1.
The carbon coated Fe3O4 nanoparticles (Fe3O4/C) were synthesized by a simple hydrothermal reaction and applied as solid-phase extraction (SPE) sorbents to extract trace polycyclic aromatic hydrocarbons (PAHs) from environmental water samples. The Fe3O4/C sorbents possess high adsorption capacity and extraction efficiency due to strong adsorption ability of carbon materials and large surface area of nanoparticles, and only 50 mg of sorbents are required to extract PAHs from 1000 mL water samples. The adsorption attains equilibrium rapidly and analytes are eluted with acetonitrile readily. Salinity and solution pH have no obvious effect on the recoveries of PAHs, which avoids fussy adjustment to water sample before extraction. Under optimized conditions, the detection limits of PAHs are in the range of 0.2–0.6 ng L−1. The accuracy of the method was evaluated by the recoveries of spiked samples. Good recoveries (76–110%) with low relative standard deviations from 0.8% to 9.7% are achieved. This new SPE method provides several advantages, such as high extraction efficiency, high breakthrough volumes, convenient extraction procedure, and short analysis times. To our knowledge, this is the first time that Fe3O4/C nanoparticles are used for the pretreatment of environmental water samples.  相似文献   

2.
Polyaniline (PANI) nanotubes containing Fe3O4 nanoparticles were synthesized under ultrasonic irradiation of the aqueous solutions of aniline, ammonium peroxydisulfate (APS), phosphoric acid (H3PO4), and the quantitative amount of Fe3O4. It was found that the obtained samples had the morphologies of nanotubes. TEM images and selected area electronic diffractions showed that Fe3O4 nanoparticles were embedded in PANI nanotubes. We thought that the mechanism of the formation of PANI/Fe3O4 nanotubes could be attributed to the ultrasonic irradiation and the H3PO4-aniline salt template. The molecular structure of PANI/Fe3O4 nanotubes were characterized by Fourier transform infrared spectroscopy (FTIR), UV-vis absorption spectra and X-ray diffraction (XRD). The conductivity and magnetic properties of the PANI nanotubes containing Fe3O4 nanoparticles were also investigated.  相似文献   

3.
A magnetic carbon nanomaterial for Fe3O4 enclosure hydroxylated multi-walled carbon nanotubes (Fe3O4-EC-MWCNTs-OH) was prepared by the aggregating effect of Fe3O4 nanoparticle on MWCNTs-OH, and combined with high-performance liquid chromatography (HPLC)/diode array detection (DAD) to determine the aconitines (aconitine, hypaconitine and mesaconitine) in human serum samples. Compared with other extraction modes investigated in experiment, Fe3O4-EC-MWCNTs-OH sorbents showed a good affinity to target analytes. Some important parameters that could influence extraction efficiency of aconitines, including the extraction mode, amounts of Fe3O4-EC-MWCNTs-OH, pH of sample solution, extraction time, desorption solvent and desorption time, were optimized. Under optimal conditions, the recoveries of spiked serum samples were between 98.0% and 103.0%; relative standard deviations (RSDs) ranged from 0.9% to 6.2%. The correlation coefficients varied from 0.9996 to 0.9998. The limits of detection ranged from 3.1 ng mL−1 to 4.1 ng mL−1 at a signal-to-noise ratio of 3. The experimental results showed that the proposed method was feasible for the analysis of aconitines in serum samples.  相似文献   

