Degree of branching (DB) of AB2‐type hyperbranched polymer has been studied using 13C‐NMR spectroscopy. For this purpose, a series of hyperbranched polyamides based on 3,5‐bis(4‐aminophenoxy)benzoic acid differing in molecular weight was prepared by adopting a fractional precipitation technique. A model compound mimicking exactly the terminal and dendritic units present in the hyperbranched polymer (HBP) was also synthesized in high yield. 13C‐NMR spectra of the polymers and the model compound were recorded under exacting experimental conditions. With the help of 13C‐NMR spectrum of model compound and the integration values, peaks for terminal (T) units, dendritic (D) units and linear (L) units present in the HBP have been assigned. The spectra of low molecular weight fractions clearly showed that the linear unit is first formed and then the dendritic unit. Plots of mole fraction of individual unit against molecular weight (Mw) and DB against molecular weight (Mw) are constructed. For the first time, it is found that there is a critical molecular weight (the value calculated is between 3200–3500 for the chosen real system) below, which DB is dependent on molecular weight and above which it becomes independent. A new term T+D/L, which has a maximum value of 20 and minimum of 1, characterizing all AB2‐type hyperbranched polymers in general, has been introduced.  相似文献   

2.
Novel AB2‐type monomers such as 3,5‐bis(4‐methylolphenoxy)benzoic acid ( monomer 1 ), methyl 3,5‐bis(4‐methylolphenoxy) benzoate ( monomer 2 ), and 3,5‐bis(4‐methylolphenoxy)benzoyl chloride ( monomer 3 ) were synthesized. Solution polymerization and melt self‐polycondensation of these monomers yielded hydroxyl‐terminated hyperbranched aromatic poly(ether‐ester)s. The structure of these polymers was established using FTIR and 1H NMR spectroscopy. The molecular weights (Mw) of the polymers were found to vary from 2.0 × 103 to 1.49 × 104 depending on the polymerization techniques and the experimental conditions used. Suitable model compounds that mimic exactly the dendritic, linear, and terminal units present in the hyperbranched polymer were synthesized for the calculation of degree of branching (DB) and the values ranged from 52 to 93%. The thermal stability of the polymers was evaluated by thermogravimetric analysis, which showed no virtual weight loss up to 200 °C. The inherent viscosities of the polymers in DMF ranged from 0.010 to 0.120 dL/g. End‐group modification of the hyperbranched polymer was carried out with phenyl isocyanate, 4‐(decyloxy)benzoic acid and methyl red dye. The end‐capping groups were found to change the thermal properties of the polymers such as Tg. The optical properties of hyperbranched polymer and the dye‐capped hyperbranched polymer were investigated using ultraviolet‐absorption and fluorescence spectroscopy. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 5414–5430, 2008  相似文献   

3.
Hyperbranched poly(ether sulfone)s were prepared by the self‐polycondensation of the novel AB2 monomer, 4‐(3,5‐hydroxyphenoxy)‐4′‐fluorodiphenylsulfone. The high‐molecular‐weight polymers were isolated in good yields. The degree of branching (DB) of the resulting polymers was investigated by the preparation of dendritic and linear model compounds. The DB determined by gated decoupling 13C NMR measurements was in the range 0.17–0.41 and was dependent on the base used for the self‐polycondensation. It was found that cesium fluoride was an effective base to form the polymer having the DB of 0.41. The resulting hyperbranched poly(ether sulfone)s showed good solubility in organic solvents. The solubility and the glass transition temperature of the polymers were influenced by the terminal functional groups. The unique thermal crosslinking phenomenon was observed during the DSC measurements of the hydroxyl‐terminated hyperbranched poly(ether sulfone) under air condition. © 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2012  相似文献   

