1.
孙秀玉 《高分子科学》2014,32(2):130-136
Poly(3-(2-methoxyphenyl)thiophene) (PMP-Th) nanowires were fabricated using porous anodic alumina (PAA) as template through electrochemical polymerization by cyclic voltammetry. The control on the size of nanowires was confirmed by electron microscopy. The results indicated that the luminescence spectra of PMP-Th nanowires in PAA nanochannels were blue-shifted and emission intensity was enhanced compared to the emission of the PMP-Th film. Moreover, the luminescent spectra of PMP-Th nanowires were size dependent, which may result from the change in the degree of confinement of nanowires in PAA. F6rster energy transfer from PAA to PMP-Th molecules is considered to be responsible for the enhancement of luminescence from PMP-Th nanowires in PAA. The results show that the emission properties of polymers with nanostructures can be tuned by controlling their size.  相似文献   

2.
溶剂热制备氧化锌纳米线   总被引:10,自引:0,他引:10  
ZnO nanowires were synthesized mildly through an absolute alcohol solvothermal process at 120 ℃ for 12 h using ZnAc2·2H2O and NaOH as raw materials and PEG400 as a soft template. The cyrstal structure and morphology of the nanowires were characterized by XRD, SEM, TEM and HRTEM. The results indicate that the diameter of ZnO nanowires is 40 nm, the length can reach 2 μm and the nanowires are of high purity, homogeneity and well crystallinty. The influence of the various factors on the formation of ZnO nanowires and formation mechanism were also discussed.  相似文献   

3.
The rapid development of internet and internet of things brings new opportunities for the expansion of intelligent sensors,and acetone as a major disease detection indicator(i.e.,diabetes) making it become extremely important clinical indicator.Herein,uniform mesoporous ZnO spheres were successfully synthesized via novel formaldehyde-assisted metal-ligand crosslinking strategy.In order to adjust the pore structure of mesoporous ZnO,various mesoporous ZnO spheres were synthesized by changing weight percentage of Zn(NO_3)_2·6 H_2 O to tannic acid(TA).Moreover,highly active heterojunction mesoporous ZnO/Co_3 O_4 has been fabricated based on as-prepared ultra-small Co_3 O_4 nanocrystals(ca.3 nm) and mesoporous ZnO spheres by flexible impregnation technique.Profit from nano-size effect and synergistic effect of p-n heterojunction,mesoporous ZnO/Co_3 O_4 exhibited excellent acetone sensing performance with high selectivity,superior sensitivity and responsiveness.Typically,5 wt% Co_3 O_4 embedded mesoporous ZnO sphere showed prominent acetone response(ca.46 for 50 ppm),which was about 11.5 times higher than that in pure ZnO sensing device,and it was also endowed high cyclic stability.The nanocrystals embedded hybrid material is expected to be used as promising efficient material in the field of catalysis and gas sensing.  相似文献   

4.
张群  陈传宝  方亮 《结构化学》2009,28(2):151-156
CaCO3 hollow spheres were prepared easily in anion surfactants (sodium dodecylbenzenesulfonate (SDBS)) and aspartic (Asp) acid binary-additive system by using an easy rapid agitation method. The as-prepared products were characterized with scanning electron microscopy (SEM), FT-IR and X-ray diffraction. The results suggested that the CaCO3 hollow spheres have diameters ranging from 1 to 2 μm, and their wall is constituted of many nano-particles. Moreover, the possible formation mechanism of the hollow spherical structure was proposed.  相似文献   

5.
PAMAM树形分子为模板低温制备纳米硫化锌空心球   总被引:4,自引:0,他引:4  
Hollow ZnS spheres have been prepared in the presence of generation 3.5 poly (amidoamine) dendrimers with surface ester groups (G3.5-COOCH3 PAMAM dendrimer) as synthetic matrix template. The products obtained were characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM) and UV-Vis absorption. TEM studies show that the hollow spheres with diameters ranging from 80 to 100 nm are prepared. The range of wall thickness was estimated to be about 20~30 nm. It was found that the concentration of PAMAM dendrimer had a significant influence on the formation of hollow ZnS spheres. The possible formation mechanism of the hollow spherical structure is also discussed.  相似文献   