4.
In the present work, a novel type of superparamagnetic nanosorbent, polythiophene-coated Fe3O4 nanoparticles (Fe3O4@PTh NPs), have been successfully synthesized. The synthesized NPs were characterized by scanning electron microscopy (SEM), Fourier transform-infrared (FT-IR) spectroscopy, and thermal gravimetric analysis (TGA). The synthesized Fe3O4@PTh NPs were applied as an efficient sorbent for extraction and preconcentration of several typical plasticizer compounds (di-n-butyl phthalate (DBP), di-(2-ethylhexyl) phthalate (DEHP), and dioctyl adipate (DOA)) from environmental water samples. Separation of Fe3O4@PTh NPs from the aqueous solution was simply achieved by applying external magnetic field. Separation and determination of the extracted plasticizers was performed by gas chromatography–flame ionization detection (GC–FID). Several variables affecting the extraction efficiency of the analytes i.e., amount of NPs sorbent, salt concentration, extraction time, and desorption conditions were investigated and optimized. The best working conditions were as follows: amount of sorbent, 100 mg; NaCl concentration, 30% (w/v); sample volume, 45 mL; extraction time, 10 min; and 100 μL of ethyl acetate for desorption of the analytes within 2 min. Under optimized conditions, preconcentration factors for DBP, DEHP, and DOA were obtained as 86, 194, and 213, respectively. The calibration curves were linear (R2 > 0.998) in the concentration range of 0.4–100 μg L−1 for both DEHP and DOA and 0.7–100 μg L−1 for DBP. The limits of detection (LODs) were obtained in the range of 0.2–0.4 μg L−1. The intra-day relative standard deviations (RSDs%) based on four replicates were obtained in the range of 4.0–12.3%. The proposed procedure was applied to analysis of water samples including river water, bottled mineral water, and boiling water exposed to polyethylene container (after cooling) and recoveries between 85 and 99% and RSDs lower than 12.8% were obtained.  相似文献   

5.
Polythiophene (PT) was used as a surface modifier of graphene/Fe3O4 (G/Fe3O4) composite to increase merit of it, and also overcome some limitations and disadvantages of using G/Fe3O4 alone as solid phase extraction (SPE) sorbent. An in-situ chemical polymerization method was employed to prepare G/Fe3O4@PT nanocomposites. Application of this newly designed material in the magnetic SPE (MSPE) of polycyclic aromatic hydrocarbons (PAHs), as model analytes, in the environmental water samples was investigated. The characterization of the hybrid material was performed using transmission electron microscopy, scanning electron microscopy, energy-dispersive X-ray analysis, Fourier transform-infrared (FT-IR) spectroscopy and vibrating sample magnetometry. Seven important parameters, affecting the extraction efficiency of PAHs, including: amount of adsorbent, adsorption and desorption times, type and volume of the eluent solvent, initial sample volume and salt content of the sample were evaluated. The optimum extraction conditions were obtained as: 4 min for extraction time, 20 mg for sorbent amount, 100 mL for initial sample volume, toluene as desorption solvent, 0.6 mL for desorption solvent volume, 6 min for desorption time and 30% (w/v) for NaCl concentration. Good performance data were obtained at the optimized conditions. Detection limits were in the range of 0.009–0.020 μg L−1 in the real matrix. The calibration curves were linear over the concentration ranges from 0.03 to 80 μg L−1 with correlation coefficients (R2) between 0.995 and 0.998 for all the analytes. Relative standard deviations were ranged from 4.3 to 6.3%. Appropriate recovery values, in the range of 83–107%, were also obtained for the real sample analysis.  相似文献   

6.
An electrochemical immunosensor, basing on a dual amplification strategy by employing a biocompatible Fe3O4/polyaniline/Nafion (Fe3O4/PANI/Nafion) layer as sensor platform and multi-enzyme-antibody functionalized highly-carbonized spheres (multi-HRP-HCS-Ab2) as label, was constructed for sensitive detection of benzo[a]pyrene (BaP). The stable film, Fe3O4/PANI/Nafion, can not only immobilize biomolecules, but also catalyze the reduction of hydrogen peroxide, indicating an accelerated electron transfer pathway of the platform. The experimental conditions, including the concentration of Nafion, concentration of Fe3O4/polyaniline (Fe3O4/PANI), pH of the detection solution and concentrations of biomolecules, were studied in detail. Basing on a competitive immunoassay, the current change was proportional to the logarithm of BaP concentration in the range of 8 pM and 2 nM with the detection limit of 4 pM. The proposed immunosensor exhibited acceptable reproducibility and stability. This new type of dual amplification strategy may provide potential applications for the detection of environmental pollutants.  相似文献   

