Investigation on Nonradiative Decay of the Er^3+^4I13/2 → ^4I15/2 Transition in Different Tellurite Glass Matrix |
| |
引用本文: | 于春雷,戴世勋,周刚,张军杰,胡丽丽,姜中宏.Investigation on Nonradiative Decay of the Er^3+^4I13/2 → ^4I15/2 Transition in Different Tellurite Glass Matrix[J].中国物理快报,2005,22(11):2926-2928. |
| |
作者姓名: | 于春雷 戴世勋 周刚 张军杰 胡丽丽 姜中宏 |
| |
作者单位: | [1]Shanghai Institute of Optics and Fine Mechanics, Chinese Academy of Sciences, Shanghai 201800 [2]College of Information Science and Engineering, Ningbo University, Ningbo 315211 |
| |
基金项目: | Project supported by the Qimingxing Program of Science and Technology of Shanghai, China (Grant No. 04QMX1448). |
| |
摘 要: | Three kinds of Er^3+-doped tellurite glasses with different hydroxyl groups are prepared by the conventional melt-quenching method. Infrared spectra are measured to estimate the exact content of OH^- groups in samples. The maximum phonon energy in glasses are obtained by measuring the Raman scattering spectra. The strength parameters Ωt (t = 2, 4, 6) for all the samples are calculated and compared. The nonradiative decay rate of the Er^3+ ^4I13/2 → ^4I15/2 transition are calculated for the glass samples with different phonon energy and OH^- group contents. Finally, the effect of OH^- groups on fluorescence decay rate of Er^3+ is analysed, the constant KOH-Er of TWN, TZPL and TZL glasses are calculated to be 9.2 × 10^-19 cm^4s^-1, 5.9 × 10^-19 cm^4s^-1, and 3.5 × 10^-19 cm^4s^-1, respectively.
|
关 键 词: | 非辐射衰退 亚碲酸盐玻璃 红外光谱 氢氧基群 声子能量 光谱散射 |