1.
A multiblock copolymer of polyethersulfone (PES) and polycarbonate (PC) was used as a compatibilizer for a blend of PES/PC. The morphology, thermal properties, mechanical properties, etc. of the resulting ternary blend systems were investigated. The addition of the compatibizer improved the compatibility between PES and PC. It was found that the interfacial adhesion was enhanced; the size of the dispersed phase was reduced and this resulted in an improvement of elongation at break and tenacity of PES/PC blends and tensile strength and tensile modulus were almost constant.  相似文献   

2.
Recycled poly(ethylene terephthalate) (R-PET) and virgin polyamide 6 (PA6) blends compatibilized with glycidyl methacrylate grafted poly(ethylene-octene) (POE-g-GMA) were melt blended. The morphological, rheological and mechanical properties of the prepared blends were investigated by scanning electron microscopy, rheology, and an electromechanical testing instrument, respectively. All of the blends showed a droplet dispersion type morphology, and the PA6 particle size decreased with increase in the POE-g-GMA concentration. The storage modulus (G′), loss modulus (G′′), and complex viscosity (η*) of the blends significantly increased at low frequency with the addition of POE-g-GMA. In addition, ‘‘Cole-Cole’’ plots showed that the elasticity of the blends was also increased by raising the compatibilizer dosage. It was also found that 10 wt% of POE-g-GMA caused 88.46 and 171.05% increments in Charpy impact strength and elongation at break with only a 21.66% decrement in tensile strength.  相似文献   

3.
Ethylene vinyl acetate copolymer (EVA), with vinyl acetate contents of 60% or 80%, was used to improve the mechanical properties of poly(hydroxybutyrate-co-hydroxyvalerate) (PHBV). Blends of PHBV/EVA were prepared with the ratios of 90:10, 70:30, and 50:50. Stress–strain results indicated that the tensile strength, elongation at break, Young's modulus, and toughness of PHBV blends could be adjusted by changing the composition of blends and miscibility. It was found that high elongation at break, ca. 200%, was obtained for PHBV/EVA80 (50:50).  相似文献   

4.
Blends of poly(vinyl chloride) (PVC) and poly(α-methylstyrene-acrylonitrile) (α-MSAN) with variable composition of 0 to 100 wt% were prepared by melt mixing. Properties of binary blends were extensively studied by differential scanning calorimetry (DSC), dynamic mechanical thermal analysis (DMTA), attenuated total reflection-Fourier transform infrared spectroscopy (ATR-FTIR), heat distortion temperature (HDT), mechanical properties, melt flow rate (MFR), and scanning electron microscope (SEM). A single glass transition temperature (Tg ) was observed by DSC and DMTA, indicating miscibility between PVC and α-MSAN. The results of ATR-FTIR indicated that specific strong interactions were not present in the blends and the miscibility was due to interaction between –CN and PVC. With increasing amount of α-MSAN, considerable increase occurred in HDT, flexural strength, and flexural modulus compared with reverse s-shaped decrease in impact strength and elongation at break. Synergism was observed in tensile strength and MFR. No phase separation was observed in SEM photographs, indicating miscibility between PVC and α-MSAN. In addition, morphology of the impact-fractured surfaces, including roughness and non-fused particles, correlated well with the mechanical properties and MFR.  相似文献   

5.
ABS/PMMA/PC (acrylonitrile-butadiene-styrene)/poly(methyl methacrylate)/bisphenol A polycarbonate) and ABS/PMMA/phenoxy ternary blends were prepared using a corotating twin-screw extruder, where the ABS content was fixed at 60% by weight, and the other ingredients varied 0 ~ 40%. Tensile modulus, yield strength, elongation at break, and notched impact strength varied linearly with compositions in ABS/PMMA/phenoxy blends, whereas positive synergisms of these properties were generally obtained with ABS/PMMA/PC blends. The results were interpreted in terms of interpositions of PMMA between ABS and PC, which were seen from the TEM micrographs and predicted from the spreading coefficient. Surface gloss of ABS increased in ABS/ PMMA(60/40) blend but decreased in ternary blends, and this phenomenon was possibly explained by the pearl gloss mechanism.  相似文献   

6.
A novel nanocomposite based on biodegradable poly(l-lactide) (PLLA) was prepared by the incorporation of surface modified magnesia (g-MgO) nanoparticles using a solution casting method. The mechanical properties, biodegradable properties and protein adhesion behavior of the g-MgO/PLLA nanocomposites were investigated. Scanning electron microscopy (SEM) results showed that g-MgO nanoparticles could comparatively uniformly disperse in PLLA matrix. The addition of g-MgO nanoparticles to PLLA matrix improved the tensile strength and elastic modulus, whereas reduced the elongation at break. The mass loss results showed that the nanocomposites with higher g-MgO content had faster degradation rates. The in vitro pH value determination results indicated that the g-MgO nanoparticles could neutralize effectively the lactic acid resulting from the degradation of PLLA. The g-MgO/PLLA nanocomposites exhibited enhanced protein adsorption, i.e., with the increase of g-MgO content, the amount of protein adsorption increased. The (5 wt%)g-MgO/PLLA nanocomposites adsorbed 33% more protein than the pure PLLA.  相似文献   