7.
Wang S  Bao H  Yang P  Chen G 《Analytica chimica acta》2008,612(2):182-189
In this report, a four-component nanocomposite, trypsin-immobilized polyaniline-coated Fe3O4/carbon nanotube composite, was synthesized for highly efficient protein digestion. Fe3O4 was deposited by the chemical coprecipitation of Fe2+ and Fe3+ in an alkaline solution containing carbon nanotubes (CNTs) to prepare nano-Fe3O4/CNT composite. Subsequently, polyaniline (PA) was assembled on the Fe3O4/CNT composite by the in situ polymerization of aniline in the presence of trypsin to obtain trypsin-immobilized PA/Fe3O4/CNT nanocomposite. The novel 1D superparamagnetic biomaterial has been characterized by TEM, SEM, XRD, and magnetometric analysis. The feasibility and performance of the unique magnetic biomaterial have been demonstrated by the tryptic digestion of bovine serum albumin, myoglobin, and lysozyme within 5 min. The digests were identified by MALDI-TOF MS with sequence coverages that were comparable to those obtained from the conventional in-solution tryptic digestion. The present biocomposite offers considerable promise for protein analysis due to its high magnetic responsivity and excellent dispersibility. It can be easily isolated from the digests with the aid of an external magnetic field. Because the enzyme-immobilized nanocomposite can be prepared by a simple two-step deposition approach at low cost, it may find a wide range of biological applications including proteome research.  相似文献   

8.
张霞  陈莉  周春彬 《无机化学学报》2010,26(11):1934-1938
借助于PANI的还原性质,PANI/Fe2O3复合载体与AgNO3发生表面氧化还原反应,合成了Ag/PANI/Fe2O3复合纳米粒子。TEM和XRD结果表明,立方晶系纳米银的平均粒径10nm。FTIR结果表明,Ag与PANI及Fe2O3复合载体之间不存在化学键合作用,但由于PANI与Ag之间的电子相互作用,Ag/PANI/Fe2O3复合纳米粒子的FTIR吸收峰发生蓝移。Ag/PANI/Fe2O3复合纳米粒子对于间硝基苯磺酸钠的硼氢化钠还原反应表现出良好的催化活性,30min内间硝基苯磺酸钠的转化率达到86.77%。  相似文献   

9.
Small molecules or analytes present at low concentrations are difficult to detect directly using conventional surface plasmon resonance (SPR) techniques because only small changes in the refractive index of the medium are typically induced by the binding of these analytes. Here, we present an amplification technique using core–shell Fe3O4@Au magnetic nanoparticles (MNPs) for an SPR bioassay. To evaluate this amplification effect, a novel SPR sensor based on a sandwich immunoassay was developed to detect α-fetoprotein (AFP) by immobilizing a primary AFP antibody (Ab1) on the surface of a 3-mercapto-1-propanesulfonate/chitosan-ferrocene/Au NP (MPS/CS-Fc/Au NP) film employing Fe3O4@Au–AFP secondary antibody conjugates (Fe3O4@Au–Ab2) as the amplification reagent. The stepwise fabrication of the biosensor was characterized using UV-vis spectroscopy, electrochemical impedance spectroscopy, and cyclic voltammetry. A calibration curve of Fe3O4@Au–Ab2 conjugates amplification for AFP detection was obtained to yield a correlation in the range of 1.0–200.0 ng mL−1 with a detection limit of 0.65 ng mL−1, and a significant increase in sensitivity was therefore afforded through the use of Fe3O4@Au–Ab2 conjugates as an amplifier. This magnetic separation and amplification strategy has great potential for the detection of other biomolecules of interest with low interference and high sensitivity by changing the antibody label used in the Fe3O4@Au–antibody conjugates.  相似文献   

10.
A series of spinel-type CoxNi1−xFe2O4 (x = 0, 0.2, 0.4, 0.5, 0.6, 0.8, 1.0) magnetic nanomaterials were solvothermally synthesized as enzyme mimics for the eletroctrocatalytic oxidation of H2O2. X-ray diffraction and scanning electron microscope were employed to characterize the composition, structure and morphology of the material. The electrochemical properties of spinel-type CoxNi1−xFe2O4 with different (Co/Ni) molar ratio toward H2O2 oxidation were investigated, and the results demonstrated that Co0.5Ni0.5Fe2O4 modified carbon paste electrode (Co0.5Ni0.5Fe2O4/CPE) possessed the best electrocatalytic activity for H2O2 oxidation. Under optimum conditions, the calibration curve for H2O2 determination on Co0.5Ni0.5Fe2O4/CPE was linear in a wide range of 1.0 × 10−8–1.0 × 10−3 M with low detection limit of 3.0 × 10−9 M (S/N = 3). The proposed Co0.5Ni0.5Fe2O4/CPE was also applied to the determination of H2O2 in commercial toothpastes with satisfactory results, indicating that CoxNi1−xFe2O4 is a promising hydrogen peroxidase mimics for the detection of H2O2.  相似文献   