4.
A new method for the synthesis of hyperbranched polymers involving the use of ABx macromonomers containing linear units have been investigated. Two types of novel hyperbranched polyurethanes have been synthesized by a one‐pot approach. The structures of monomers and polymers were characterized by elemental analysis, 1H NMR, 13C NMR, Fourier transform infrared spectroscopy, gel permeation chromatography, and thermogravimetric analysis. The hyperbranched polymers have been proven to be extremely soluble in a wide range of solvents. Polymer electrolytes were prepared with hyperbranched polymer, linear polymer as the host, and lithium perchlorate (LiClO4) as the ion source. Analysis of the isotherm conductivity dependence of the ion concentration indicated that these hyperbranched polymers could function as a “solvent” for the lithium salt. The conductivity increased with the increasing concentration of hyperbranched polymers in the host polymer. © 2001 John Wiley & Sons, Inc. J Polym Sci Part A: Polym Chem 40: 344–350, 2002  相似文献   

5.
Starting from 3,5‐diamino benzoic acid, 2‐hydroxy propyl[3,5‐bis{(benzoxycarbonyl)imino}]benzyl ether, an AB2‐type blocked isocyanate monomer with flexible ether group, and 2‐hydroxy propyl[3,5‐bis{(benzoxycarbonyl)imino}]benzoate, an AB2‐type blocked isocyanate monomer with ester group, were synthesized for the first time. Using the same starting compound, 3,5‐bis{(benzoxycarbonyl)imino}benzylalcohol, an AB2‐type blocked isocyanate monomer, was synthesized through a highly efficient short‐cut route. Step‐growth polymerization of these monomers at individually optimized experimental conditions results in the formation of hyperbranched polyurethanes with and without ether and ester groups. Copolymerizations of these monomers with functionally similar AB monomers were also carried out. The molecular weights of the polymers were determined using GPC and the values (Mw) were found to vary from 1.5 × 104 to 1.2 × 106. While hyperbranched polyurethanes having no ether or ester group were found to be thermally stable up to 217 °C, hyperbranched poly(ether–urethane)s and poly(ester–urethane)s were found to be thermally stable up to 245 and 300 °C, respectively. Glass transition temperature (Tg) of polyurethane was reduced significantly when introducing ether groups into the polymer chain, whereas Tg was not observed even up to 250 °C in the case of poly(ester–urethane). Hyperbranched polyurethanes derived from all the three different AB2 monomers were soluble in highly polar solvents and the copolymers showed improved solubility. Polyethylene glycol monomethyl ether of molecular weight 550 and decanol were used as end‐capping groups, which were seen to affect the thermal, solution, and solubility properties of polymers. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 3877–3893, 2007  相似文献   

6.
Hyperbranched polymers are important soft nanomaterials but robust synthetic methods with which the polymer structures can be easily controlled have rarely been reported. For the first time, we present a one‐pot one‐batch synthesis of polytriazole‐based hyperbranched polymers with both low polydispersity and a high degree of branching (DB) using a copper‐catalyzed azide–alkyne cycloaddition (CuAAC) polymerization. The use of a trifunctional AB2 monomer that contains one alkyne and two azide groups ensures that all Cu catalysts are bound to polytriazole polymers at low monomer conversion. Subsequent CuAAC polymerization displayed the features of a “living” chain‐growth mechanism with a linear increase in molecular weight with conversion and clean chain extension for repeated monomer additions. Furthermore, the triazole group in a linear (L) monomer unit complexed CuI, which catalyzed a faster reaction of the second azide group to quickly convert the L unit into a dendritic unit, producing hyperbranched polymers with DB=0.83.  相似文献   

7.
Hyperbranched polyurethanes, with varying oligoethyleneoxy spacer segments between the branching points, have been synthesized by a one-pot approach starting from the appropriately designed carbonyl azide that incorporates the different spacer segments. The structures of monomers and polymers were confirmed by IR and 1H-NMR spectroscopy. The solution viscosity of the polymers suggested that they were of reasonably high molecular weight. Reversal of terminal functional groups was achieved by preparing the appropriate monohydroxy dicarbonyl azide monomer. The large number of terminal isocyanate groups at the chain ends of such hyperbranched macromolecules caused them to crosslink prior to its isolation. However, carrying out the polymerization in the presence of 1 equiv of a capping agent, such as an alcohol, resulted in soluble polymers with carbamate chain ends. Using a biphenyl-containing alcohol as a capping agent, we have also prepared novel hyperbranched polyurethanes with pendant mesogenic segments. These mesogen-containing polyurethanes, however, did not exhibit liquid crystallinity probably due to the wholly aromatic rigid polymer backbone. © 1996 John Wiley & Sons, Inc.  相似文献   