6.
A novel method applying simple, rapid, effective and inexpensive excitation-emission matrix (EEM) fluorescence spectroscopy coupled with second-order calibration method for simultaneous determination of ethoxyquin (EQ) and tert-butylhydroquinone (TBHQ) contents in biological fluid samples was developed. After a simple data preprocessing that was to insert zeros below the first-order Rayleigh scattering, the second-order calibration method based on the alternating normalization-weighed error (ANWE) algorithm was used to deal with EEM data. Via the introduced "second-order advantage", the individual con- centrations of the analytes of interest could be obtained even in the presence of uncalibrated interferences. The experimental concentration ranges for the analytes were as follows: EQ, from 4.58 to 20.6 g mL 1 in plasma and from 6.87 to 20.6 g mL 1 in urine; TBHQ, from 4.49 to 20.2 g mL-1 in plasma and from 6.73 to 22.4 g mL-1 in urine. The recoveries from spiked biological fluid samples were in the ranges of 92.8%-106.2% for EQ and 94.6%-107.2% for TBHQ. These results demonstrate that the three-dimensional EEM fluorescence with second-order calibration method is a powerful tool for obtaining both EQ and TBHQ quantitative results in plasma and urine samples, and could be applied to more complex matrices.  相似文献   

7.
A surfactant-assisted method for preparing colloidal spheres with narrow size distribution from a polydispersed azo polymer has been developed in this work. The colloidal spheres were formed through gradual hydrophobic aggregation of the polymeric chains in THF-H2O dispersion media, which was induced by a steady increase in the water content. Results showed that the addition of a small amount of surfactant (SDBS) could significantly narrow the size distribution of the colloidal spheres. The size distribution of the colloidal spheres was determined by the concentrations of azo polymer and the amount of surfactant in the systems. When the concentrations of polymer and surfactant amount were in a proper range, colloidal spheres with narrow size distribution could be obtained. The colloidal spheres formed by this method could be elongated along the polarization direction of the laser beams to be a new type of the colloid-based functional materials. upon Ar^+ laser irradiation. The colloidal spheres are considered  相似文献   

8.
李宗木  徐法强 《中国化学》2005,23(3):337-340
Single-crystalline SnO2 nanowires have been successfully prepared in large scale on Au-coated silicon substrate by heating the mixture of self-made high-purity SnO2 powders and graphite powders at 900℃. Besides the line type nanowires some more features were observed. The products were characterized by means of X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), selected area electron diffraction (SAED) and Raman spectrum techniques. The results indicate that the tin dioxide nanowires have a rutile structure with diameters ranging from 30 to 120 nm and lengths up to several tens of micrometers. The possible mechanism of the growth and reaction for the nanowires was also discussed.  相似文献   

9.
电化学法制备硅纳米线   总被引:1,自引:0,他引:1  
Silicon nanowires were synthesized from nanometer silicon dioxide powder under potentiostatic electrolysis at -1.20 V (vs Pt reference) for 4 h in molten CaCl2 at 900 ℃. The morphology, structure and chemical composition of the samples prepared by electroreduction method were characterized by field-emission scanning electron microscopy(FE-SEM), High-resolution transmission electron microscopy(HRTEM) coupled with electron energy dispersive spectroscopy(EDS), laser Raman and X-ray diffraction(XRD). The results revealed that silicon nanowires were crystalline with a diamond cubic structure, the diameter was distributed from 50 nm to 80 nm and the length was generally several micrometers. The formed nanowires basically consisted of silicon monocrystalline and amorphous oxide sheath.  相似文献   

10.
Uniform CePO_4 nanowires with diameter of about 25 nm were synthesized by the water-in-oil microemulsion method at room temperature from cerous chloride,sodium orthophosphate,sodium chloride,cyclohexane,Triton X-100 and cetyltrimethyl ammonium bromide(CTAB).The crystal structure and morphology of the nanowires were characterized by XRD and TEM, respectively.The UV-vis absorption was detected by UV-vis spectrophotometer techniques.The results showed that as-prepared nanowires with the hexagonal phase have...  相似文献   