11.
通过简易的超声法以及原位还原法成功制备出了负载型可再生Au/Fe3O4催化剂。利用3-氨丙基三乙氧基硅烷(APTES)作为有机桥键,将Au固定在Fe3O4的表面,得到单分散磁性Au/Fe3O4。Au0在氨基的作用下不会团聚,因此具有较高的催化活性及稳定性。XRD、HRTEM、EDS和XPS等测试结果表明Au/Fe3O4已被成功制备。将其用于催化还原4-硝基苯酚得到4-氨基苯酚,表现出较高的催化活性,速率常数可达0.225 6 min-1。重复性实验表明该催化剂具有良好的稳定性,反应9个循环之后,催化还原反应的转化率仍可达到94%。  相似文献   

12.
通过简易的超声法以及原位还原法成功制备出了负载型可再生Au/Fe_3O_4催化剂。利用3-氨丙基三乙氧基硅烷(APTES)作为有机桥键,将Au固定在Fe_3O_4的表面,得到单分散磁性Au/Fe_3O_4。Au0在氨基的作用下不会团聚,因此具有较高的催化活性及稳定性。XRD、HRTEM、EDS和XPS等测试结果表明Au/Fe_3O_4已被成功制备。将其用于催化还原4-硝基苯酚得到4-氨基苯酚,表现出较高的催化活性,速率常数可达0.225 6 min~(-1)。重复性实验表明该催化剂具有良好的稳定性,反应9个循环之后,催化还原反应的转化率仍可达到94%。  相似文献   

13.
通过焙烧-超声混合法成功地制备了BiOBr/g-C3N4S型异质结复合光催化剂。采用多种表征手段对样品物理属性进行了表征,包括X射线多晶粉末衍射仪(XRD)、扫描电子显微镜(SEM)、X射线光电子能谱(XPS)、紫外可见漫反射光谱(UV-Vis DRS)。研究了所制备样品有/无Fe3+的光-自芬顿催化/光催化降解罗丹明B(RhB)性能。通过捕获实验确定了光催化反应中的主要活性物种,提出了光-自芬顿反应的降解机理。研究结果表明,BiOBr/g-C3N4S型异质结能原位生成H2O2,添加Fe3+后,H2O2被原位活化成活性物种且光生电流和载流子分离效率获得显著提高。该光-自芬顿过程能高效降解RhB,其反应速率常数为0.208 min-1,约为无Fe3+光催化反应速率常数的5.3倍,在光-自芬顿循环使用过程中表现出良好的稳定性。Fe...  相似文献   

14.
A boronate-decorated nanomagnetic organic-inorganic hybrid material was facilely synthesized by utilizing the nanomagnetic polyhedral oligomeric silsesquioxanes (POSS) composite (Fe3O4@POSS) as the base platform. A simple copolymerization occurred between 3-acrylamidophenylboronic acid (AAPBA) and the residual end vinyl groups supplied by the substrate. Here the special emphasis was placed on the octavinyl POSS, which not only acted as the building blocks for a hybrid architecture but also facilitated the process of grafting boronate groups onto the surface of POSS based nanomagnetic composite (Fe3O4@POSS). The successful immobilization of affinity ligand-AAPBA on the Fe3O4@POSS was confirmed by Fourier transform infrared (FT-IR), elemental analysis, inductively coupled plasma atomic emission spectrometer (ICP-AES), field emission scanning electron microscope. A magnetic solid-phase extraction (MSPE) for cis-diols enrichment was developed using the as-prepared Fe3O4@POSS-AAPBA material as an affinity sorbent and three catecholamines (CAs), namely noradrenaline, epinephrine and isoprenaline, as model analytes. Under the optimal extraction conditions, sensitive and simultaneous analysis of three CAs from the urine sample was achieved by high-performance liquid chromatography with UV detection (HPLC-UV). The limits of detection (LOD, S/N = 3) and the limits of quantitation (LOQ, S/N = 10) for the target analytes were 0.81–1.32 ng mL−1 and 2.70–4.40 ng mL−1, respectively. Also good recoveries (85.5–101.7%) and repeatability (RSD≤10.1%) were obtained by this method. This work not only showed a facility for the utilization of Fe3O4@POSS as a substrate for constructing a boronate functionalized nanomagnetic sorbent, but also demonstrated the capability of the derived material for recognition of trace amount of cis-diols biomolecules presented in complicated biological matrices.  相似文献   