8.
Two different molecular weight hyperbranched polymers (HBP(L)-(PA)2 and HBP(H)-(PA)2) with two phosphonic acid groups as a functional group at the periphery and a low molecular weight hyperbranched polymer (HBP(L)-(PA)2-Ac) with both two phosphonic acid groups and an acryloyl group as a cross-linker at the periphery were successfully synthesized as thermally stable proton-conducting electrolytes. A cross-linked electrolyte membrane (CL-HBP(L)-(PA)2) was prepared by thermal polymerization of the HBP(L)-(PA)2-Ac using benzoyl peroxide. Ionic conductivities of the HBP(L)-(PA)2, the HBP(H)-(PA)2, and the CL-HBP(L)-(PA)2 under dry condition and their thermal properties were investigated, and also, the effect of the phosphonic acid group number on them was discussed. Ionic conductivities of the HBP(L)-(PA)2 and the HBP(H)-(PA)2 were found to be 1.5?×?10?5 S cm?1 at 150 °C and 3.6?×?10?6 S cm?1 at 143 °C, respectively, under dry condition, and showed the Vogel–Tamman–Fulcher type temperature dependence. The hyperbranched polymers and the cross-linked electrolyte membrane were thermally stable up to 300 °C, and the cross-linked electrolyte membrane (CL-HBP-(PA)2) had suitable thermal stability as an electrolyte membrane for the high-temperature fuel cells under dry condition. Fuel cell measurement using a single membrane electrode assembly cell with the cross-linked membrane was performed.  相似文献   

9.
Thermally stable hyperbranched polyamide-ethers (HBPAEs) containing pyrimidine moieties were synthesized using new AB2 type monomer, 6-hydroxy-2,4-bis(4′-nitrobenzamide)pyrimidine (NAL), which was prepared through amidation and its structural characterization was made by FTIR, 1H, 13C NMR spectrometry and elemental analysis. Polymerization of NAL proceeded homogeneously to yield a gel-free polymer (HBPAE 1). End group derivatization of nitro-terminated HBPAE 1 yielded HBPAE 2 and 3. FTIR confirmed the structure and complete modification of ensuing polymers. DB and inherent viscosity (ηinh) of HBPAE 1 was found to be 0.41 and 0.23 dL/g, respectively. Modified HBPAE 2 and 3 were soluble in various organic solvents including NMP, DMAc and DMSO but amorphous HBPAE 1 was partially soluble in DMF. Glass transition temperature (Tg) of thermally stable HBPAEs was affected by nature of end groups as well as introduction of pyrimidine rings.  相似文献   

10.
A convenient and cost‐effective strategy for synthesis of hyperbranched poly(ester‐amide)s from commercially available dicarboxylic acids (A2) and multihydroxyl secondary amine (CB2) has been developed. By optimizing the conditions of model reactions, the AB2‐type intermediates were formed dominantly during the initial reaction stage. Without any purification, the AB2 intermediate was subjected to thermal polycondensation in the absence of any catalyst to prepare the aliphatic and semiaromatic hyperbranched poly(ester‐amide)s bearing multi‐hydroxyl end‐groups. The FTIR and 1H NMR spectra indicated that the polymerization proceeded in the proposed way. The DBs of the resulting polymers were confirmed by a combination of inverse‐gated decoupling 13C NMR, and DEPT‐135 NMR techniques. The DBs of the hyperbranched poly(ester‐amide)s were in the range of 0.44–0.73, depending on the structure of the monomers used. The hyperbranched polymers exhibited moderate molecular weights with relatively broad distributions determined by SEC. All the polymers displayed low inherent viscosity (0.11–0.25 dL/g) due to the branched nature. Structural and end‐group effects on the thermal properties of the hyperbranched polymers were investigated using DSC. The thermogravimetric analysis revealed that the resulting polymers exhibit reasonable thermal stability. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 5077–5092, 2008  相似文献   

