double bond in its structure to permit polymer crosslinking. Alanine ethyl ester was chosen as a co‐substituent to tune hydrolysis rates without severely affecting the glass transition temperatures of the final polymers. Hydrolysis of the uncrosslinked polymers in the form of films in deionized water at 37 °C showed between ~8 and 16% mass loss and between a ~28 and 88% molecular weight decline over 12 weeks. Polymers were also crosslinked using ultraviolet radiation for increasing amounts of time. Preliminary mechanical testing of the homo‐citronellol polymer indicated increasing modulus and decreasing tensile strength with increased crosslink density. © 2014 Wiley Periodicals, Inc. J. Polym. Sci., Part A: Polym. Chem. 2014 , 52, 2258–2265  相似文献   