15.
以天然凹凸棒(ATP)为载体,分别利用机械混合法、浸渍法和溶胶-凝胶法制备了3种铁基复合载氧体。利用X射线衍射(XRD)、能谱(EDS)、N2-吸附脱附等温线等对其进行物化表征,并在900 ℃流化床中考察其煤化学链燃烧反应性能。结果表明,ATP能显著增加载氧体比表面积和抗磨损能力,并对煤转化过程有催化作用,其与Fe2O3的协同作用使初始碳转化速率显著提高。溶胶-凝胶法制备的U-Fe4ATP6表面Ca元素含量为4.3%,比表面积为4.920 7 m2/g,均高于其他两种载氧体,表现出更高的催化性能和反应活性:初始碳转化速率为0.168 min-1,平均CO2浓度为98.6%,燃烧效率为98.7%。20次反应后,U-Fe4ATP6催化性能略有降低,对应的初始碳转化速率降至0.108 min-1,停留时间t95延长到18 min;且能维持较高的反应活性,对应的CO2捕集效率和燃烧效率分别稳定在98.6%和96.7%。  相似文献   

16.
A novel magnetic solid-phase extraction (MSPE) sorbent, magnetite/silica/poly (methacrylic acid–co-ethylene glycol dimethacrylate) (Fe3O4/SiO2/P(MAA-co-EGDMA)), was developed. This MSPE material was prepared by distillation–precipitation polymerization of MAA and EGDMA in the presence of Fe3O4/SiO2 microspheres with the surface containing abundant reactive double bonds. The resultant sorbent material was characterized by elemental analysis, electron microscopy, X-ray diffraction and Fourier-transformed infrared spectroscopy. In this work, eleven sulfonamides (SAs) were selected as model analytes to validate the extraction performance of this new MSPE sorbent. Noticeably, the extraction can be carried out quickly, the extraction time for the SAs onto Fe3O4/SiO2/P(MAA-co-EGDMA) sorbent can be clearly shortened to 0.5 min. The desorption solution of SAs was analyzed by LC–MS/MS, and the results showed that the recoveries of these compounds were in the range of 87.6–115.6%, with relative standard deviations ranging between 0.9% and 10.8%; the limit of detection were in the range of 0.5–49.5 ng/L.  相似文献   

17.
In-tube magnetic solid phase microextraction (in-tube MSPME) of fluoroquinolones from water and urine samples based on the use of sodium dodecyl sulfate (SDS) coated Fe3O4 nanoparticles packed tube has been reported. After the preparation of Fe3O4 nanoparticles (NPs) by a batch synthesis, these NPs were introduced into a stainless steel tube by a syringe and then a strong magnet was placed around the tube, so that the Fe3O4 NPs were remained in the tube and the tube was used in the in-tube SPME-HPLC/UV for the analysis of fluoroquinolones in water and urine samples. Plackett–Burman design was employed for screening the variables significantly affecting the extraction efficiency. Then, the significant factors were more investigated by Box–Behnken design. Calibration curves were linear (R2 > 0.990) in the range of 0.1–1000 μg L−1 for ciprofloxacin (CIP) and 0.5–500 μg L−1 for enrofloxacin (ENR) and ofloxacin (OFL), respectively. LODs for all studied fluoroquinolones ranged from 0.01 to 0.05 μg L−1. The main advantages of this method were rapid and easy automation and analysis, short extraction time, high sensitivity, possibility of fully sorbent collection after analysis, wide linear range and no need to organic solvents in extraction.  相似文献   