11.
In this article, our main goal is to combine hyperbranched polymer with β‐cyclodextrin (β‐CD) to establish a novel functional polymer species with core‐shell structure and supramolecular system for further application in inclusion technologies and the complex drugs delivery system. Therefore, two β‐CD polymer brushes based on hyperbranched polycarbosilane (HBP) as a hydrophobic core and poly(N,N‐dimethylaminoethyl methacrylate) (PDMA) carrying β‐CD units as a hydrophilic shell were synthesized. Hyperbranched polycarbosilane macroinitiator carrying ? Cl groups (HBP‐Cl) was also prepared by using 1,1,3,3‐tetrmethyldisiloxane, allyl alcohol, and chloroacetyl chloride as reagents. The molecular structures of HBP‐Cl macroinitiator and β‐CD polymer brushes were characterized by Fourier transform infrared spectroscopy (FTIR), 1H nuclear magnetic resonance (1H NMR), 13C nuclear magnetic resonance (13C NMR) spectroscopies, size exclusion chromatography/multi‐angle laser light scattering (SEC/MALLS) and laser particle size analyzer. The results indicate that the grafted chain length of two β‐CD polymer brushes can be controlled by changing the feed ratio. Differential scanning calorimetry (DSC) results show that two β‐CD polymer brushes have two glass transition temperatures (Tgs) from a hydrophobic core part and a hydrophilic shell part, respectively, and the Tg from PDMA is higher than that of HBP‐g‐PDMA. Thermalgravimetric analyzer (TGA) analysis indicates that the thermostability of two β‐CD polymer brushes is higher than that of HBP, but is lower than that of HBP‐g‐PDMA. Using phenolphthalein (PP) as a guest molecule, molecular inclusion behaviors for two β‐CD polymer brushes were studied. It reveals that two β‐CD polymer brushes possess molecular inclusion capability in PP buffer solution with a fixed concentration. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 5036–5052, 2008  相似文献   

12.
A new controllable approach to synthesize hyperbranched poly(siloxysilanes) via hydrosilylation of A2‐ and B′Bx‐type monomers was developed in this work. A2 monomers (dimethylbis(dimethylsiloxy)siloxane and tetramethyldisiloxane), B′Bx monomers (methylvinyldiallylsilane and vinyltriallylsilane), and the resultant hyperbranched poly(siloxysilanes) were well characterized using FTIR, 1H NMR, 13C NMR, 29Si NMR, and SEC/MALLS. The In situ FTIR results indicate that the controllable polymerization can be carried out quickly and the reaction process was obviously performed in two stages. At the first stage, silicon hydride selectively reacts with vinyl silane groups, which produces intermediate structures with one Si? H and two (or three) allyl groups. Consequently, at the second stage, these intermediates act as new AB2 (or AB3) type monomers and continue to be self‐polymerized to generate hyperbranched polymers. By this novel controllable approach, molecular weights and their polydispersity of the resulted hyperbranched poly(siloxysilanes) can be conveniently regulated via adjusting the process parameters, such as feeding ratio of two monomers. © 2008 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 46: 2708–2720, 2008  相似文献   

13.
Hyperbranched poly(ether nitrile)s were prepared from a novel AB2 type monomer, 2‐chloro‐4‐(3,5‐dihydroxyphenoxy)benzonitrile, via nucleophilic aromatic substitution. Soluble and low‐viscous hyperbranched polymers with molecular weights upto 233,600 (Mw) were isolated. According to the 1H NMR and GPC data, the unique polymerization behavior was observed, which implies that the weight average molecular weight increased after the number average molecular weight reached plateau region. Model compounds were prepared to characterize the branching structure. Spectroscopic measurements of the model compounds and the resulting polymers, such as 1H, DEPT 13C NMR, and MS, strongly suggest that the ether exchange reaction and cyclization are involved in the propagation reaction. The side reactions would affect the unique polymerization behavior. The resulting polymers showed a good solubility in organic solvents similar to other hyperbranched aromatic polymers. The hydroxy‐terminated polymer was even soluble in basic water. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 5835–5844, 2009  相似文献   