7.
Poly(ethylene glycol) (PEG) was added as a plasticizer to the composite of poly(lactic acid) (PLA) and a modified carbon black (MCB). Among the three different molecular weight (Mn = 1000, 2000, 6000) PEGs used, PEG2000 promoted crystallization of PLA and enhanced the nucleation activity of MCB more efficiently than the other two. The crystallization rate of PLA/PEG2000/3 wt% MCB composite was three times that of PLA. Although a small decrease in tensile strength and modulus of elasticity of the composite was found as the PEG content increased, the elongation at break of the PLA/PEG/MCB composites significantly improved. When the PEG2000 content was 15 wt%, the elongation at break of the blend was 90%, 4.5 times that of the neat PLA.  相似文献   

8.
A range of blends based on 70 wt% of poly(trimethylene terephthalate) PTT with 30 wt% dispersed phase were produced via melt blending. The dispersed phase composition was varied from pure maleic anhydride grafted poly(ethylene-octene) (POE-g-MA) over a range of POE-g-MA:polypropylene (PP) ratios. The micromorphology and mechanical properties of the ternary blends were investigated. The results indicated that the domains of the POE-g-MA are dispersed in the PTT matrix, and at the same time the POE-g-MA encapsulate the PP domains. The interfacial reaction between the hydroxyl-end group of PTT and maleic anhydride (MA) during melt blending changes the formation from “isolated formation” to “capsule formation,” where the PP domains are encapsulated by POE-g-MA. Compared to the PTT/POE-g-MA blends, mechanical properties of ternary blends, such as tensile strength and Young's modulus, were improved significantly.  相似文献   

9.
This study deals with some results on morphology, miscibility and mechanical properties for polymethyl methacrylate/polycarbonate (PMMA/PC) polymer blends prepared by solution casting method at different concentration between 0 and 100 wt%. Dynamic storage modulus and tan δ were measured in a temperature range from 30 to 180°C using dynamical mechanical analyzer (DMA). The value of the storage modulus was found to increase with the addition of the PC in the matrix. Transition temperature of pure PMMA and pure PC is found to be 83.8 and 150°C, respectively. The result shows that the two polymers are miscible for whole concentration of PC in PMMA. The distribution of the phases in the blends was studied through scanning electron microscopy (SEM). Also the mechanical properties like elongation at break and fracture energy of the PMMA/PC blends increase with the increase in concentration of PC in PMMA.  相似文献   

10.
Blend films of poly(N-vinyl-2-pyrrolidone) (PVP) and chitosan (CTS) were prepared by casting method from acetic acid solutions. All blend films obtained are optically clear to the naked eye. The structure and physical properties of the blend films were analyzed by attenuated total reflectance Fourier transform infrared spectroscopy (ATR-FTIR), thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), mechanical testing (Instron) and contact-angle measurements. The ATR-FTIR results indicated that there is no detectable band shifts at 1650 cm−1. From TGA studies, it was found that the onset degradation temperature of the blends almost unchanged due to the presence of a weak interaction between PVP and CTS chains. The DSC analysis showed a single glass transition temperature for all the blends, indicating that these polymers are miscible over the entire composition range. The mechanical properties of the blends, such as breaking stress and elongation at break and Young modulus were greatly affected with increase of CTS content. In addition, we found that the blends exhibit well defined contact angle titration curves from which the surface pKa values were determined. In conclusion, these experimental findings provide fundamental knowledge for the preparation of bioreactive surfaces of controlled reactivity on CTS based blends.  相似文献   

11.
《Composite Interfaces》2013,20(3):171-186
A comparative study of interfacial effects due to styrene-butadiene-based triblock copolymer (SEBS) addition and to corona treatment has been investigated for blends of polyethylene (PE) and polystyrene (PS). Blends of PS/PE covering a wide range of weight composition have been prepared in the molten state. Scanning electron microscopy demonstrated that moderate amounts of SEBS copolymer addition (2-5%) resulted in finer particle dispersion and in better interfacial adhesion between PE and PS phases. Tensile strength and elongation at break were also significantly improved. In the case of corona treatment of both polyethylene and polystyrene, the tensile strength of the blends increased while their elongation at break remained almost unchanged. The same trend was found when small amounts of corona-treated blend (5%) were added to the non-modified PS/PE blends. Rheological measurements revealed that corona treatment resulted in a decrease of dynamic shear viscosity of both PE and PS. From a view-point of morphological and mechanical properties, the triblock copolymer was found to be the more efficient modifier. Nevertheless, much higher tensile strengths, but lower elongations at break were obtained when the blends were modified by corona-treated SEBS copolymer. The results suggest that a combination of the two modification methods may be a promising route to enhance performance properties in the immiscible PS/PE system.  相似文献   