18.
以有机碱四甲基氢氧化铵(TMAH)为沉淀剂合成了纳米Fe3O4和Co2+掺杂的纳米Fe3O4粒子。分别讨论了碱用量,铁盐溶液浓度,反应温度,有机碱及PEG-4000的分散性等因素对纳米Fe3O4的形貌影响。结果表明,所合成的纳米Fe3O4为30nm左右的反尖晶石型面心立方结构,有机碱除了起沉淀剂作用,还能够提高纳米Fe3O4的分散性。本文还讨论了不同Co2+掺入量的纳米Fe3O4粒子的磁性质,结果表明Co2+掺杂的纳米Fe3O4粒子的矫顽力在不同掺入量的下有较大的改变。当Co2+掺入量为10.0%时,纳米Fe3O4的矫顽力达到最大值,为1628Oe。  相似文献   

19.
Phase transitions in MgAl2O4 were examined at 21-27 GPa and 1400-2500 °C using a multianvil apparatus. A mixture of MgO and Al2O3 corundum that are high-pressure dissociation products of MgAl2O4 spinel combines into calcium-ferrite type MgAl2O4 at 26-27 GPa and 1400-2000 °C. At temperature above 2000 °C at pressure below 25.5 GPa, a mixture of Al2O3 corundum and a new phase with Mg2Al2O5 composition is stable. The transition boundary between the two fields has a strongly negative pressure-temperature slope. Structure analysis and Rietveld refinement on the basis of the powder X-ray diffraction profile of the Mg2Al2O5 phase indicated that the phase represented a new structure type with orthorhombic symmetry (Pbam), and the lattice parameters were determined as a=9.3710(6) Å, b=12.1952(6) Å, c=2.7916(2) Å, V=319.03(3) Å3, Z=4. The structure consists of edge-sharing and corner-sharing (Mg, Al)O6 octahedra, and contains chains of edge-sharing octahedra running along the c-axis. A part of Mg atoms are accommodated in six-coordinated trigonal prism sites in tunnels surrounded by the chains of edge-sharing (Mg, Al)O6 octahedra. The structure is related with that of ludwigite (Mg, Fe2+)2(Fe3+, Al)(BO3)O2. The molar volume of the Mg2Al2O5 phase is smaller by 0.18% than sum of molar volumes of 2MgO and Al2O3 corundum. High-pressure dissociation to the mixture of corundum-type phase and the phase with ludwigite-related structure has been found only in MgAl2O4 among various A2+B3+2O4 compounds.  相似文献   

20.
Fe2O3/SiO2 nanocomposites based on fumed silica A-300 (SBET = 337 m2/g) with iron oxide deposits at different content were synthesized using Fe(III) acetylacetonate (Fe(acac)3) dissolved in isopropyl alcohol or carbon tetrachloride for impregnation of the nanosilica powder at different amounts of Fe(acac)3 then oxidized in air at 400–900 °C. Samples with Fe(acac)3 adsorbed onto nanosilica and samples with Fe2O3/SiO2 including 6–17 wt% of Fe2O3 were investigated using XRD, XPS, TG/DTA, TPD MS, FTIR, AFM, nitrogen adsorption, Mössbauer spectroscopy, and quantum chemistry methods. The structural characteristics and phase composition of Fe2O3 deposits depend on reaction conditions, solvent type, content of grafted iron oxide, and post-reaction treatments. The iron oxide deposits on A-300 (impregnated by the Fe(acac)3 solution in isopropanol) treated at 500–600 °C include several phases characterized by different nanoparticle size distributions; however, in the case of impregnation of A-300 by the Fe(acac)3 solution in carbon tetrachloride only α-Fe2O3 phase is formed in addition to amorphous Fe2O3. The Fe2O3/SiO2 materials remain loose (similar to the A-300 matrix) at the bulk density of 0.12–0.15 g/cm3 and SBET = 265–310 m2/g.  相似文献   