14.
Hyperbranched polymers consisting of aromatic or aliphatic polyether cores and epoxide chain‐end peripheries were prepared by proton transfer polymerization. AB2 diepoxyphenol monomer 1 proved to be well suited for the preparation of hyperbranched aromatic polymer 2 by this proton transfer polymerization. The use of chloride‐ion catalysis, rather than conventional base catalysis, for the preparation of polymers from diepoxyphenol 1 offered a unique method to control the ultimate molecular weight of the polymer product through variations of the initial concentration of monomer 1 in tetrahydrofuran. An alternative route to hyperbranched polyether epoxies made use of commercially available or easily prepared aliphatic monomers of the types AB2, AB3, and A2 + B3. Although these aliphatic polymerizations can be initiated with a base, chloride‐ion catalysis proved most effective for controlling the polymerization. The hyperbranched epoxies were characterized by NMR spectroscopy, gel permeation chromatography, and multi‐angle laser light scattering. Chemical modification of the polymers after polymerization was carried out via nucleophilic addition on the epoxide groups or derivatization of the hydroxy substituents within the hyperbranched polymer structure. Spectroscopic measurements suggested that some such ring‐opened materials may adopt reverse unimolecular micellar structures in appropriate solution environments. © 2000 John Wiley & Sons, Inc. J Polym Sci A: Polym Chem 38: 4850–4869, 2000  相似文献   

15.
Novel AB2‐type azide monomers such as 3,5‐bis(4‐methylolphenoxy)carbonyl azide (monomer 1) , 3,5‐bis(methylol)phenyl carbonyl azide (monomer 2) , 4‐(methylol phenoxy) isopthaloyl azide (monomer 3) , and 5‐(methylol) isopthaloyl azide (monomer 4) were synthesized. Melt and solution polymerization of these monomers yielded hydroxyl‐ and amine‐terminated hyperbranched polyurethanes with and without flexible ether groups. The structures of theses polymers were established using FT‐IR and NMR spectroscopy. The molecular weights (Mw) of the polymers were found to vary from 3.2 × 103 to 5.5 × 104 g/mol depending on the experimental conditions used. The thermal properties of the polymers were evaluated using TGA and DSC: the polymer obtained from monomer ( 1 ) exhibited lowest Tg and highest thermal stability and the polymer obtained from monomer ( 2 ) registered the highest Tg and lowest thermal stability. All the polymers displayed fluorescence maxima in the 425–525 nm range with relatively narrow peak widths indicating that they had pure and intense fluorescence. Also, the polymers formed charge transfer (CT) complexes with electron acceptor molecules such as 7,7,8,8‐tetracyano‐quino‐dimethane (TCNQ) and 1,1,2,2‐tetracyanoethane (TCNE) as evidenced by UV‐visible spectra. © 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 47: 3337–3351, 2009  相似文献   

16.
A series of novel hyperbranched polyselenides and polytellurides with multiple catalytic sites at the branching units has been synthesized via the polycondensation of A2 + B3 monomers. The GPx‐like activities of these polymer mimics were assessed and it was found that the polytellurides showed higher GPx‐like activities than the corresponding polyselenides. Interestingly, the polymers with higher molecular weights and degree of branching (DB) showed higher GPx‐like activities than the analogous lower molecular weight polymer. The enhancement in the catalytical activity of the hyperbranched polymers with increasing molecular weight affirmed the importance of the incorporation of multiple catalytic groups in the macromolecule which increases the local concentration of catalytic sites.  相似文献   

17.
3,5‐bis(4‐aminophenoxy)phenyl phenylcarbamate—a novel AB2‐type blocked isocyanate monomer and 3,5‐bis{ethyleneoxy(4‐aminophenoxy)}phenyl carbonyl azide—a novel AB2‐type azide monomer were synthesized in high yield. Step‐growth polymerization of these monomers were found to give a first example of hyperbranched poly (aryl‐ether‐urea) and poly(aryl‐alkyl‐ether‐urea). Molecular weights (Mw) of the polymer were found to vary from 1,858 to 52,432 depending upon the monomer and experimental conditions used. The polydispersity indexes were relatively narrow due to the controlled regeneration of isocyanate functional groups for the polymerization reaction. The degree of branching (DB) was determined using 1H‐NMR spectroscopy and the values ranged from 87 to 54%. All the polymers underwent two‐stage decomposition and were stable up to 300 °C. Functionalized end‐capping of poly(aryl‐ether‐urea) using phenylchloroformate and di‐t‐butyl dicarbonate (Boc)2O changed the thermal properties and solubility of the polymers. Copolymerization of AB2‐type blocked isocyante monomer with functionally similar AB monomer were also carried out. The molecular weights of copolymers were found to be in the order of 6 × 105 with narrow dispersity. It was found that the Tg's of poly(aryl‐alkyl‐ether‐urea)s were significantly less (46–49 °C) compared to poly(aryl‐ether‐urea)s. Moreover the former showed melting transition at 154 °C, which was not observed in the latter case. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 2959–2977, 2007  相似文献   