12.
The elastomeric chlorinated polyethylene (CPE) blended with a low melting point copolyamide (PA6/PA66/PA1010, PA) was prepared by a melt mixing technique. The mixing characteristics of the blends were analyzed from the rheographs. The influence of copolyamide (PA) content on the morphology, mechanical properties, crystallization and oil-resistance, and the addition of compatibilizers on the mechanical properties were also systematically investigated. Morphological examinations clearly revealed a two-phase system in which CPE/PA blends exhibit a cocontinuous morphology for 50/50 composition, and the continuous phase of PA turns into a disperse phase for 70/30, 80/20, and 90/10. There is a distinct interface between the two phases. The mechanical properties, crystallization, and oil-resistance have a strong dependence on the amount of PA. The blends with higher proportions of PA have superior mechanical properties; they are explained on the basis of the morphology of the blend and the cystallinity of PA. In addition, compatibilizers, including chlorinated polyethylene-graft-copolyamide (CPE-G-PA), chlorinated polyethylene-graft-maleic anhydride (CPE-G-MAH), ethylene-n-butyl acrylate-monoxide (EnBACO), and ethylene-n-butyl acrylate-monoxide-graft-maleic anhydride (EnBACO-g-MAH) were added into the blends. Tensile strength and elongation at break go through a maximum value at a compatibilizer resin content (on the basis of the total mass of the blend) of 20 wt% while the PA content is 30 wt%.  相似文献   

13.
Blends of ethylene-propylene diene terpolymer/acrylonitrile butadiene copolymer (EPDM/NBR) loaded with different types [(N326-HAF) and (N774-SRF)] and ratios of carbon black (CB) fillers were prepared. The mechanical properties of the EPDM/NBR rubber blends unloaded and loaded with different ratios of CB were investigated. Among the blends, the one with 75% EPDM and 25% NBR, both loaded and unloaded with CB, were found to exhibit the highest tensile strength and elongation at break. The observed changes in the mechanical properties of the blends were correlated to the morphology as observed by scanning electron microscopy. The changes of the electrical resistivity of the rubber blend composites during compression were investigated. The experimental results were explained from the position that an external pressure induces either an increase or decrease of the resistivity of the blend composites according to whether annihilation or creation of effective conductive paths occurs, respectively.  相似文献   

14.
Ethylene‐α‐olefin copolymer (POE)/polystyrene (PS)/poly(styrene‐b‐ethylene‐co‐butylene‐b‐styrene) (SEBS) blends were prepared via melt blending in a co‐rotating twin‐screw extruder. The effects of SEBS copolymer on the morphology and rheological and mechanical properties of the blends were studied. Scanning electron microscopy (SEM) photos showed that the addition of SEBS copolymer resulted in finer dispersion of PS particles in the POE matrix and better interfacial adhesion between POE and PS compared with POE/PS blends, which exhibited a very coarse morphology due to the immiscibility between them. Interestingly, the tensile strength increased from 12.5 MPa for neat POE to 23.5 MPa for the POE/PS/SEBS (60/10/30) blend, whereas the tensile strengths of POE/PS (85.7/14.3) blend and POE/SEBS (66.7/33.3) blend were only 10.5 and 16.5 MPa, respectively. This indicates that both SEBS copolymer and PS have a synergistic reinforcing effect on POE. Dynamic mechanical thermal analysis (DMTA) and dynamic rheological property measurement also revealed that there existed some interactions between POE and SEBS as well as between SEBS and PS. DMTA results also showed that the storage modulus of POE increased when PS and SEBS were incorporated, especially at high temperature, which means that the service temperature of POE was improved.  相似文献   

15.
Polypropylene (PP) blends based on isotactic polypropylene (iPP), propylene-ethylene block copolymer (bPP), and propylene–ethylene random copolymer (rPP) were prepared by melt blending and the effects of content of bPP and rPP on the shrinkage during solidification and storage and mechanical properties of the blends were studied. It was found that the addition of polypropylene copolymer could effectively reduce the processing shrinkage of iPP and the lowest shrinkage of the blends was achieved at a loading of 2 wt% bPP or rPP. The flexural modulus and tensile strength of the blends decreased a little while the impact strength and elongation at break were improved greatly compared with those of iPP.  相似文献   