18.
A new straightforward strategy for synthesis of novel hyperbranched poly (ether amide)s from readily available monomers has been developed. By optimizing the reaction conditions, the AB2‐type monomers were formed dominantly during the initial reaction stage. Without any purification, the AB2 intermediate was subjected to further polymerization in the presence (or absence) of an initiator, to prepare the hyperbranched polymer‐bearing multihydroxyl end‐groups. The influence of monomer, initiator, and solvent on polymerization and the molecular weight (MW) of the resultant polymers was studied thoroughly. The MALDI–TOF MS of the polymers indicated that the polymerization proceeded in the proposed way. Analyses of 1H NMR and 13C NMR spectra revealed the branched structures of the polymers obtained. These polymers exhibit high‐moderate MWs and broad MW distributions determined by gel permeation chromatography (GPC) in combination with triple detectors, including refractive index, light scattering, and viscosity detectors. In addition, the examination of the solution behavior of these polymers showed that the values of intrinsic viscosity [η] and the Mark–Houwink exponent α were remarkably lower compared with their linear analogs, because of their branched nature. © 2007 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 45: 4309–4321, 2007  相似文献   

19.
N-三羟甲基甲基氨基乙磺酸(TES)的胺基与异佛尔酮二异氰酸酯(IPDI)环上活性较高的NCO在低温15℃下发生选择性反应,生成AB3型单体.随后提高反应温度(70~90℃),使AB3型单体原位聚合,一锅法合成出含磺酸基超支化聚氨酯.随着聚合温度的提高,超支化聚氨酯的支化度、分子量及分子量分布系数变大.90℃时,聚合产物的Mn为22410,支化度达到0.87.以此含磺酸基超支化聚氨酯为基础制得的聚合物电解质膜具有良好的耐热性、机械强度,其锂盐室温(约25℃)的离子电导率为3.1×10-5S/cm,100℃达到1.4×10-3 S/cm.  相似文献   

20.
Two UV‐curable hyperbranched poly(siloxysilane)s ( I and III ) containing vinyl and allyl end groups were synthesized via polyhydrosilylation with methylbis(methylethylvinylsiloxy)silane and methylbis(dimethylallylsiloxy)silane monomers. A cationic UV‐curable hyperbranched polymer ( II‐Ep ) with epoxy end groups was prepared via the hydrosilylation of hyperbranched polymer II with Si? H terminated groups and glycidyl methacrylate, and II was also obtained via the polyhydrosilylation of AB2‐type monomer methylvinylbis(methylethylsiloxy)silane. All hydrosilylation reactions were catalyzed by Pt/C or chloroplatinic acid. Three AB2‐type monomers were synthesized via the hydrolysis of functional chlorosilane, which was prepared with Grignard reagents and dichlorosilane. The molecular structures of the polymers were characterized with 1H NMR, Fourier transform infrared, and gel permeation chromatography, and the UV‐curing behaviors of the polymers under different atmospheres and with different photoaccelerators were also investigated. The thermostability of uncured and cured polymers was examined with thermogravimetric analysis, and the data indicated that the orders of the onset decomposition temperatures for the cured polymers and the residue weights were as follows: III (380 °C) > I (320 °C) > II‐Ep (280 °C) and I (70.4%) > III (64.1%) > II‐Ep (60.9%), respectively. © 2005 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 43: 1883–1894, 2005  相似文献   