16.
In this study the blends of polyethylene terephthalate (PET)/ethylene propylene diene rubber (EPDM) in the presence of multi-walled carbon nanotubes (MWCNT) (1 and 3?wt %) were prepared by melt compounding in an internal mixer. Mechanical and morphological properties of the nanocomposites were investigated. The thermal behaviors of the PET/EPDM nanocomposites were also investigated, by differential scanning calorimetry (DSC) and thermogravimetric analysis (TGA). The results of the mechanical tests showed that the tensile strength, elastic modulus and the hardness of the blends were increased with increasing CNT, while the impact strength and elongation at break decreased. The DSC and TGA results showed an increase of melting temperature (Tm) and degradation temperature of the nanocomposites with the addition of the carbon nanotubes, because the carbon nanotubes serve both as nucleating agents to increase Tm and prevent the composite from degradation to increase the thermal stability. The microstructure of the composites was evaluated through field emission scanning electron microscopy (FESEM) and the results showed a good distribution of the MWCNT within the polymer blend.  相似文献   

17.
Polypropylene (PP)/polyester (PES)–blend fibers were prepared by extruder melt spinning. The polymer blend consisted of PP and a “master batch” (MB) based on polytrimethylene terephthalate (PTT) or polyethylene terephthalate (PET), binary PTT/PET or PP/PTT blends, and also on a ternary PP/(PTT/PET) blend. The phase structure of PP/PES–blend fibers was examined. PES microfibers showed separation from the PP matrix in blend fibers. The impact of MB composition and rheological characteristics on phase structure parameters indicate a significant contribution of the PTT in the binary MB on the length of dispersed PES microfibers in the PP matrix. However, the blends of PP and ternary MB (PP/PTT/PET) have a lower diameter and length of the PES microfibers. The presence of PTT/PET (PES) enhances the structural and mechanical properties of the blend PP/PES fibers. In addition, PTT increases the tensile strength of the PP/PES–blend fibers if a binary MB is used, while the fiber nonuniformity is reduced in the presence of a ternary MB.  相似文献   

18.
Blends of two grades of acrylonitrile‐butadiene‐styrene (ABS) with three different compounds of poly (vinyl chloride) (PVC) were prepared via melt processing and their morphology, flammability, and physical and mechanical properties were investigated. SEM results showed that the ABS/PVC blend is a compatible system. Also, it can be inferred from fracture surface images that ABS/PVC blends are tough, even at low temperatures. It was found that properties of these blends significantly depend on blend composition and PVC compound type; however, the ABS types have only a small effect on blend properties. On blending of ABS with a soft PVC compound, impact strength, and melt flow index (MFI) increased, but tensile and flexural strength decreased. In contrast, blending of ABS with a rigid PVC compound improved fire retardancy and some mechanical properties and decreased MFI and impact strength.  相似文献   

19.
Abstract

Thermoplastic elastomers and their foams were prepared by blending elastomeric acrylonitrile butadiene rubber (NBR) and rigid poly(lactic acid) (PLA) with various PLA compositions ranging between 0 and 40%. The thermal and mechanical properties and the morphologies of the blends with various PLA contents were investigated through universal testing machine, differential scanning calorimetry, thermogravimetric analysis, and scanning electron microscope analysis. The rheological properties during gel formation were in situ monitored through the evolution of torque with curing time. Furthermore, the microcellular structures and physical properties of the NBR/PLA foams prepared using organic blowing agents were studied. The NBR/PLA blends showed a two-phase morphology made of a continuous NBR matrix and micron or submicron nodules and the tensile strength and modulus; also, hardness of the NBR/PLA blends increased with the increase of the added PLA content. While the foamed samples exhibited a similar cell structure and foaming ratio to that of the pure NBR, the cell formation was considerably reduced as the added PLA content exceeded 30%. We conclude that the mechanical properties of NBR thermoplastic elastomer as well as its foams can be controlled by a judicious introduction of rigid and biodegradable PLA.  相似文献   

20.
Thermoplastic elastomers (TPEs) based on ethylene-vinyl acetate (EVA)/waste nitrile butadiene rubber powder (WNBRP) blends compatibilized by chlorinated polyethylene (CPE) were prepared by melt-compounding. The tensile strength and the elongation at break of the EVA/CPE/WNBRP blends were increased significantly compared with those of the EVA/WNBRP blends. The fracture surfaces of the EVA/CPE/WNBRP blends were smooth; moreover, the WNBRP in the etched EVA/CPE/WNBRP blends were inserted in the EVA matrix tightly. DMA results revealed that when the CPE dosage was 5 phr in the EVA/CPE/WNBRP blend, the Payne effect was weakened significantly.  相似文献   